Long-term reliability of high-zinc Al-Zn-Mg-Cu alloys against stress corrosion cracking
Source abstract
Abstract
High-zinc-content Al-Zn-Mg-Cu alloys exhibit excellent mechanical strength but suffer from severe stress corrosion cracking (SCC), limiting their long-term structural reliability. In this study, a modified Al-Zn-Mg-Cu alloy (designated as T+Mn alloy) was developed by adding Mn to promote Mn-rich dispersoids and applying high-temperature aging to introduce T-phase precipitates, aiming to suppress SCC. Standardized C-Ring testing revealed that the SCC lifetime of the T+Mn alloy was 1–2 orders of magnitude longer than that of the conventional η-phase alloy. The η alloy exhibited intergranular cracking (IGC) and quasi-cleavage fracture (QCF), driven by grain boundary corrosion and hydrogen accumulation, whereas the T+Mn alloy showed delayed crack initiation and QCF-dominated propagation. These improvements were attributed to reduced anodic dissolution and hydrogen redistribution toward benign trap sites. The findings establish a microstructural design strategy to enhance the long-term SCC resistance of high-strength aluminum alloys.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Material Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Effect of precipitate state on the stress corrosion behaviour of 7050 aluminum alloy10.1016/j.matchar.2016.01.022 ↗
2. Revisiting stress-corrosion cracking and hydrogen embrittlement in 7xxx-Al alloys at the near-atomic-scale10.1038/s41467-022-31964-3 ↗
3. Stress corrosion crack initiation and propagation characteristics of 7xxx high-strength Al alloy plate: experiments and modelling10.1016/j.engfailanal.2025.109412 ↗
4. Corrosion behaviour and mechanism of Al–Zn–Mg–Cu alloy based on the characterization of the secondary phases10.1016/j.matchar.2022.111974 ↗
5. Role of retrogression and reaging in suppressing hydrogen-induced transgranular cracking in 7xxx Al alloys10.1016/j.scriptamat.2024.116383 ↗
6. Effect of recrystallization on plasticity, fracture toughness and stress corrosion cracking of a high-alloying Al-Zn-Mg-Cu alloy10.1016/j.matlet.2020.128074 ↗
7. Correlations among stress corrosion cracking, grain-boundary microchemistry, and Zn content in high Zn-containing Al−Zn−Mg−Cu alloys10.1016/S1003-6326(21)65650-9 ↗
8. Environmental cracking performance of new generation thick plate 7000-T7x series alloys in humid air10.1016/j.corsci.2020.108701 ↗
9. Correlations between stress corrosion cracking susceptibility and grain boundary microstructures for an Al–Zn–Mg alloy10.1016/j.corsci.2013.07.032 ↗
10. The postulated mechanisms for stress corrosion cracking of aluminum alloys: a review of the literature 1980-198910.5006/1.3585235 ↗
11. The effect of inhomogeneous microstructures on strength and stress corrosion cracking of 7085 aluminum alloy thick plate10.1016/j.jmrt.2024.05.045 ↗
12. Microstructure and phase composition of novel crossover Al-Zn-Mg-Cu-Zr-Y(Er) alloys with equal Zn/Mg/Cu ratio and Cr addition10.3390/met14050547 ↗
13. Comparative study of stress corrosion cracking and corrosion-induced mechanical property degradation of 7050-T7451 aluminum alloy in chloride solution containing bisulfite10.1016/j.engfailanal.2024.109054 ↗
14. Switching nanoprecipitates to resist hydrogen embrittlement in high-strength aluminum alloys10.1038/s41467-022-34628-4 ↗
15. Hydrogen-accelerated spontaneous microcracking in high-strength aluminium alloys10.1038/s41598-020-58834-6 ↗
16. Healing the high-temperature-retrogression-caused wide precipitation-free zones in Al-Zn-Mg-Cu alloy via strain-aging induced precipitates10.1016/j.msea.2024.147398 ↗
17. Effects of quenching rate and over-aging on microstructures, mechanical properties and corrosion resistance of an Al–Zn–Mg (7046A) alloy10.1016/j.jallcom.2020.157272 ↗
18. The effect of Mn and Zr dispersoid-forming additions on recrystallization resistance in Al–Cu–Li AA2198 sheet10.1016/j.actamat.2014.05.028 ↗
19. Effect of Mn content on the microstructure and corrosion resistance of Al-Cu-Mg-Mn alloys10.1016/j.jallcom.2021.162903 ↗
20. Effect of Er on the hot deformation behaviour of the crossover Al3Zn3Mg3Cu0.2Zr Alloy10.3390/met14101114 ↗
21. Structurally complex phase engineering enables hydrogen-tolerant Al alloys
22. Suppressed hydrogen embrittlement of high-strength Al alloys by Mn-rich intermetallic compound particles10.1016/j.actamat.2022.118110 ↗
23. A high-strength AlZnMg alloy hardened by the T-phase precipitates10.1016/j.jallcom.2014.04.185 ↗
24. Advancing the hydrogen tolerance of ultrastrong aluminum alloys via nanoprecipitate modification10.1016/j.corsci.2024.112471 ↗
25. Exceptional stress corrosion cracking resistance-strength synergy of Al-Zn-Mg-Cu alloys via tailored nano-sized particles
26. ASTM G44-21. Standard practice for exposure of metals and alloys by alternate immersion in neutral 3.5% sodium chloride solution, (2021).
27. Stress corrosion cracking in Al-Zn-Mg-Cu aluminum alloys in saline environments10.1007/s11661-012-1528-3 ↗
28. Assessment of hydrogen embrittlement behaviour in Al-Zn-Mg alloy through multi-modal 3D image-based simulation10.1016/j.ijplas.2024.103897 ↗
29. The effect of quench rate and overageing temper on the corrosion behaviour of AA705010.1016/j.corsci.2013.10.010 ↗
30. Mechanism of low exfoliation corrosion resistance due to slow quenching in high strength aluminium alloy10.1016/j.corsci.2014.11.024 ↗
31. Environment-induced cracking of high-strength Al-Zn-Mg-Cu aluminum alloys: past, present, and future10.5006/4149 ↗
32. Quantitative study of the corrosion evolution and stress corrosion cracking of high strength aluminum alloys in solution and thin electrolyte layer containing Cl-10.1016/j.corsci.2020.109076 ↗
33. Nanoparticle promoted solution treatment by reducing segregation in AA703410.1016/j.msea.2021.141691 ↗
34. Microstructure and mechanical properties of a high-Zn aluminum alloy prepared by melt spinning and extrusion10.1016/j.jallcom.2019.152990 ↗
35. Hydrogen induced debonding of Mg2Si particle/aluminum interface in Al-Mg-Si Alloy10.2320/matertrans.MT-M2024026 ↗
36. Mechanical properties, corrosion behaviour and microstructures of a non-isothermal ageing treated Al-Zn-Mg-Cu alloy10.1016/j.msea.2017.01.086 ↗
37. An experimental study on the dynamic fracture of extruded AA6xxx and AA7xxx aluminium alloys10.1016/j.msea.2009.06.007 ↗
38. Effect of pre-immersion on the SCC of heat-treated AA7050 in an alkaline 3.5%NaCl10.1016/j.corsci.2008.10.037 ↗
39. Study on influence of native oxide and corrosion products on atmospheric corrosion of pure Al10.1016/j.corsci.2013.11.027 ↗
40. The relation between Mn additions, microstructure and corrosion behaviour of new wrought Mg-5Al alloys10.1016/j.matchar.2018.08.033 ↗
41. Anisotropic response in corrosion behaviour of laser powder bed fusion Al-Mn-Mg-Sc-Zr alloy10.1016/j.corsci.2022.110634 ↗
42. SCC susceptibility of RRA treated high-zinc 7068 aluminum alloy10.1016/j.corsci.2023.111257 ↗
43. Hydrogen trapping and embrittlement in high-strength Al alloys10.1038/s41586-021-04343-z ↗
44. The role of precipitates in hydrogen embrittlement of precipitation-hardenable aluminum alloys10.3390/met14111287 ↗
45. New insights into hydrogen trapping and embrittlement in high strength aluminum alloys10.1016/j.corsci.2023.111453 ↗
46. Investigation on microstructure and mechanical properties of Al-Zn-Mg-Cu alloys with various Zn/Mg ratios10.1016/j.jmst.2020.12.045 ↗
47. Corrosion behaviour of nano-treated AA7075 alloy with TiC and TiB2 nanoparticles10.1016/j.corsci.2022.110479 ↗
48. Corrosion behavior of 7050 and 7075 aluminum alloys processed by reactive additive manufacturing10.1016/j.electacta.2023.143357 ↗