Pitting corrosion failure of an AISI stainless steel pointer rod
Source abstract
Abstract
In this study, failure analysis of a thermostatic mixing valve pointer rod made of AISI 304 stainless steel was performed. Visual examination, followed by an in-depth microstructural characterization using optical and scanning electron microscopy, was carried out for understanding the primary cause of failure. Energy dispersive X-ray, X-ray diffraction analysis and transmission electron microscopic analyses were also necessary supplements to this investigation. Finally, the obtained results infer that the combined effect of large amounts of MnS inclusions and the presence of deformation induced martensite adversely affected the pitting corrosion resistance of the pointer rod material. It is concluded that the pointer rod material was not properly investigated for defects prior to and after its fabrication.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Wren J, Persson P, Loyd D. Thermostatic mixing valves: thermostatic temperature distribution during various operating conditions. Department of Mechanical Engineering, Linköpings Universitet, SE581 83 Linköping, Sweden.
2. Guardian equipment, installation, operation and maintenance guide of thermostatic mixing valves. Report no: 0114/2014.
3. The initiation of pitting corrosion at MnS inclusions10.1016/0010-938X(93)90279-P ↗
4. Why stainless steel corrodes10.1038/415770a ↗
5. Effects of Mn on the localized corrosion behavior of Fe–18Cr alloys10.1016/j.electacta.2010.01.006 ↗
6. The initiation of pitting corrosion on austenitic stainless steel: on the role and importance of sulphide inclusions10.1016/0010-938X(92)90074-D ↗
7. Role of manganese sulfide inclusions on pit initiation of super austenitic stainless steels10.5006/1.3277537 ↗
8. Initiation of pitting at sulfide inclusions in stainless steel10.1149/1.2401840 ↗
9. Phase transformation influence on corrosion resistance of AISI 316 austenitic stainless steel
10. Effect of deformation-induced martensite on the microstructure, mechanical properties and corrosion resistance of X5CrNi18-8 stainless steel
11. Effects of pre-deformation on electrochemical behavior of AISI304 stainless steel10.1016/j.proeng.2011.12.630 ↗
12. The effect of (γ→α′) phase transformation on microstructure and properties of austenitic Cr–Ni steels
13. Structural variations ahead of crack tip during monotonic and cyclic fracture tests of AISI 304LN stainless steel10.1016/j.msea.2012.10.074 ↗
14. Deformation fatigue and fracture vis-à-vis deformation induced martensite in AISI 304LN Stainless Steel10.4028/www.scientific.net/AMR.794.415 ↗
15. Pitting corrosion of metals – a review of the critical factors10.1149/1.1838615 ↗
16. Corrosion at sulphide inclusions in stainless steel
17. Hydrogen-induced delayed cracking in the AISI 301 unstable austenitic steel sheet10.1016/j.matdes.2010.03.004 ↗
18. Effect of strain-induced martensite on hydrogen environment embrittlement of sensitized austenitic stainless steels at low temperatures10.1016/S1359-6454(98)00136-0 ↗
19. Effect of chemical compositions on season cracking of metastable austenitic stainless steel10.2355/isijinternational1966.20.147 ↗
20. Stress corrosion cracking of hydrogen-containing austenitic stainless steel in H2SO4–NaCl solution10.2355/isijinternational1966.21.464 ↗
21. Hydrogen-facilitated anodic dissolution of austenitic stainless steels10.5006/1.3284854 ↗