Corrosion problems in tinplate cans for storing contact glues for shoes
Source abstract
Abstract
Abstract Tinplate steel cans were used to store contact glue for shoes. A few months after its storage, the glue displayed a change in colour to a darker brown. The visual inspection of the interior of the cans showed the presence of corrosion of steel, which was evidenced by the typical colour of the iron oxides on the sheet. SEM/EDS and FTIR tests confirmed that the anomaly was due to the following factors: (a) a bad tin coating, small thickness and lack of homogeneity; (b) a degradation of glue, hydrolysis of chloroprene, which led to its acidification. Some recommendations are made to overcome similar situations within the same use of these packages looking at the specifications of tinplate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Observations on the influence of microstructure on electrolytic tinplate corrosion10.1016/1044-5803(94)00060-X ↗
2. Lacquered tinplate: corrosion resistance in the function of lacquering conditions
3. Corrosion behaviour of tinplate in NaCl solution10.1016/S1003-6326(11)61236-3 ↗
4. Resnik D, Can corrosion, In: Marsch K, Brody A, (editors.) Wiley’s Encyclopedia; 1997.
5. Recent case histories of food product-metal container interactions using scanning electron microscopy – X-ray microanalysis10.1002/sca.4950190710 ↗
6. Generation reason and corrosion characteristic of cavity of tinplate alloy layer10.1007/s11771-004-0075-5 ↗
7. Electrodeposited lanthanum film as chromate replacement for tinplate10.1016/j.matlet.2007.05.071 ↗
8. Influence of essential onion oil on tin and chromium dissolution from tinplate10.1016/j.fct.2009.04.003 ↗
9. Corrosion inhibition with different protective layers in tinplate cans for food preservation10.1002/jsfa.4101 ↗
10. Titanium-passivated tinplate for canning foods10.1177/1082013205054933 ↗
11. IR and Raman spectroelectrochemical studies of corrosion films on tin10.1016/S0013-4686(00)00660-5 ↗
12. Corrosion products of tin in humid air containing sulfur dioxide and nitrogen dioxide at room temperature10.1016/S0010-938X(02)00151-8 ↗
13. Anodic behaviour of tin in citrate solutions: the IR and XPS study on the composition of the passive layer10.1016/j.tsf.2007.11.118 ↗
14. Electrochemical studies of the pitting corrosion of tin in citric acid solution containing Cl−10.1016/j.electacta.2008.01.051 ↗
15. Protective film growth on tin in perchlorate and citric acid electrolytes10.1016/S0254-0584(00)00458-2 ↗
16. Electrochemical studies on the anodic behaviour of tin in citrate buffer solutions10.1016/j.jelechem.2009.12.002 ↗
17. Electrochemical impedance spectroscopic investigation of dissolution, passivation and pitting corrosion of tin in Na2CO3 solution and the effect of Cl− and I− ions10.1016/S0169-4332(98)00282-7 ↗
18. Electrochemical behaviour of tin in sodium borate solutions and the effect of halide ions and some inorganic inhibitors10.1016/j.corsci.2005.08.002 ↗
19. The electrochemical behaviour of the tin–iron couple in dilute acid media10.1039/tf9343000472 ↗
20. Internal corrosion of tinplate food containers10.1108/eb007005 ↗
21. Dithiocarbamates, carbon disulphide and the corrosion of tinplate10.1179/000705968798325966 ↗
22. Lin-Vien · 1991
23. Blackley · 1997
24. Reconsidering differential aeration cells10.1016/j.electacta.2006.05.056 ↗