journal article·2020-11-01

Engineering Surface Texture of Pads for Improving CMP Performance of Sub-10 nm Nodes

Aniruddh J. Khanna, Veera Raghava Kakireddy, Jason Fung, Mayu Yamamura, Puneet Jawali, Ashwin Chockalingam, Nandan Baradanahalli Kenchappa, Daniel Redfield, Rajeev Bajaj

Publisher page

Abstract

Shallow trench isolation (STI) chemical mechanical planarization (CMP) will continue to be a critical step in the device fabrication of future technology nodes. A CMP process needs the right combination of pad, slurry, and pad conditioner to be able to deliver the best performance. Engineered pad surface along with usage of non-Prestonian ceria slurries can be used to solve key STI CMP challenges. Herein, it is demonstrated that relative to a reference pad, reducing and optimizing pad surface roughness, can help improve material removal rate by 26%–95% at different wafer pressures, lower the dishing by 34%–51% for feature size of 50–200 μ m, thereby leading to an improved planarization performance. This work illustrates that the surface texture of a pad can be used to achieve a stable dishing range over different feature scales for various over polish times. Also, optimizing the pad surface roughness minimizes slurry consumption by 33% and enables polishing at a lower downforce. Further, it is demonstrated that relative to a reference pad, defectivity can be improved up to 85% for the pad without impacting the planarization performance by reducing the pad material hardness and polishing at an optimized pad surface roughness.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Semiconductor materials and devices · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Potassium Oleate as a dissolution and corrosion inhibitor during chemical mechanical planarization of chemical vapor deposited Co films for interconnect applications10.1149/2.0251712jss ↗
2. Ammonium Persulfate and Potassium Oleate containing silica dispersions for chemical mechanical polishing for cobalt interconnect applications10.1149/2.0021905jss ↗
3. Formation of Cobalt-BTA complexes and their removal from various surfaces relevant to cobalt interconnect applications10.1149/2.0011905jss ↗
4. Microlens array fabrication by chemical mechanical polishing10.1149/1.3065966 ↗
5. Surface shaping using chemical mechanical polishing10.1149/1.3547710 ↗
6. Analysis of light out-coupling from microlens array10.1016/j.optcom.2011.06.005 ↗
7. Operational aspects of chemical mechanical polishing polish pad profile optimization10.1149/1.1393997 ↗
8. Pad surface microstructure and optimization of the conditioning sweep
9. Effect of conditioner type and downforce, and pad break-in time, on pad surface micro-texture in chemical mechanical planarization10.1149/2.0261811jss ↗
10. Effect of process conditions on uniformity of velocity and wear distance of pad and wafer during chemical mechanical planarization10.1007/s11664-004-0294-4 ↗
11. Chemical mechanical polishing: theory and experiment10.1007/s40544-013-0035-x ↗
12. In situ profile control with titan edge™ heads for dielectric planarization of advanced CMOS devices
13. Planarization improvement using non-porous polishing pad in ILD CMP
14. Semi-empirical material removal rate distribution model for SiO2 chemical mechanical polishing (CMP) processes10.1016/j.precisioneng.2012.12.006 ↗
15. Influence of colloidal abrasive size on material removal rate and surface finish in SiO2 chemical mechanical polishing10.1080/10402000208982545 ↗
16. Study of agglomeration behavior of chemical mechanical polishing slurry under controlled shear environments10.1149/2.0091805jss ↗
17. Method for determining stability of CMP slurry10.1149/2.0241808jss ↗
18. Novel method to synthesize ceria coated silica particles10.1557/PROC-1157-E08-07 ↗
19. Potassium periodate-based solutions for minimizing galvanic corrosion at the Cu-Mn interface and for polishing the associated Cu interconnect structures10.1149/2.026304jss ↗
20. Role of potassium permanganate-based solutions in controlling the galvanic corrosion at Al-Co interface10.1149/2.016303jss ↗
21. Effects of CMP pad conditioner properties and performance on polishing pad, process and wafer removal rate10.1149/1.3489056 ↗
22. Effect of temperature on copper damascene chemical mechanical polishing process10.1116/1.2825143 ↗
23. Methodology for pad conditioning sweep optimization for advanced nodes10.1016/j.mee.2019.111101 ↗
24. Quantification of shear induced agglomeration in chemical mechanical polishing slurries under different chemical environments10.1016/j.mee.2019.03.012 ↗
25. Impact of pad material properties on CMP performance for Sub-10nm technologies10.1149/2.0121905jss ↗
26. Characterization of the nature of shear induced agglomerates as hard & soft in chemical mechanical polishing slurries10.1116/1.5065516 ↗
27. Quantification of particle agglomeration during CMP of metals and dielectrics
28. Effect of temperature on copper chemical mechanical planarization
29. Effect of slurry characteristics on the surface tribology during copper CMP process10.1149/1.2819480 ↗
30. Retaining ring design impact on CMP process stability and optimization10.1557/PROC-1249-E02-01 ↗
31. Some tribological aspects of thin film copper during CMP10.1115/IJTC2006 ↗
32. Interconnect, International Technology Roadmap for Semiconductors · 2003 · FEP · 1
33. Interconnect, International Technology Roadmap for Semiconductors · 2007 · FEP · 1
34. International Technology Roadmap for Semiconductors · 2013 · FEP · 1
35. Polishing pads produced by an additive manufacturing process
36. Polishing pads produced by an additive manufacturing process
37. Polishing pads produced by an additive manufacturing process
38. Techniques for combining CMP process tracking data with 3D printed CMP consumables
39. Managing STI CMP performances through pad microstructure control using disruptive technology
40. Thin plastic polishing article for cmp applications
41. Method for improved CMP pad conditioning performance10.1109/ASMC.2010.5551441 ↗
42. Khanna · ECS J. Solid State Sci. Technol. · 2020 · 910.1149/2162-8777/aba9fd ↗
43. The theory and design of plate glass polishing machines
44. Sub · AIP Conference Proceedings · 2017 · 187510.1063/1.4998394 ↗
45. STI CMP stop in Silicon Nitride controlled by FullVisionTM endpoint
46. Comparison of Silica- and Ceria-Slurry for Direct STI-CMP
47. Shallow trench isolation chemical mechanical planarization: a review10.1149/2.0071511jss ↗
48. Ceria-based slurries for non-prestonian removal of silicon dioxide films10.1149/2.0091502jss ↗
49. Effect of conditioning downforce and pad break-in time on pad surface micro-texture10.1149/2.0271805jss ↗
50. A method for characterizing the pad surface texture and modeling its impact on the planarization in CMP10.1016/j.mee.2012.10.007 ↗
51. Advances in CMP pad conditioning
52. ILD CMP with silica abrasive particles: effect of pore size of CMP pad on removal rate profiles10.1149/2.020303jss ↗
53. Khanna · ECS J. Solid State Sci. Technol. · 2020 · 910.1149/2162-8777/aba726 ↗