The stability of offset inks on paper upon ageing
Source abstract
Abstract
The standard moist heat (80 °C and 65% relative humidity) and dry heat (105 °C) techniques of accelerated paper ageing were applied in stability investigations of offset ink films printed on alkaline offset paper. The measured characteristics of paper sample evidenced its first-class mechanical properties, large alkali reserve, in addition to high values of brightness and opacity. The pseudoplastic flow behaviour was established for original offset CMYK printing inks by rheological measurements. The results obtained, following application of both ageing procedures, revealed the significant exponential decrease of relative optical density for MAGENTA and YELLOW ink layers. The variance in visible reflectance spectra and in total colour difference ΔE* (L*a*b* CIE) of ink films evidenced the considerable damage of CYAN and YELLOW ink films, especially upon moist heat treatment. The differences in lightness ΔL* play the dominant role in ΔE* values of BLACK ink films upon both ageing procedures. The FT-IR spectroscopy was additionally used in the characterization of paper, inks, as well as ink films on paper before and after ageing.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Cultural Heritage Materials Analysis · Material Properties and Processing · Advanced Cellulose Research Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Porck · 1996
2. Near-UV and visible pulsed laser interaction with paper10.1016/S1296-2074(00)00149-7 ↗
3. Near-UV, visible and IR pulsed laser light interaction with cellulose10.1007/PL00021097 ↗
4. Browning · 1977
5. Ink corrosion aqueous and non aqueous treatment of paper objects—state of the art10.1515/rest.1999.20.3-4.167 ↗
6. Derivative infrared spectroscopy and electron spectroscopy for chemical analysis of ancient paper documents
7. Phytate10.1515/rest.1995.16.3.143 ↗
8. Hoel IAL. Standards for permanent paper. In: 64th IFLA General Conference, 16–21 August 1998. Conference Programme and Proceedings 115–114-E. Available from: (http://www.ifla.org/IV/ifla64/115–114e.htm).
9. Walne P. Selected guidelines for the management of records and archives: a RAMP reader. Paris: Unesco, 1990 [PGI-90/WS/6]. Available from: http://www.unesco.org/webworld/ramp/html/r9006e00.htm.
10. The stability of printing inks10.1515/rest.1993.14.3.141 ↗
11. Overview of the lightfastness of commercial printing inks
12. Overview of the lightfastness of commercial printing inks. Part II: Influence of solar and fluorescent light
13. Chromatographic and electrophoretic approaches in ink analysis10.1016/S0378-4347(99)00312-6 ↗
14. The effect of ink types and printing processes on floatation deinking efficiency of wastepaper recycling10.1007/s100220050005 ↗
15. Ink receptivity on paper—characterization of paper materials10.1016/S0927-7757(00)00489-1 ↗
16. Viscosity measurement of viscoelastic inks at high shear rates
17. Tollenaar · Adv. Print. Sci. Technol · 1962 · 2 · 214
18. Hummel · 1991
19. Investigations of paper aging—a search for archive paper10.1023/A:1013696127691 ↗
20. The chemistry of paper preservation. T 2. The yellowing of paper and conservation bleaching10.1021/ed073p1068 ↗
21. New colourimetric method for determination of hydroxyl radicals during ageing of cellulose10.1016/S0003-2670(00)01322-2 ↗
22. Effect of metals on paper
23. The hydrogen bond network in Iβ cellulose as observed by infrared spectroscopy10.1016/S0022-2860(99)00389-0 ↗
24. Proniewicz · J. Mol. Struct. · 2001 · 596 · 16310.1016/S0022-2860(01)00706-2 ↗
25. Spectroscopic studies of the ageing of cellulosic paper10.1016/S0032-3861(00)00691-1 ↗