Influences of lattice strain and SiGe buffer layer thickness on electrical characteristics of strained Si/SiGe/Si(110) heterostructures
Source abstract
Abstract
In previous studies, we reported on significantly high hole mobility in a strained Si/SiGe/Si(110) heterostructure pMOSFET. In this study, we investigated impact of strain on the hole mobility in this structure. 20-nm thick (110)-oriented strained Si films with different strain levels were formed using solid-source molecular beam epitaxy. A positive correlation between the hole mobility and the strain of the Si layer is verified. It is also shown that formation of growth twins and strain relaxation of SiGe layer in the [ 1 ‾ 10 ] direction deteriorate the hole mobility. The maximum mobility enhancement factor obtained in this study is about 3. In addition, the influence of the SiGe layer thickness on the off-state leakage current in pMOSFET operation is discussed. It is found that the upper part of the thick SiGe samples includes cause of the leakage current, indicating change of conductivity with the progress of the crystal growth of SiGe layer. This phenomenon is related to the formation process of the crystalline defects. Another finding is the existence of a current path through the substrate, which suggests a defect-assisted current flow across the SiGe/n-Si(110) junction.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Semiconductor materials and devices · Advancements in Semiconductor Devices and Circuit Design · Silicon Carbide Semiconductor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Monte Carlo study of apparent mobility reduction in nano-MOSFETs
2. Ballistic mobility degradation in scaled-down channel of a MOSFET
3. The Channel mobility degradation in a nanoscale metal–oxide–semiconductor field effect transistor due to injection from the ballistic contacts10.1063/1.3554623 ↗
4. Mobility degradation in a nano-MOSFET due to ballistic and high-field effects
5. Balestra · 2013
6. 110)-Surface strained-SOI CMOS Devices with higher carrier mobility
7. High performance CMOS fabricated on hybrid substrate with different crystal orientations
8. 1.5-Nm gate oxide CMOS on [110] surface-oriented Si substrate10.1109/TED.2003.812085 ↗
9. 110)-Surface strained-SOI CMOS devices10.1109/TED.2005.843894 ↗
10. Very high carrier mobility for high-performance CMOS on a Si(110) surface10.1109/TED.2007.896372 ↗
11. Understanding of strain effects on high-field carrier velocity in (100) and (110) CMOSFETs under quasi-ballistic transport
12. Hole mobility enhancement observed in (110)-oriented strained Si10.7567/1347-4065/ab6591 ↗
13. Engineering strain, defects, and electronic properties of (110)-oriented strained Si10.1149/09805.0277ecst ↗
14. Stability of strain in Si layers formed on SiGe/Si(110) heterostructures10.1088/1361-6641/aaeb10 ↗
15. Relaxation of strain in Si layers formed on (110)-oriented SiGe/Si heterostructures10.1149/09301.0079ecst ↗
16. Hole mobility in strained Si/relaxed SiGe/Si(110) heterostructures studied by gated Hall measurements10.1016/j.mssp.2020.105052 ↗
17. Dependences of the hole mobility in the strained Si PMOSFET and gated Hall bars formed on SiGe/Si(1 1 0) on the channel direction and the strained Si thickness10.1016/j.jcrysgro.2021.126246 ↗
18. Growth of strained Si/relaxed SiGe heterostructures on Si(110) substrates using solid-source molecular beam epitaxy10.1088/1361-6641/aa8a87 ↗
19. Strain relaxation process and evolution of crystalline morphologies during the growths of SiGe on Si(110) by solid-source molecular beam epitaxy10.1016/j.mssp.2020.105042 ↗
20. Taur · 2021
21. Structural, electronic, and luminescence investigation of strain‐relaxation induced electrical conductivity type conversion in GeSi/Si heterostructures10.1063/1.363200 ↗
22. Acceptorlike behavior of defects in SiGe alloys grown by molecular beam epitaxy10.1143/JJAP.47.4630 ↗
23. Hole generation associated with intrinsic defects in SOI-based SiGe thin films formed by solid-source molecular beam epitaxy10.1063/1.5004077 ↗