journal article·2020-12Open access

Low melting point solders based on Sn, Bi, and In elements

Y. Liu, K.N. Tu

Abstract

In the big data era, Si chips are integrated more and more to satisfy the fast growing demand from customers. In addition, in the post-COVID-19 virus era, the trend of distance teaching and home office has increased greatly the need of advanced consumer electronic products. To provide more processing tolerance and to build a wider temperature window in manufacturing, it becomes necessary to develop low melting temperature solders because a hierarchy of solders is needed in the packaging technology. Much research has been on Pb-free and Sn-based solders with a melting point from 180 to 230 °C. In this review, we will concentrate on low melting point solder alloys with a melting point lower than 180 °C and even below 100 °C. We review eutectic SnBi, eutectic SnIn, and the alloys with trace addition of a third element to them. Eutectic Sn-Bi solder is too brittle, and Sn-In solder is too soft. However, third element addition can only improve the solder properties partially; thus, we will further review the properties of Sn-Bi-In ternary alloys and the effect on the addition of a fourth element to them. This approach, when we include the Cu substrate, becomes a 5-element system, which leads us to consider high entropy alloys for soldering. With these Sn-, Bi-, and In-based alloys, we hope to develop new ways to design industrial applicable low melting point solders.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Additive Manufacturing Materials and Processes · Adhesion, Friction, and Surface Interactions

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. Material innovation opportunities for 3D integrated circuits from a wireless application point of view10.1557/mrs.2015.9 ↗
2. Effect of Joule heating and current crowding on electromigration in mobile technology10.1063/1.4974168 ↗
3. Scaling effect of interfacial reaction on intermetallic compound formation in Sn/Cu pillar down to 1 μm diameter10.1016/j.actamat.2016.07.004 ↗
4. Synergistic effect of electromigration and Joule heating on system level weak-link failure in 2.5 D integrated circuits10.1063/1.4932598 ↗
5. Thermomechanical behaviour of environmentally benign Pb-free solders10.1179/174328009X461069 ↗
6. A review: on the development of low melting temperature Pb-free solders10.1016/j.microrel.2014.02.025 ↗
7. Intermetallic compound growth suppression at high temperature in SAC solders with Zn addition on Cu and Ni–P substrates10.1016/j.jallcom.2011.09.024 ↗
8. Reliability challenges in 3D IC packaging technology10.1016/j.microrel.2010.09.031 ↗
9. A comprehensive reliability study on a CoWoS 3D IC package
10. Package on Package warpage-impact on surface mount yields and board level reliability
11. A study of Sn-Bi-Ag-(In) lead-free solders10.1023/A:1022822127193 ↗
12. Comparison of interfacial reactions of Ni and Ni–P in extended contact with liquid Sn–Bi-based solders10.1016/j.actamat.2006.09.003 ↗
13. Skin electronics from scalable fabrication of an intrinsically stretchable transistor array10.1038/nature25494 ↗
14. Multifunctional materials for implantable and wearable photonic healthcare devices
15. Nanowired bioelectric interfaces: focus review10.1021/acs.chemrev.8b00795 ↗
16. Precision electronic medicine in the brain10.1038/s41587-019-0234-8 ↗
17. Creating functional interfaces with biological circuits10.1021/acs.accounts.8b00167 ↗
18. Characterization of eutectic Sn-Bi solder joints10.1007/BF02655427 ↗
19. Effects of minor Cu and Zn additions on the thermal, microstructure and tensile properties of Sn–Bi-based solder alloys10.1016/j.jallcom.2014.06.015 ↗
20. Effect of silver and indium addition on mechanical properties and indentation creep behavior of rapidly solidified Bi-Sn based lead-free solder alloys10.1016/j.msea.2012.09.038 ↗
21. Effects of trace amounts of rare earth additions on microstructure and properties of Sn-Bi-based solder alloy10.1007/s11664-008-0458-8 ↗
22. Eutectic Sn–Bi as an alternative Pb-free solder
23. Interfacial reactions between molten Sn–Bi–X solders and Cu substrates for liquid solder interconnects10.1016/j.actamat.2006.02.030 ↗
24. Kinetic analysis of the soldering reaction between eutectic SnPb alloy and Cu accompanied by ripening10.1103/PhysRevB.53.16027 ↗
25. Activation energies of intermetallic growth of Sn-Ag eutectic solder on copper substrates10.1007/s11664-997-0268-4 ↗
26. Selective interfacial reaction between Ni and eutectic BiSn lead-free solder10.1021/cm000803l ↗
27. Long-term aging study on the solid-state reaction between 58Bi42Sn solder and Ni substrate10.1007/s11664-000-0013-8 ↗
28. Bi-induced voids at the Cu3Sn/Cu interface in eutectic SnBi/Cu solder joints10.1016/j.scriptamat.2007.10.025 ↗
29. Coarsening kinetics of Ni3Sn4 scallops during interfacial reaction between liquid eutectic solders and Cu/Ni/Pd metallization10.1063/1.1321791 ↗
30. Self-diffusion in liquid tin10.1063/1.1732419 ↗
31. Growth kinetics of intermetallic phases at the liquid Sn and solid Ni interface10.1016/0036-9748(80)90338-5 ↗
32. Eutectic Sn-Bi as an alternative to Pb-free solders
33. Comparison of electroplated eutectic Bi/Sn and Pb/Sn solder bumps on various UBM systems10.1109/6104.980035 ↗
34. The effect of aging on microstructure, room temperature deformation, and fracture of Sn-Bi/Cu solder joints10.1007/BF02653346 ↗
35. Residual shear strength of Sn-Ag and Sn-Bi lead-free SMT joints after thermal shock10.1109/6040.883762 ↗
36. Drop reliability of epoxy-contained Sn-58 wt.% Bi solder joint with ENIG and ENEPIG surface finish under temperature and humidity test10.1007/s11664-016-4517-2 ↗
37. Electromigration-induced Bi segregation in eutectic SnBi solder joint10.1007/s11664-006-0025-0 ↗
38. Electromigration study in the eutectic SnBi solder joint on the Ni/Au metallization[J]10.1557/jmr.2006.0113 ↗
39. Thermal cycling test in Sn-Bi and Sn-Bi-Cu solder joints10.1023/A:1008928729212 ↗
40. Wettability of molten Sn-Bi-Cu solder on Cu substrate10.1016/j.matlet.2009.06.052 ↗
41. Effects of a third element on microstructure and mechanical properties of eutectic Sn-Bi solder10.5104/jiepeng.2.98 ↗
42. Effect of In on microstructure, thermodynamic characteristic and mechanical properties of Sn-Bi based lead-free solder10.1016/j.jallcom.2015.01.219 ↗
43. Effects of In and Ni addition on microstructure of Sn-58Bi solder joint10.1007/s11664-014-3359-z ↗
44. Interactions between liquid Sn-Bi based solders and contact metals for high temperature applications
45. Properties and microstructures of Sn-AgCu-X lead-free solder joints in electronic packaging10.1155/2015/639028 ↗
46. Electro-migration study of nano Al doped lead- free Sn-58Bi on Cu and Au/Ni/Cu ball grid array (BGA) packages
47. Effects of Zn addition on mechanical properties of eutectic Sn-58Bi solder during liquid-state aging10.1016/S1003-6326(15)63719-0 ↗
48. Effects of Zn concentration on the aging reactions and IMC massive spalling phenomenon in the Sn–58Bi–xZn/Cu system10.1007/s10854-014-2544-4 ↗
49. Microstructure, thermal and wetting properties of Sn-Bi-Zn lead-free solder10.1007/s11664-013-2620-1 ↗
50. Microstructures and properties of Sn58Bi, Sn35Bi0.3Ag, Sn35Bi1.0Ag solder and solder joints10.1007/s10854-015-3400-x ↗
51. Effect of Sb content on properties of Sn-Bi solders10.1016/S1003-6326(14)63046-6 ↗
52. Effect of La addition on the interfacial intermetallics and bonding strengths of Sn-58Bi solder joints with Au/Ni/Cu pads10.1016/j.jallcom.2009.11.017 ↗
53. Effects of Co alloying and size on solidification and interfacial reactions in Sn-57 wt.%Bi-(Co)/Cu couples10.1007/s11664-010-1386-y ↗
54. Effective suppression of interfacial intermetallic compound growth between Sn–58 wt.% Bi solders and Cu substrates by minor Ga addition10.1016/j.jallcom.2013.10.035 ↗
55. Microstructure and mechanical properties of Sn-In and Sn-Bi solders10.1007/BF03222376 ↗
56. Binary alloy phase diagrams
57. Low temperature fluxless bonding technique using In-Sn composite
58. Crystallization, decomposition and superconductivity of β-In3Sn10.1016/0022-5088(79)90116-4 ↗
59. Properties of solders with low melting point10.1016/j.jallcom.2007.03.062 ↗
60. Microstructure and creep of eutectic indium/tin on copper and nickel substrates10.1007/BF02655434 ↗
61. Rapid thermal cycling of three phase change materials (PCMs) for cooking applications10.1007/s40430-018-1253-y ↗
62. Influence of silver on structural, electrical, mechanical and soldering properties of tin-indium based alloys10.1080/10420150410001670288 ↗
63. Interface reaction systematics in the Cu/In–48Sn/Cu system bonded by diffusion soldering10.1016/j.intermet.2006.10.050 ↗
64. The interfacial reaction between In-48Sn solder and polycrystalline Cu substrate during solid state aging10.1016/j.jallcom.2017.12.355 ↗
65. Interfacial reactions and growth kinetics for intermetallic compound layer between In–48Sn solder and bare Cu substrate10.1016/j.jallcom.2004.05.055 ↗
66. Intermetallic compound layer formation between copper and hot-dipped 100In, 50In-50Sn, 100Sn, and 63Sn-37Pb coatings10.1007/BF02653343 ↗
67. Phase identification and growth kinetics of the intermetallic compounds formed during In-49Sn/Cu soldering reactions10.1007/s11664-002-0136-1 ↗
68. Reliability of In-48Sn solder/Au/Ni/Cu BGA packages during reflow process10.1007/s11664-005-0166-6 ↗
69. Indium solders
70. Microstructural development of eutectic Bi-Sn and eutectic In-Sn during high temperature deformation10.1007/BF02671233 ↗
71. Solder joint reliability of indium-alloy interconnection10.1007/BF02659725 ↗
72. Diffusion in indium near the melting point
73. Self-diffusion in tin single crystals
74. Self-diffusion in tin at high pressure10.1021/j100790a032 ↗
75. Thermal fatigue behaviour of low melting point solder joints10.1108/eb037812 ↗
76. Fatigue of solders
77. Reliable bonding using indium-based solders
78. Characterization of the shear test method with low melting point In–48Sn solder joints10.1016/j.msea.2005.02.040 ↗
79. Effect of surface finish of substrate on mechanical reliability of In-48Sn solder joints in MOEMS package10.1007/s00542-006-0344-3 ↗
80. Interfacial reactions and mechanical properties of In–48Sn solder joint with electroplated Au/Ni ball grid array (BGA) substrate after multiple reflows10.1557/JMR.2008.0223 ↗
81. Current-induced phase partitioning in eutectic indium-tin Pb-free solder interconnect10.1007/s11664-007-0206-5 ↗
82. Phase segregation, interfacial intermetallic growth and electromigration-induced failure in Cu/In–48Sn/Cu solder interconnects under current stressing10.1016/j.jallcom.2016.02.244 ↗
83. Electromigration in eutectic In-48Sn ball grid array (BGA) solder interconnections with Au/Ni/Cu pads10.1007/s10854-015-3524-z ↗
84. Hansen · 1958
85. Microstructure and mechanical properties of the In–48Sn–xAg low-temperature alloy
86. Effect of zinc addition on the microstructure, thermal and mechanical properties of indium-tin-xZinc alloys10.1007/s11664-018-6768-6 ↗
87. Effects of zinc on the interfacial reactions of tin–indium solder joints with copper10.1007/s10853-014-8092-8 ↗
88. Solid-state reactions between Sn-20.0 wt.%In-x wt.%Zn solders and Ag and Ni substrates10.1016/j.matchemphys.2015.01.045 ↗
89. Phase relationships in Bi–In–Sn alloy system10.1179/mst.1986.2.10.985 ↗
90. Thermodynamic re-optimisation of the Bi–In–Sn system based on new experimental10.1016/j.jallcom.2006.03.050 ↗
91. In situ observation of microstructure evolution in low-melting Bi–In–Sn alloys by light microscopy10.1016/j.actamat.2005.04.015 ↗
92. Low-temperature solders
93. Investigation of the phase equilibria in the Sn-Bi-In alloy system10.1007/s11661-999-0087-8 ↗
94. Microstructure and mechanical behavior of low-melting point Bi-Sn-In solder joints10.1007/s13391-017-1614-1 ↗
95. Interfacial microstructure and mechanical properties of In–Bi–Sn lead-free solder10.1007/s10854-013-1143-0 ↗
96. Characteristic of low temperature of Bi-In-Sn solder alloy
97. Characterization of In-based eutectic alloys used in Josephson packaging10.1007/BF02644794 ↗
98. Characterization of intermetallic compound formation on In/Bi/Sn solder bumps used in Pb-alloy Josephson chip packaging10.1109/TCHMT.1987.1134729 ↗
99. Phase evolution of superconducting Sn–In–Bi solder alloys10.1109/TASC.2016.2514843 ↗
100. The effect of growth rate on microstructure and microindentation hardness in the In–Bi–Sn ternary alloy at low melting point10.1016/j.jallcom.2008.02.056 ↗