journal article·2017-12

Sigma phase-induced failure of AISI 310 stainless steel radiant tubes

Abbas Bahrami, Ali Ashrafi, Seyed Mahdi Rafiaei, Maryam Yazdan Mehr

Publisher page

Abstract

Abstract Failure of AISI 310 stainless steel tubes, used as radiant tubes in a heat treatment furnace, operating at temperature range 480 to 700 °C, is investigated. Longitudinal cracks were observed in tubes after around five years of operation. Optical microscope, scanning electron microscope (SEM) and energy dispersive spectroscopy (EDS) were used to analyze the observed failure. Results revealed that the failure is due to the formation of sigma phase. Sigma phase formation is accompanied with loss of ductility and formation of voids and subsequently cracks. Possible reasons for the formation of sigma phase, its implications for the mechanical integrity of the tubes, and strategies to avoid observed failure in similar cases are presented and discussed in this paper.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fatigue and fracture mechanics · Aluminum Alloy Microstructure Properties · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Effects of surface laser treatments on microstructure, tension, and fatigue behavior of AISI 316LVM biomedical wires10.1016/j.msea.2017.01.083 ↗
2. Analysis of failed reformer tubes10.1016/S1350-6307(02)00029-8 ↗
3. Failure due to structural degradation in turbine blades10.1016/j.engfailanal.2004.12.041 ↗
4. Microstructural aspects of the failure analysis of nickel base superalloys components10.1016/j.engfailanal.2004.09.010 ↗
5. Microstructure effects on high temperature fatigue crack initiation and short crack growth in turbine disc nickel-base superalloy Udimet 720Li10.1016/j.msea.2006.11.016 ↗
6. On the effect of σ-phase formation during metal dusting10.1016/j.matchemphys.2003.09.041 ↗
7. Grain size effect on high-temperature fatigue properties of alloy71810.1016/j.matlet.2004.09.029 ↗
8. Failure analysis of welded joints in a power plant exhaust flue10.1016/j.engfailanal.2005.02.019 ↗
9. σ phase embrittlement of a type 310 stainless steel10.1016/0921-5093(91)90695-J ↗
10. The kinetics of σ-phase precipitation in AISI310 and AISI316 steels10.1007/BF02643779 ↗
11. Devine TM
12. Effects of sigma phase precipitation on seawater pitting of duplex stainless steel10.1016/j.desal.2006.05.021 ↗
13. Influence of σ-phase on mechanical properties and corrosion resistance of duplex stainless steels10.1016/S0010-938X(99)00009-8 ↗
14. Sigma phase formation and embrittlement of cast iron-chromium-nickel (Fe–Cr–Ni) alloys
15. Overview of intermetallic sigma (σ) phase precipitation in stainless steels10.5402/2012/732471 ↗
16. Sigma phase precipitation and its effect on the mechanical properties of a super duplex stainless steel10.1016/0921-5093(94)91083-9 ↗
17. Balancing the composition of cast 25 per cent chromium-12 per cent nickel type alloys
18. Microstructural changes and corrosion resistance of AISI 310S steel exposed to 600–800°C10.1016/j.matchar.2008.12.005 ↗
19. Pardal JM, Carvalho SS; Barbosa, C.; Montenegro, T.R.; Tavares, S.S.M. Failure analysis of AISI 310S plate in an inert gas generator used in off-shore oil platform. Eng. Fail. Anal., v. 18, p. 1435-1444, 2011.10.1016/j.engfailanal.2011.04.005 ↗