journal article·2008-10

A tannic acid/ferrous sulfate aftertreatment for dyed nylon 6,6

S.M. Burkinshaw, N. Kumar

Dyes and Pigments· Volume 79· Issue 1
Publisher page

Abstract

Both a single-stage and a two-stage aftertreatment using tannic acid in conjunction with ferrous sulfate improved the fastness to repeated washing at 60 °C of two acid dyes on nylon 6,6 most likely via the formation of a low solubility, large molecular size, iron tannate complex within the periphery of the dyed fibre. The iron tannate complex imparted a slight greyish-brown colour to dyeings, although this did not affect the λmax of the dyeings and also increased the colour strength of the dyeings. Neither the single-stage nor the two-stage aftertreatment affected the light fastness of dyeings but both aftertreatments reduced rub fastness.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Dyeing and Modifying Textile Fibers · Cultural Heritage Materials Analysis · melanin and skin pigmentation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (6)

Show source-provided references
1. Burkinshaw · 1995
2. The aftertreatment of acid dyes on nylon 6,6 fibres. Part 1 – 1:2 Pre-metallised acid dyes10.1016/S0143-7208(00)00077-2 ↗
3. The development of a metal-free, tannic acid-based aftertreatment for nylon 6,6 dyed with acid dyes. Part 3 – Different enzymes
4. The development of a metal-free, tannic acid-based aftertreatment for nylon 6,6 dyed with acid dyes. Part 1 – Initial studies10.1016/S0143-7208(03)00046-9 ↗
5. 1990
6. Nikolaides N, personal communication.