journal article·2003-09

Effect of oxidation on flexural strength of liquid phase sintered SiC with AlN and Er2O3additives between 1200°C and 1400°C

S. Guo, N. Hirosaki, H. Tanaka, Y. Yamamoto, T. Nishimura

Materials Science and Technology· Volume 19· Issue 9
Publisher page

Abstract

The effect of oxidation on the room temperature flexural strength of liquid phase sintered SiC with AlN and Er2O3 additives exposed to air between 1200°C and 1400°C, for up to 200 h, was investigated. After oxidation, the room temperature flexural strength of the material increased, and was dependent on exposure temperature. After 200 h exposure at 1200°C, 1300°C, and 1400°C, increases of approximately 2%, 10% and 40%, respectively, were obtained. The increase in the flexural strength was associated with the decrease of stress concentration induced by processing defects at the surface and/or a subsurface.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. 10.1111/j.1151-2916.1983.tb10084.x10.1111/j.1151-2916.1983.tb10084.x ↗
2. 10.1111/j.1151-2916.1994.tb04637.x10.1111/j.1151-2916.1994.tb04637.x ↗
3. 10.1557/JMR.1996.020010.1557/JMR.1996.0200 ↗
4. 10.1111/j.1151-2916.1994.tb07024.x10.1111/j.1151-2916.1994.tb07024.x ↗
5. 10.1016/S0955-2219(97)00163-510.1016/S0955-2219(97)00163-5 ↗
6. 10.1557/JMR.1991.194510.1557/JMR.1991.1945 ↗
7. 10.1111/j.1151-2916.2001.tb00958.x10.1111/j.1151-2916.2001.tb00958.x ↗
8. 10.1111/j.1151-2916.2002.tb00211.x10.1111/j.1151-2916.2002.tb00211.x ↗
9. 10.1111/j.1151-2916.2002.tb00319.x10.1111/j.1151-2916.2002.tb00319.x ↗
10. GUO S. Q. · Philos. Mag. A · 2002 · 82 · 3027