Ammonium Persulfate and Potassium Oleate Containing Silica Dispersions for Chemical Mechanical Polishing for Cobalt Interconnect Applications
Source abstract
Abstract
We investigated the suitability of ammonium persulfate (APS) and potassium oleate (PO) containing silica dispersions for polishing Co interconnects based on removal and dissolution rates, corrosion, post-polish surface quality, and post-polish particle contamination. A slurry consisting of 3 wt% silica, 1 wt% APS and 0.2 mM PO produced a removal rate of ∼465 nm/min at pH 9, along with removal rate selectivity of >100:1 between Co and TiN. The same composition but without abrasives reduced the ΔEcorr between Co and TiN to ∼7 mV and Igc to ∼0.04 μAcm−2, indicating minimal galvanic corrosion. Addition of PO led to no measurable dissolution of the Co films. Surface analysis showed very good post-polish surface quality and minimal contamination with silica particles. These and results obtained with similar H2O2 containing slurries suggest that the APS and PO-based silica slurry is more suitable for the Co bulk CMP process. The roles of persulfates ions, pH, and PO on the removal process and passivation behavior of Co are discussed and a removal mechanism is proposed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Surface Polishing Techniques · Advanced materials and composites · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. 10.1016/j.sse.2004.10.01410.1016/j.sse.2004.10.014 ↗
2. 10.1149/2.029311jss10.1149/2.029311jss ↗
3. Simon A. H. Bolom T. Niu C. Baumann F. H. Hu C. K. Parks C. Nag J. Kim H. Lee J. Y. Yang C. C. , Electromigration Comparison of Selective CVD Cobalt Capping with PVD Ta(N) and CVD Cobalt Liners on 22nm-Groundrule Dual-Damascene Cu Interconnects. In IEEE International Reliability Physics Symposium Proceedings , IEEE, 2013, p 3F.4.1.10.1109/IRPS.2013.6532002 ↗
4. 10.1016/j.mee.2012.08.00810.1016/j.mee.2012.08.008 ↗
5. 10.1149/2.009312jes10.1149/2.009312jes ↗
6. 10.1016/j.mee.2011.04.01710.1016/j.mee.2011.04.017 ↗
7. 10.1146/annurev-matsci-082908-14541510.1146/annurev-matsci-082908-145415 ↗
8. Roberts J. M. Kaushik A. P. Clarke J. S. , Resistivity of Sub-30 Nm Copper Lines. In 2015 IEEE International Interconnect Technology Conference and 2015 IEEE Materials for Advanced Metallization Conference (IITC/MAM), IEEE, 2015, pp 341.10.1109/IITC-MAM.2015.7325595 ↗
9. Hosseini M. Koike J. Sutou Y. Zhao L. Lai S. Arghavani R. , Amorphous Co-Ti Alloy as a Single Layer Barrier for Co Local Interconnect Structure. In 2016 IEEE International Interconnect Technology Conference / Advanced Metallization Conference (IITC/AMC), IEEE, 2016, pp 162.10.1109/IITC-AMC.2016.7507718 ↗
10. Kamineni V. Raymond M. Siddiqui S. Mont F. Tsai S. Niu C. Labonte A. Labelle C. Fan S. Peethala B. Tungsten and Cobalt Metallization: A Material Study for MOL Local Interconnects. In 2016 IEEE International Interconnect Technology Conference / Advanced Metallization Conference (IITC/AMC), IEEE, 2016, pp 105.10.1109/IITC-AMC.2016.7507698 ↗
11. Bekiaris N. Wu Z. Ren H. Naik M. Park J. H. Lee M. Ha T. H. Hou W. Bakke J. R. Gage M. Cobalt Fill for Advanced Interconnects. In 2017 IEEE International Interconnect Technology Conference (IITC), IEEE, 2017, pp 1.10.1109/IITC-AMC.2017.7968981 ↗
12. Pedreira O. V. Croes K. Lesniewska A. Wu C. van der Veen M. H. Messemaeker J. de Vandersmissen K. Jourdan N. Wen L. G. Adelmann C. Reliability Study on Cobalt and Ruthenium as Alternative Metals for Advanced Interconnects. In 2017 IEEE International Reliability Physics Symposium (IRPS), IEEE, 2017, p 6B–2.1–6B–2.8.10.1109/IRPS.2017.7936340 ↗
13. Kelly J. Chen J. H.-C. Huang H. Hu C. K. Liniger E. Patlolla R. Peethala B. Adusumilli P. Shobha H. Nogami T. Experimental Study of Nanoscale Co Damascene BEOL Interconnect Structures. In 2016 IEEE International Interconnect Technology Conference / Advanced Metallization Conference (IITC/AMC), IEEE, 2016, pp 40.10.1109/IITC-AMC.2016.7507673 ↗
14. 10.1088/1361-6463/aa893410.1088/1361-6463/aa8934 ↗
15. Jezewski C. J. Clarke J. S. Indukuri T. K. Gstrein F. Zierath D. J. , Cobalt Based Interconnects and Methods of Fabrication Thereof. U.S. Pat. No. 9,514,983, December 6, 2016.
16. Doubina N. V. Rigsby M. A. Reid J. D. , Chemistry Additives and Process for Cobalt Film Electrodeposition. U.S. Pat. 9,777,386, October 3, 2017.
17. Shi X. Schlueter J. A. O'Neill M. L. , Chemical Mechanical Polishing (CMP) of Cobalt-Containing Substrate. U.S. Pat. Application No. US14/800,323, January 28, 2016.
18. 10.1016/j.mee.2008.11.04710.1016/j.mee.2008.11.047 ↗
19. 10.1016/j.mee.2014.02.00210.1016/j.mee.2014.02.002 ↗
20. 10.1149/07705.0093ecst10.1149/07705.0093ecst ↗
21. David L. , CRC Handbook of Chemistry and Physics, CRC press, 2008.
22. 10.1149/2.093403jes10.1149/2.093403jes ↗
23. 10.1149/2.073206jes10.1149/2.073206jes ↗
24. 10.1149/2.0171705jss10.1149/2.0171705jss ↗
25. Nishizawa H. Nojo H. Isobe A. , Fundamental Study of Chemical-Mechanical Polishing Slurry of Cobalt Barrier Metal for the next-Generation Interconnect Process, Japanese Journal of Applied Physics, 49 (5 PART 3) (2010).10.1143/JJAP.49.05FC03 ↗
26. 10.1149/2.017204esl10.1149/2.017204esl ↗
27. 10.1088/1674-4926/39/4/04600110.1088/1674-4926/39/4/046001 ↗
28. Sikma E. Paw W. Petro B. Cross J. Whitener G. , Slurry for Chemical Mechanical Polishing of Cobalt. U.S. Pat. No. 9,944,828, April 17, 2018.
29. Kraft S. Wolff A. Carter P. W. Hayes K. Petro B. , Cobalt Polishing Accelerators, U.S. Pat. No. 9,688,885, June 27, 2017.
30. 10.1149/2.0111709jss10.1149/2.0111709jss ↗
31. 10.1149/2.0251712jss10.1149/2.0251712jss ↗
32. 10.1016/S0169-4332(03)00272-110.1016/S0169-4332(03)00272-1 ↗
33. 10.1016/j.mee.2004.10.00810.1016/j.mee.2004.10.008 ↗
34. Li Y. , Microelectronic Applications of Chemical Mechanical Planarization, John Wiley & Sons, 2008.10.1002/9780470180907 ↗
35. 10.1149/2.023309jss10.1149/2.023309jss ↗
36. Effects of Liner Metal and CMP Slurry Oxidizer on Copper Galvanic Corrosion10.1149/1.2778386 ↗
37. 10.1016/j.matchemphys.2015.06.01710.1016/j.matchemphys.2015.06.017 ↗
38. Lu H. Qu X. Wang J. , Slurry for Chemical Mechanical Polishing of Cobalt. U.S. Pat. Application No. 13/813,699, June 6, 2013.
39. 10.1016/j.ultsonch.2009.11.01910.1016/j.ultsonch.2009.11.019 ↗
40. 10.1021/ie401690h10.1021/ie401690h ↗
41. 10.1016/j.jhazmat.2010.03.03910.1016/j.jhazmat.2010.03.039 ↗
42. 10.1149/2.0351709jss10.1149/2.0351709jss ↗
43. Reichardt R. Siebert M. Lan Y. Lauter M. Ibrahim S. A. U. Golzarian R. Guevenc H. O. Proelss J. Leunissen L. , Use of a Chemical Mechanical Polishing (CMP) Composition for Polishing of Cobalt and/or Cobalt Alloy Comprising Substrates. Application No. 15/538,334, December 28, 2017.
44. 10.1021/cm048478f10.1021/cm048478f ↗
45. 10.1149/1.139397910.1149/1.1393979 ↗
46. 10.1016/j.wear.2004.02.00710.1016/j.wear.2004.02.007 ↗
47. 10.1149/2.0171707jss10.1149/2.0171707jss ↗
48. 10.1063/1.55580810.1063/1.555808 ↗
49. 10.1063/1.55580510.1063/1.555805 ↗
50. 10.1016/j.cej.2014.02.10010.1016/j.cej.2014.02.100 ↗
51. 10.1016/j.apcatb.2003.12.01810.1016/j.apcatb.2003.12.018 ↗
52. 10.1021/es026379210.1021/es0263792 ↗
53. 10.1021/ie401690h10.1021/ie401690h ↗
54. 10.1016/S1001-0742(13)60598-710.1016/S1001-0742(13)60598-7 ↗
55. 10.1039/C5RA22457H10.1039/C5RA22457H ↗
56. 10.1016/j.jhazmat.2014.12.02610.1016/j.jhazmat.2014.12.026 ↗
57. 10.1023/A:100389312220110.1023/A:1003893122201 ↗
58. 10.1023/A:102656042209010.1023/A:1026560422090 ↗
59. 10.1021/am201011410.1021/am2010114 ↗
60. 10.1021/la104257k10.1021/la104257k ↗
61. 10.1016/j.jallcom.2009.12.10310.1016/j.jallcom.2009.12.103 ↗
62. Babu S. V. Seo J. Vegi S. S. R. K. H. , System and Method for Identification of Contamination of Cobalt CMP Slurry. US Pat. Pending App. No. 62/726,242, September 1, 2018.