Processing and microwave dielectric properties of Sr5Ta4TiO17 ceramics
Source abstract
Abstract
Abstract Sr5Ta4TiO17 ceramics was processed via solid state mixed oxide sintering route. X-ray diffraction revealed single phase formation of Sr5Ta4TiO17 ceramics that crystallized into an orthorhombic crystal structure with a space group Pnnm with lattice parameters of a = 5.681 Å, b = 32.542 Å and c = 3.968 Å, refined by the least squares method. The unit cell density (ρth) was 6.71 g/cm3. The microstructure consisted of plate-like grains and the average size was increased from 2 μm to 5 μm with an increase in sintering temperature from 1450 °C to 1575 °C. Optimum microwave dielectric properties, i.e. єr ~ 66,Qufo ~ 8500 GHz and τf ~ 180 ppm/°C, were achieved for Sr5TaTiO17 ceramics sintered at 1550 °C for 4 h.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Ferroelectric and Piezoelectric Materials · Dielectric properties of ceramics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Laboratory for Research in Advanced Materials, Department of Physics, University of Science and Technology Bannu, 28100, Khyber Pakhtunkhwa , Pakistan
2 Departments of Physics, Islamia College Peshawar, 25120, Khyber Pakhtunkhwa , Pakistan
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, School of Materials Science and Engineering, Wuhan University of Technology, Wuhan , 430070, China
Department of Civil Engineering, International Islamic University Islamabad , Pakistan
References (22)
Show source-provided references
1. [1] REANEY I.M., IDLES D., J. Am. Ceram. Soc., 89 (2006), 2068.
2. [2] IQBAL Y., MANAN A., REANEY I.M., Mater. Res. Bull., 46 (2011), 1092.10.1016/j.materresbull.2011.03.002 ↗
3. [3] CHEN Y.C., ZENG Y.W., Opt. Tech. Lett., 51 (2009), 98.10.1002/mop.24437 ↗
4. [4] CHEN Y.C., YAO S.H., TASI R. J., CHEN K.C., J. Alloy. Compd., 486 (2009), 410.10.1016/j.jallcom.2009.06.189 ↗
5. [5] IQBAL Y., MANAN A., REANEY I.M., Mater. Res. Bull., 46 (2011), 1092.10.1016/j.materresbull.2011.03.002 ↗
6. [6] JAWAHAR I.N., SANTHA N., SEBASTIAN M.T., MOHANANE P., J. Mater. Res., 17 (2002), 3084.10.1557/JMR.2002.0446
7. [7] ZHAO F., YUE Z., GUI Z., LI L., J. Am. Ceram. Soc., 89 (2006), 3421.10.1111/j.1551-2916.2006.01236.x ↗
8. [8] CHEN Y.C., TSAI J.M., Jpn. J. Appl. Phys., 47 (2008), 7959.10.1143/JJAP.47.1683 ↗
9. [9] ISUPOV V.A., SMIRNOVA P., ISUPOVA E. N., ZAITSEVAN V., PIKUSHL G., SMOLENSGK G.A., Sov. Phys. Solid State., 18 (1976), 835.10.1016/0038-1098(76)90217-9 ↗
10. [10] IQBAL Y., REANEY I.M., Ferroelectrics, 302 (2004), 259.10.1080/00150190490454990 ↗
11. [11] IQBAL Y., MANAN A., J. Electon. Mater., 41 (2012), 2394.
12. [12] FANG L., WU M., LIU Q., TANG Y., ZHOU H., ZHANG H., Mater. Chem. Phys., 136 (2012), 599.10.1016/j.matchemphys.2012.07.032 ↗
13. [13] MANAN A., QAZI I., ULLAH A., J. Electon. Mater., 42 (2013), 138.
14. [14] BIJUMON P.V., MOHANAN P., SEBASTIAN M.T., Mater. Lett., 57 (2003), 1380.10.1016/S0167-577X(02)00991-6 ↗
15. [15] OGAWA H., KAN A., ISHIHARA S., HIGASHIDA Y., J. Eur. Ceram. Soc., 23 (2003), 2485.10.1016/S0955-2219(03)00167-5
16. [16] SHANNON R.D., Acta Crystallogr. A, 32 (1976), 751.10.1107/S0567739476001551
17. [17] MANAN A., HUSSAIN I., Int. J. Modern Phys. B, 28 (2014), 1450092.10.1142/S0217984914500924 ↗
18. [18] SHANNON R.D., J. Appl. Phys., 73 (1993), 348.10.1063/1.353856 ↗
19. [19] RATHEESH R., WOHLECKE M., BERGE B., WAHLBRINK T., HAEUSELER H., RUHI E., BLACHNIK R., BALAN P., SANTHA N., SEBASTIAN M.T., J. Appl. Phys., 88 (2000), 2813.10.1063/1.1287762
20. [20] XIA W.S., ZHANG L.Y., WANG Y., JIN S.E., XU Y.P., ZUO Z.W., SHI L.W., J. Mater. Sci. Mater. El., 27 (2016), 11325.10.1007/s10854-016-5256-0
21. [21] REANEY I.M., COLLA E.L., SETTER N., Jpn. J. Appl. Phys., 33 (1994), 3984.10.1143/JJAP.33.3984 ↗
22. [22] HARROP P., J. Mater. Sci., 4 (1969), 370.10.1007/BF00550407