Evaluation of high strength steels fracture based on uniaxial stress-strain curves
Source abstract
Abstract
Predicting the ultimate capacity of components made of high strength steel (HSS) is a numerically challenging task. The fracture performance of HSS from different steel grades, producers, and manufacturing processes (rolling, cold forming, etc.) varies greatly. It is costly to conduct a series of experiments for each typical HSS structural component to identify the parameters of the fracture model. An attempt is made to evaluate the fracture material properties based only on the standardized uniaxial stress-strain curve. The uncoupled fracture model was implemented through a user subroutine VUMAT (ABAQUS) to evaluate the ductile fracture of HSS, where a rate-independent non-linear isotropic J2 hardening model is used in combination with a separate Hosford-Coulomb fracture model. The detailed procedure to identify the material parameters based on only the uniaxial stress-strain curve of steel grades S700 and S960 are provided for the sake of illustration of possible applications. The proposed fracture model and identified parameters are validated based on the experimental results of the HSS plate with different hole sizes in the middle of the dog bone specimens. Besides, a desktop study of a single K gap joint with β = 0.5 made of square hollow sections using S700 and S960 is used to illustrate a possible application of the fracture model in a simplified model of the structural joint.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal Forming Simulation Techniques · Fatigue and fracture mechanics · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Section capacity of very high strength (VHS) circular tubes under compression10.1016/S0263-8231(00)00017-3 ↗
2. Development and use of high performance steel10.1016/S0143-974X(03)00118-4 ↗
3. Design of hybrid steel girders10.1016/S0143-974X(03)00128-7 ↗
4. H. Xin, A.F.O. Correia José, M. Veljkovic, Three-dimensional Fatigue Crack Propagation Simulation Using Extended Finite Element Methods for Steel Grades S355 and S690 Considering Mean Stress Effects, Eng. Struct. https://doi.org/10.1016/j.engstruct.2020.111414.10.1016/j.engstruct.2020.111414 ↗
5. Fatigue crack initiation prediction using phantom nodes-based extended finite element method for S355 and S690 steel grades10.1016/j.engfracmech.2019.04.026 ↗
6. Residual stress effects on fatigue crack growth rate of mild steel S355 exposed to air and seawater environments10.1016/j.matdes.2020.108732 ↗
7. A.A. Benzerga, J.-B. Leblond, Ductile fracture by void growth to coalescence, in: Advances in Applied Mechanics. Adv Appl Mech 10 (2010) 169–305. https://doi.org/10.1016/S0065-2156(10)44003-X.10.1016/S0065-2156(10)44003-X ↗
8. F.A. McClintock, A criterion for ductile fracture by the growth of holes, 1968.10.1115/1.3601204 ↗
9. On the ductile enlargement of voids in triaxial stress fields∗10.1016/0022-5096(69)90033-7 ↗
10. A.L. Gurson, Continuum theory of ductile rupture by void nucleation and growth: Part I—Yield criteria and flow rules for porous ductile media, 1977.10.1115/1.3443401 ↗
11. Influence of voids on shear band instabilities under plane strain conditions10.1007/BF00036191 ↗
12. Analysis of the cup-cone fracture in a round tensile bar10.1016/0001-6160(84)90213-X ↗
13. Plastic potentials for anisotropic porous solids10.1016/S0997-7538(01)01147-0 ↗
14. Modification of the Gurson Model for shear failure10.1016/j.euromechsol.2007.08.002 ↗
15. G.R. Johnson, W.H. Cook, A constitutive model and data for metals subjected to large strains, high strain rates and high temperatures, Proc. 7th Int. Symp. Ballist., vol. 21, The Netherlands, 1983, p. 541–547.
16. Application of extended Mohr–Coulomb criterion to ductile fracture10.1007/s10704-009-9422-8 ↗
17. Ductile fracture experiments with locally proportional loading histories10.1016/j.ijplas.2015.08.004 ↗
18. Hybrid experimental–numerical analysis of basic ductile fracture experiments for sheet metals10.1016/j.ijsolstr.2009.12.011 ↗
19. Micromechanically-motivated phenomenological Hosford–Coulomb model for predicting ductile fracture initiation at low stress triaxialities10.1016/j.ijsolstr.2015.02.024 ↗
20. A new model of metal plasticity and fracture with pressure and Lode dependence10.1016/j.ijplas.2007.09.004 ↗
21. On fracture locus in the equivalent strain and stress triaxiality space10.1016/j.ijmecsci.2004.02.006 ↗
22. Modeling of shear ductile fracture considering a changeable cut-off value for stress triaxiality10.1016/j.ijplas.2013.08.006 ↗
23. Models for ductile damage and fracture prediction in cold bulk metal forming processes: a review10.1007/s12289-015-1262-7 ↗
24. L.H. Pál Turána, Experimental behaviour of tension plates with centre hole made from high strength steel. Nord. Steel Constr. Conf. 2015, Tampere, Finland, 2015.
25. Rui Yan, Haohui Xin, Milan Veljkovic, Identification of GTN damage parameters as a surrogate model for S355, Proc. 17th Int. Symp. Tubul. Struct., Singapore, 2019. https://doi.org/10.3850/978-981-11-0745-0_066-cd.10.3850/978-981-11-0745-0_066-cd ↗
26. A surrogate modeling approach for additive-manufactured materials10.1615/IntJMultCompEng.2017024632 ↗
27. Discrete element simulations of powder-bed sintering-based additive manufacturing10.1016/j.ijmecsci.2017.11.028 ↗
28. 6.14 Documentation
29. A note on calibration of ductile failure damage indicators10.1007/BF00027274 ↗
30. W. Ramberg, W.R. Osgood, Description of stress-strain curves by three parameters, 1943.
31. Uniaxial true stress-strain after necking
32. Mechanical characterization of a unidirectional pultruded composite lamina using micromechanics and numerical homogenization10.1016/j.conbuildmat.2019.04.191 ↗
33. Computational homogenization simulation on steel reinforced polymer used in the injected bolted connections10.1016/j.compstruct.2018.11.069 ↗
34. 1993-1-1 EN. Eurocode 3: Design of steel structures: General rules and rules for buildings, 2005.
35. Standardization. EN1993-1-8 ver. 2020-03-30. Eurocode 3: Design of steel structures - Part 1-8: Design of joints. n.d.