Influence of long-term cold climate operation on structure, fatigue durability and impact toughness of 09Mn2Si pipe steel
Source abstract
Abstract
Abstract The microstructure and mechanical properties of 09Mn2Si steel used for the transmission natural gas pipeline “Mastakh-Berge-Yakutsk” have been investigated comprehensively after 37 years of operation. The results obtained for the specimens cut from the pipe were compared to those obtained using the preserved (reference) specimens. It is demonstrated that long-term operation in harsh climate does change the pearlitic microstructure appreciably. The strain aging however can be noticed through precipitation of finely dispersed carbides in the grain interior. The latter causes some embrittlement of the steel measured under impact loading. Revealed microstructural changes are not practically important for “quasi-static” tension or hardness properties. Nonetheless, under cyclic testing the microstructure degradation, which occurred during long-term operation, results in a considerable reduction of fatigue life, which is particularly pronounced during the crack initiation stage. The microstructure degradation is most clearly seen in sharply reduced impact toughness which dropped by a factor of two at temperatures below zero Centigrade. Reasons and mechanisms of the observed phenomena are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Material Properties and Failure Mechanisms · Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Environmentally assisted "in-bulk" steel degradation of long term service gas trunkline10.1016/j.engfailanal.2009.04.007 ↗
2. Assessment of the in-service degradation of pipeline steel by destructive and nondestructive methods10.1007/s11003-012-9431-z ↗
3. Evaluation of the In-service degradation of steels of gas pipelines according to the criterion of mechanical stability10.1007/s11003-015-9790-3 ↗
4. Prediction of remaining strength of corroded pressurised pipelines10.1016/S0308-0161(96)00081-6 ↗
5. Frost-induced deformations and stresses in pipelines10.1016/0308-0161(95)00120-4 ↗
6. Scientific basis for cold brittleness of structural BCC steels and their structural degradation at below zero temperatures10.1134/S1029959917020023 ↗
7. Diagnostics and safety of aging large mechanical systems operating under conditions of the Far North: the problem and ways to solve it10.1134/S1061830908060053 ↗
8. Scientific and Technical bases of risk analysis for petrochemistry objects in the Arctic Zone10.1007/s10556-014-9914-x ↗
9. Methods for analysis of the remaining service life of pipelines and pressure vessels operating at low climatic temperatures10.1007/s10556-012-9546-y ↗
10. Degradation of physical and mechanical condition of the main gas pipeline metal at long operation in the conditions of the cryolitozone
11. Chemical, hydrodynamic, and metallurgical factors in West Siberian oil pipeline corrosion failure10.1023/B:CAPE.0000024135.34938.9b ↗
12. Determination of the actual parameters of the metal of technological objects of oil and gas complexes10.1007/BF02368687 ↗
13. In-service degradation of gas trunk pipeline X52 steel10.1007/s11003-008-9049-3 ↗
14. Effect of temperature for the start of finish rolling on coiled steel X70 microstructure and cold resistance10.1007/s11015-012-9608-6 ↗
15. Relationship between rupture stress and microstructure parameters of plastically deformed heat-resistant steel10.1007/s11223-007-0039-8 ↗
16. Degradation of the main gas pipeline material and mechanisms of its fracture10.3846/13923730.2014.971128 ↗
17. Effect of long-term service of the gas pipeline on the properties of the ferrite–pearlite steel10.1002/maco.200805158 ↗
18. Hydrogen degradation of steels in gas mains after long periods of operation10.1007/s11003-008-9010-5 ↗
19. A review of the fatigue failure mechanism of metallic materials under a corroded environment10.1016/j.engfailanal.2014.04.016 ↗
20. Fatigue-crack-growth behavior of two pipeline steels10.1002/adem.201600340 ↗
21. Influence of long-term operation on the toughness of 17GS pipeline steel10.1023/A:1022066316622 ↗
22. Peculiarities of the static and dynamic failure mechanism of long-term exploited gas pipeline steel10.1177/1687814016641565 ↗
23. Effect of operating degradation in arctic conditions on physical and mechanical properties of 09Mn2Si pipeline steel
24. Experimental evaluation of crack resistance of structural steels using quantitative fractography10.1007/BF00767465 ↗
25. Theory of critical distances versus gradient mechanics in modelling the transition from the short to long crack regime at the fatigue limit10.1111/ffe.12066 ↗
26. Fatigue crack growth in thin steel sheets10.1007/BF00779252 ↗
27. Microstructurally-dependent model for predicting the kinetics of physically small and long fatigue crack growth10.1016/j.ijfatigue.2015.08.002 ↗
28. Fatigue crack propagation behaviour of short cracks; the effect of microstructure10.1111/j.1460-2695.1981.tb01116.x ↗
29. Fatigue and failure of steel of offshore gas pipeline after the laying operation10.1016/j.acme.2016.03.003 ↗