Effects of direct aging on precipitation behavior, mechanical properties and thermal conductivity of an Mg-3Al-5Zn-3Ca alloy
Source abstract
Abstract
This work reveals the precipitation behavior in an Mg-3Al-5Zn-3Ca alloy during isothermal aging (without prior solution treatment) and its effects on mechanical properties and thermal conductivity. Significant precipitation of micro-scale C15-Al 2 Ca Laves phase occurs within the grains only when the temperature reaches 350 °C. During the initial aging stage, the precipitation fraction, number density, and size increase with aging time, while the solute-enriched zones near the grain boundary Ca-containing second phases are gradually consumed by nearby precipitation. Peak aging is achieved after 20 h. Upon further aging to 60 h, the volume fraction and average size of the precipitates continue to increase, exhibiting a balanced combination of properties. Dissolution of the grain boundary phases and precipitates occurred after 100 h.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Nanchang Hangkong University
Funding
Natural Science Foundation of Jiangxi Province · National Natural Science Foundation of China
References (39)
Show source-provided references
1. 10.1016/j.jma.2019.08.00110.1016/j.jma.2019.08.001 ↗
2. 10.1080/02670836.2019.160390110.1080/02670836.2019.1603901 ↗
3. 10.1016/j.jma.2023.09.01510.1016/j.jma.2023.09.015 ↗
4. 10.1016/j.jallcom.2021.16253910.1016/j.jallcom.2021.162539 ↗
5. 10.1016/j.jallcom.2015.12.05710.1016/j.jallcom.2015.12.057 ↗
6. 10.1007/s00170-007-1279-210.1007/s00170-007-1279-2 ↗
7. 10.1080/02670836.2023.218605510.1080/02670836.2023.2186055 ↗
8. 10.1179/1743284713Y.000000040110.1179/1743284713Y.0000000401 ↗
9. 10.1016/j.jma.2024.02.00710.1016/j.jma.2024.02.007 ↗
10. 10.1016/j.jmrt.2023.09.00910.1016/j.jmrt.2023.09.009 ↗
11. 10.1016/j.matdes.2022.11147010.1016/j.matdes.2022.111470 ↗
12. 10.1016/j.actamat.2012.01.01710.1016/j.actamat.2012.01.017 ↗
13. 10.1016/j.ijplas.2025.10429510.1016/j.ijplas.2025.104295 ↗
14. 10.1016/j.jma.2019.08.00210.1016/j.jma.2019.08.002 ↗
15. 10.1016/j.jallcom.2022.16801410.1016/j.jallcom.2022.168014 ↗
16. 10.1016/j.jmrt.2023.03.05310.1016/j.jmrt.2023.03.053 ↗
17. 10.1016/j.msea.2017.07.06010.1016/j.msea.2017.07.060 ↗
18. 10.1016/j.msea.2023.14476510.1016/j.msea.2023.144765 ↗
19. 10.1016/j.jallcom.2024.17772810.1016/j.jallcom.2024.177728 ↗
20. 10.1016/j.actamat.2005.03.00110.1016/j.actamat.2005.03.001 ↗
21. 10.1016/j.jallcom.2015.06.06010.1016/j.jallcom.2015.06.060 ↗
22. 10.1016/j.jallcom.2023.17329910.1016/j.jallcom.2023.173299 ↗
23. 10.1016/j.jallcom.2013.03.18410.1016/j.jallcom.2013.03.184 ↗
24. 10.1016/j.jma.2020.11.02010.1016/j.jma.2020.11.020 ↗
25. Yuan J, Li Y, Li X, et al. Homogenizing heat treatment and thermal conductivity of Mg-4Zn-1Mn magnesium alloy. Trans Mater Heat Treat 2012; 33: 27–32.
26. 10.1016/S0921-5093(02)00233-210.1016/S0921-5093(02)00233-2 ↗
27. 10.1080/14786435.2017.131456210.1080/14786435.2017.1314562 ↗
28. 10.1016/j.jallcom.2016.05.26110.1016/j.jallcom.2016.05.261 ↗
29. 10.1016/j.scriptamat.2008.10.02210.1016/j.scriptamat.2008.10.022 ↗
30. 10.1016/j.jmst.2017.12.01110.1016/j.jmst.2017.12.011 ↗
31. 10.1016/j.jallcom.2025.18084310.1016/j.jallcom.2025.180843 ↗
32. Liu M, Sun M, Li J, et al. Research progress on discontinuous precipitation modification of Mg-Al alloy. Nonferrous Metal Mater Eng 2020; 41: 39–47.
33. 10.1016/j.matdes.2018.10755410.1016/j.matdes.2018.107554 ↗
34. 10.1016/j.jallcom.2014.02.02910.1016/j.jallcom.2014.02.029 ↗
35. 10.1016/j.mtcomm.2025.11254510.1016/j.mtcomm.2025.112545 ↗
36. 10.1016/j.msea.2024.14658810.1016/j.msea.2024.146588 ↗
37. 10.1016/j.jallcom.2022.16739210.1016/j.jallcom.2022.167392 ↗
38. 10.1016/j.jallcom.2020.15557310.1016/j.jallcom.2020.155573 ↗
39. 10.1177/0267083625131582810.1177/02670836251315828 ↗