Magnetic characterization of nanocrystalline iron samples with different size distributions
Source abstract
Abstract
Abstract Nanocrystalline iron was obtained by fusing magnetite and promoters. The oxidized form was reduced with hydrogen and passivated (sample P0). The average nanocrystallite size in sample P0 was d(P0) =16 nm and the width of size distribution was σ(P0) = 18 nm. Samples of nanocrystalline iron with narrower diameter ranges and larger and smaller average crystallite sizes were also synthesized. They were: sample P1 (d(P1) = 28 nm, σ(P1) = 5 nm), sample P2 (d(P2) = 22 nm, σ(P1) = 5 nm), sample P3 (d(P3) = 12 nm, σ(P1) = 9 nm). These four samples were studied at room temperature by dc magnetization measurements and ferromagnetic resonance at microwave frequency. Correlations between samples sizes distributions (average size and width of the sizes) and magnetic parameters (effective magnetization, anisotropy field, anisotropy constant, FMR linewidth) were investigated. It was found that the anisotropy field and effective magnetization determined from FMR spectra scale linearly with nanoparticle sizes, while the effective magnetic anisotropy constant determined from the hysteresis loops decreases with nanoparticle size increase.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnetic Properties and Synthesis of Ferrites · Metallic Glasses and Amorphous Alloys · Magnetic properties of thin films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute of Physics, West Pomeranian University of Technology, 48 Piastow Str., 70-311, Szczecin, Poland
Institute of Chemical and Environment Engineering, West Pomeranian University of Technology, 10 Pulaskiego Str., 70-322, Szczecin, Poland
References
Reference metadata was not supplied for this record.