Deposition and corrosion characteristics of liquid-solid droplets on tubular corrosion probes in desulfurized flue gas
Source abstract
Abstract
Abstract In coal-fired boilers, low-temperature corrosion occurring in the back-end is always threatening. Particularly, the desulfurized flue gas from outlet of the flue gas desulfurization (FGD) unit is quite aggressive. The flue gas reheater placed after FGD is usually operating under a much more severe condition than the condensing heat exchangers before FGD. In this paper, field corrosion tests were conducted in a coal-fired heating plant and tubular corrosion probes made of different grades of steels were tested. The total testing period was 6 weeks. The corroded probes were then analyzed by X-ray fluorescence (XRF), X-ray diffraction (XRD), scanning electron microscope (SEM) and energy dispersive spectrometer (EDS), and the deposition and corrosion mechanisms were studied. The droplets entrained by the flue gas resulted in deposition and corrosion on the probe, especially on the windward side. During the tests, 2507 and 2205 showed good corrosion resistance, while ND, 304L, 316L suffered considerable corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: nanoparticles nucleation surface interactions · High-Temperature Coating Behaviors · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. Failure analysis of spiral finned tube on the economizer10.1016/j.engfailanal.2012.10.010 ↗
2. Experimental study on dew point corrosion characteristics of the heating surface in a 65t/h biomass-fired circulating fluidized bed boiler10.1016/j.applthermaleng.2015.10.151 ↗
3. Mechanism research on coupling effect between dew point corrosion and ash deposition10.1016/j.applthermaleng.2012.12.013 ↗
4. Experimental study and mechanism analysis on low temperature corrosion of coal fired boiler heating surface10.1016/j.applthermaleng.2015.02.003 ↗
5. Corrosion analysis and inhibition studies in the process of natural gas wet desulfurization10.1016/j.engfailanal.2014.04.030 ↗
6. Analysis of degradation of a super-austenitic stainless steel for flue gas desulfurization system after a fire accident10.1016/j.engfailanal.2007.04.006 ↗
7. Failure analysis of enamel-coated carbon steel heating elements of gas-gas heater for flue gas desulfurization system10.1016/j.engfailanal.2006.02.009 ↗
8. Research on the influence of salt water on the corrosion and scaling of the absorption tower
9. Technical features of lower temperature high efficiency flue gas treatment system and its application prospects in China
10. Corrosion in flue gas desulfurization plants and other low temperature equipment10.1002/maco.19920430610 ↗