Self-Limiting Growth and Thickness- and Temperature- Dependence of Optical Constants of ALD AlN Thin Films
Source abstract
Abstract
We have investigated the growth characteristics and optical constants of thin AlN films made by thermal atomic layer deposition (ALD) from trimethylaluminum (TMA) and ammonia (NH3). We observed the nucleation, closure and growth after closure of the films using atomic force microscopy and in-situ spectroscopic ellipsometry. A fully covered surface was obtained for films with a thickness of about 2 nm. The self-limiting ALD growth was observed at temperatures of 330 and 350◦C with deposition rates of 1.5 and 2.1 Å/cycle, respectively. At 370◦C, thermal decomposition of TMA dominated the growth mechanism, resulting in a fast and non-self-limiting deposition. Low concentrations of oxygen (0.8−2.5%) and carbon (5−7.5%) incorporated into the films were measured. We found that the refractive index increased remarkably with increasing film thickness and growth temperature.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: GaN-based semiconductor devices and materials · Semiconductor materials and devices · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. 10.1038/nature0476010.1038/nature04760 ↗
2. 10.1063/1.153254510.1063/1.1532545 ↗
3. 10.1002/adma.20040050410.1002/adma.200400504 ↗
4. 10.1063/1.200983810.1063/1.2009838 ↗
5. 10.1063/1.321658610.1063/1.3216586 ↗
6. 10.1063/1.319414810.1063/1.3194148 ↗
7. 10.1116/1.58203510.1116/1.582035 ↗
8. 10.1016/j.jnoncrysol.2005.08.00910.1016/j.jnoncrysol.2005.08.009 ↗
9. 10.1063/1.242322410.1063/1.2423224 ↗
10. 10.1063/1.298832310.1063/1.2988323 ↗
11. 10.1063/1.271637510.1063/1.2716375 ↗
12. 10.1149/1.330166410.1149/1.3301664 ↗
13. 10.1063/1.481879210.1063/1.4818792 ↗
14. 10.1109/LED.2012.218592110.1109/LED.2012.2185921 ↗
15. 10.1088/0268-1242/28/7/07401510.1088/0268-1242/28/7/074015 ↗
16. 10.1016/j.apsusc.2011.04.03710.1016/j.apsusc.2011.04.037 ↗
17. 10.1016/j.tsf.2011.11.08110.1016/j.tsf.2011.11.081 ↗
18. 10.1557/PROC-811-D1.910.1557/PROC-811-D1.9 ↗
19. 10.1002/cvde.1996002061210.1002/cvde.19960020612 ↗
20. 10.1021/cm00016a01610.1021/cm00016a016 ↗
21. 10.1109/LED.2013.227442910.1109/LED.2013.2274429 ↗
22. 10.1149/2.015304jss10.1149/2.015304jss ↗
23. 10.1103/PhysRevB.84.05442010.1103/PhysRevB.84.054420 ↗
24. 10.1103/PhysRevB.81.16543510.1103/PhysRevB.81.165435 ↗
25. Doering R. Nishi Y. , Handbook of Semiconductor Manufacturing Technology, 2nd Ed., CRC Press, Boca Raton, FL (2008).10.1201/9781420017663 ↗
26. 10.1116/1.368793710.1116/1.3687937 ↗
27. Holtz M. Kipshidze G. Chandolu A. Yun J. Borisov B. Kuryatkov V. Zhu K. Chu S. N. G. Nikishin S. A. Temkin H. , Preparation of Optoelectronic Devices Based on AlN/AlGaN Superlattices, unpublished.
28. Tompkins H. G. Irene E. A. , Handbook of Ellipsometry, William Andrew, New York, p.180 (2005).10.1007/3-540-27488-X ↗
29. 10.1063/1.302114810.1063/1.3021148 ↗
30. 10.1063/1.11912710.1063/1.119127 ↗
31. 10.1023/A:101125792816010.1023/A:1011257928160 ↗
32. 10.1143/JJAP.40.28510.1143/JJAP.40.285 ↗