Electrochemical impedance behavior and corrosion resistance of amorphous 316-type stainless steel microfibers in saline environment
Source abstract
Abstract
The resistance of commercial stainless steel (SS) types in harsh environments is problematic because of the breakdown of the passive chromium oxide layer. This study aims to improve the corrosion resistance and passivation properties of commercial SS by producing fully amorphized 316 SS microfibers with multi-nozzle melt-spinning. Electrochemical tests in 3.5 wt.% NaCl shows a low current density of 0.77×10 –5 A cm –2 under ambient conditions, which increases slightly to 1.0×10 –5 A cm –2 as the temperature rises to 50 °C. Sample electrochemically tested at 25°C also shows a current density at the level of 10 –4 A cm –2 with long-term stability, and minor metastable pitting due to metal-Cl ─ ion interactions is observed for the sample at 50 °C until 1.5 V. Electrochemical impedance spectroscopy before and after polarization at 50 °C shows an increase in both charge transfer resistance and double-layer admittance, suggesting double-layer formation on the outer surface due to Cl ─ ion accumulation. Cross-sectional investigation by scanning transmission electron microscopy–electron energy loss spectroscopy corroborates the homogenous bulk composition and Fe-rich, Ni and Cr-containing amorphous oxide (<200 nm), both of which contribute to the corrosion resistance and passivation properties compared to nanocrystalline SS counterparts.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Electrodeposition and Electroless Coatings · Anodic Oxide Films and Nanostructures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (78)
Show source-provided references
1. Microstructural features contributing to macroscopic corrosion: the role of oxide inclusions on the corrosion properties of additively manufactured 316L stainless steel10.1016/j.corsci.2022.110354 ↗
2. Corrosion properties of CVD grown Ti(C,N) coatings in 3.5 wt% NaCl environment10.1080/1478422X.2018.1467150 ↗
3. Effect of heat treatment on microstructure evolution and erosion-corrosion behavior of a nickel-aluminum bronze alloy in chloride solution10.1016/j.corsci.2015.05.037 ↗
4. Material properties of long term naturally aged die cast Al-Si-Cu alloys10.1179/1743133611Y.0000000001 ↗
5. Study of stainless steel electrodes after electrochemical analysis in sea water condition10.1016/j.envres.2019.03.069 ↗
6. Surface modification of type 304 stainless steel with duplex coatings for corrosion resistance in sea water environments10.1179/1743294414Y.0000000354 ↗
7. Effect of corrosion temperature on the corrosion of Q235 steel and 16Mn steel in sodium aluminate solutions10.1021/acsomega.1c02220 ↗
8. Synthesis and characterization of functionalized polyacrylonitrile coated with iron oxide nanoparticles and its applicability in nitrate removal from aqueous solution10.1080/19443994.2013.867816 ↗
9. Role of the microstructures on uniform corrosion and SCC behavior of high-strength low-alloy steels10.1007/s10853-022-07976-1 ↗
10. Effect of microstructure on corrosion behavior of high strength martensite steel—A literature review10.1007/s12613-020-2242-6 ↗
11. Passivity breakdown of 316L stainless steel during potentiodynamic polarization in NaCl solution10.1016/j.corsci.2016.06.011 ↗
12. Effect of elevated temperature variations on the corrosion resistance of S31603 and SS2562 austenitic stainless steels in chloride-sulphate environments10.1016/j.jmrt.2019.09.008 ↗
13. Pitting corrosion of metals: a review of the critical factors10.1149/1.1838615 ↗
14. Experimental design to study the influence of temperature, pH, and chloride concentration on the pitting and crevice corrosion of UNS S30403 stainless steel10.1016/j.corsci.2019.108160 ↗
15. Super-hydrophobic multilayer coatings with layer number tuned swapping in surface wettability and redox catalytic anti-corrosion application10.1038/s41598-017-04651-3 ↗
16. Corrosion protection of NiNb metallic glass coatings for 316SS by magnetron sputtering10.1016/j.jmst.2020.12.004 ↗
17. Electrochemical and localized corrosion behavior of 316 L SS/copper/316 L SS sandwich composite in chloride-containing environment10.1016/j.corsci.2022.110719 ↗
18. Chloride corrosion behavior on heating pipeline made by AISI 304 and 316 in reclaimed water10.1039/D1RA06695A ↗
19. Fouling influence on pitting corrosion of stainless steel heat exchanging surface
20. Mitigation of concrete reinforced steel corrosion by penta sodium triphosphate: physicochemical and electrochemical investigations10.1007/s42452-020-03586-1 ↗
21. Dispersion, workability and mechanical properties of different steel-microfiber-reinforced concretes with low fiber content10.3390/su10072335 ↗
22. Corrosion behavior of Fe41Co7Cr15Mo14C15B6Y2 bulk metallic glass in NaCl solution10.1016/j.matlet.2011.10.116 ↗
23. Acid corrosion process of Fe-based bulk metallic glass10.1016/j.corsci.2012.05.004 ↗
24. Surface-governed electrochemical hydrogenation in FeNi-based metallic glass10.1016/j.jpowsour.2020.228700 ↗
25. Prominent Fe-based bulk amorphous steel alloy with large supercooled liquid region and superior corrosion resistance10.1016/j.jallcom.2013.09.186 ↗
26. Effects of ambient gases on surface profile and related properties of amorphous alloy ribbons fabricated by melt-spinning10.1143/JJAP.19.1781 ↗
27. Bio-corrosion studies of Fe-based metallic glasses10.1016/j.matpr.2020.07.588 ↗
28. Formation of metallic glass nanowires by gas atomization10.1021/nl3003864 ↗
29. Recent advances in metallic glass nanostructures: synthesis strategies and electrocatalytic applications
30. Correlation of microstructural evolution and tensile mechanical behavior of Gd–Al–Co–Fe series “metallic glass” fibers10.1016/j.jmrt.2021.07.053 ↗
31. Micro-and nanoscale metallic glassy fibers10.1002/adem.201000204 ↗
32. Fabrication of stainless-steel microfibers with amorphous-nanosized microstructure with enhanced mechanical properties10.1038/s41598-022-14475-5 ↗
33. Photocalorimetric cooling rate measurements on a Ni-5 wt% A1 alloy rapidly solidified by melt spinning10.1016/0001-6160(85)90005-7 ↗
34. Improvement of hardness in Ti-stabilized austenitic stainless steel10.1016/j.matdes.2022.111242 ↗
35. Validation of corrosion rates measured by the Tafel extrapolation method10.1016/j.corsci.2005.05.046 ↗
36. Enhanced localized and uniform corrosion resistances of bulk nanocrystalline 304 stainless steel in high-concentration hydrochloric acid solutions at room temperature10.1016/j.jmst.2018.06.006 ↗
37. Chemical states in oxide films on stainless steel treated in supercritical water: factor analysis of X-ray photoelectron spectra10.1149/1.2098347 ↗
38. Material No.: 1.4401, 〈https://woite-edelstahl.com/14401en.html〉.
39. Transition metal-based high entropy alloy microfiber electrodes: corrosion behavior and hydrogen activity10.1016/j.corsci.2021.109880 ↗
40. Salt coatings functionalize inert membranes into high-performing filters against infectious respiratory diseases10.1038/s41598-020-70623-9 ↗
41. Electrochemical behavior of B(iii) on a molybdenum electrode in NaCl–KCl eutectic molten salt10.1039/C6RA08850C ↗
42. Universal and reusable virus deactivation system for respiratory protection10.1038/srep39956 ↗
43. Electrochemical behaviour of Fe-based metallic glasses in acidic and neutral solutions10.1016/j.corsci.2012.05.025 ↗
44. General and pitting corrosion deduced from current oscillations in the passive–active transition state of the Fe∣H2SO4 electrochemical system10.1016/S0013-4686(02)00412-7 ↗
45. Observations of localised instability of passive titanium in chloride solution10.1016/0013-4686(95)00126-Y ↗
46. Influence of grain size on the corrosion behavior of a Ni-based superalloy nanocrystalline coating in NaCl acidic solution10.1016/j.electacta.2007.10.048 ↗
47. Growth of corrosion pits on stainless steel in chloride solution containing dilute sulphate10.1016/0010-938X(92)90191-5 ↗
48. Electron energy-loss spectroscopy in the TEM10.1088/0034-4885/72/1/016502 ↗
49. The corrosion of tin under thin electrolyte layers containing chloride10.1016/j.corsci.2012.08.040 ↗
50. Effect of temperature on corrosion behavior of E690 steel in 3.5wt% NaCl solution10.1088/2053-1591/abda69 ↗
51. Effects of temperature and applied strain on corrosion of X80 pipeline steel in chloride solutions10.1080/1478422X.2018.1491111 ↗
52. Corrosion improvement of 304L stainless steel by ZrSiN and ZrSi(N,O) mono- and double-layers prepared by reactive cathodic arc evaporation10.3390/coatings11101257 ↗
53. Incorporation of silicon fume and fly ash as partial replacement of Portland cement in reinforced concrete: electrochemical study on corrosion behavior of 316LN stainless steel rebar10.20964/2020.05.77 ↗
54. Electrochemical corrosive behaviors of Fe-Based amorphous/nanocrystalline coating on stainless steel prepared by HVOF-sprayed10.3390/coatings9040226 ↗
55. The corrosion behaviour of amorphous metal fiber compared with that of stainless steel fiber10.1088/1742-6596/1637/1/012010 ↗
56. Effect of alloyed molybdenum on corrosion behavior of plasma immersion nitrogen ion implanted austenitic stainless steel10.1016/j.corsci.2013.04.030 ↗
57. Effect of surface finish on the pitting corrosion behavior of sensitized AISI 304 austenitic stainless steel alloys in 3.5% NaCl solutions10.3103/S1068375518010039 ↗
58. Influence of temperature and hydrostatic pressure on the galvanic corrosion between 90/10 Cu–Ni and AISI 316L stainless steel10.1016/j.jmrt.2021.05.067 ↗
59. Influence of chloride ion concentration and temperature on the electrochemical properties of passive films formed on a superduplex stainless steel10.1016/j.matchar.2009.12.004 ↗
60. A protective role of Cl− ion in corrosion of stainless steel10.1016/j.corsci.2023.111631 ↗
61. Passivation potential regulating corrosion resistance and antibacterial property of 316L-Cu stainless steel in different simulated body fluids10.1080/10667857.2020.1734723 ↗
62. Electrochemical corrosion behaviours of AISI 304 austenitic stainless steel in NaCl solutions at different pH10.1063/1.5066757 ↗
63. Effect of thiosulfate on pitting corrosion of 316SS: II. Metastable pitting and transition to stability10.1149/2.0041504jes ↗
64. Mechanical and electrochemical characterization of supersolidus sintered austenitic stainless steel (316 L)10.1515/htmp-2019-0032 ↗
65. Uhlig · 2011
66. Corrosion behavior of mild-steel in cooling towers using high salinity solution
67. Electrochemical and thermodynamic study on the corrosion performance of API X120 steel in 3.5% NaCl solution10.1038/s41598-020-61139-3 ↗
68. Influence of low temperature heat treatment on microstructure, corrosion resistance and biological performance of 316L stainless steel manufactured by selective laser melting10.1016/j.cirpj.2022.11.006 ↗
69. The influence of heat treatment on the microstructure and corrosion behavior of selective laser melted 316L stainless steel in Ringer’s solution
70. Electrochemical behavior of additively manufactured 316L stainless steel in H2SO4 solution containing methionine as an amino acid10.1016/j.colsurfa.2021.127120 ↗
71. Enhancing effects of NaHSO3 on Corrosion of T91 Steel
72. Electrochemical impedance spectroscopy and its applications
73. Orazem · 2008 · 523
74. Time-resolved corrosion behavior of transition-metal-based high-entropy alloy in saline and phosphate buffer solutions10.3390/met13050951 ↗
75. The determination of coating performance with impedance measurements-I. Coating polymer properties10.1016/0010-938X(93)90245-C ↗
76. Effects of chloride ions on electrochemical reaction of 316 stainless steel in mixtures of molten nitrate salts10.1002/mawe.201900016 ↗
77. Analysis of electrochemical impedance spectroscopy response for commercial lithium-ion batteries: modeling of equivalent circuit elements10.3906/kim-1910-72 ↗
78. Study on pitting process of 316L stainless steel by means of staircase potential electrochemical impedance spectroscopy10.1007/s12613-011-0398-9 ↗