Investigation of mechanism of cleavage fracture initiation in intercritically coarse grained heat affected zone of HSLA steel
Source abstract
Abstract
The degradation of the fracture toughness of high strength low alloy steels is attributed to the formation of ‘local brittle zones’ in the welded joint. These local brittle zones are mainly located within the coarse grained heat affected zone (CGHAZ) and the intercritically reheated CGHAZ (ICCGHAZ). Cracking and debonding of M-A constituents from the surrounding matrix are generally accepted as initiation events of fracture in the ICCGHAZ. In the present work, the low temperature fracture toughness of X80 pipeline steel was examined. The main purposes were (i) to evaluate possible crack initiation sites of cleavage fracture and (ii) to identify the mechanism by which M-A constituents deteriorate the ICCGHAZ toughness. The results revealed that the microstructure of ICCGHAZ contained blocky M-A constituents along prior austenite grain boundaries. Finally, it was shown that fracture initiation occurred preferentially at M-A constituents by a debonding mechanism rather than cracking of the M-A constituents.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Fatigue and fracture mechanics · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Material Science and Engineering Norwegian University of Science and Technology (NTNU), Trondheim, Norway
Statoil ASA Trondheim, Norway
Department of Applied Mechanics and Corrosion SINTEF, Trondheim, Norway
References (19)
Show source-provided references
1. 10.1016/j.matchar.2006.03.00410.1016/j.matchar.2006.03.004 ↗
2. 10.1016/j.msea.2006.05.09310.1016/j.msea.2006.05.093 ↗
3. 10.1016/j.msea.2007.01.11510.1016/j.msea.2007.01.115 ↗
4. 10.1007/s11661-004-1007-610.1007/s11661-004-1007-6 ↗
5. 10.1016/j.matdes.2009.12.02310.1016/j.matdes.2009.12.023 ↗
6. 10.1007/BF0283033810.1007/BF02830338 ↗
7. 10.1179/026708309X1251274415436010.1179/026708309X12512744154360 ↗
8. Akselsen OM · Scand. J. Metall. · 1988 · 17 · 194
9. Akselsen OM · Scand. J. Metall. · 1990 · 19 · 258
10. Laitinen R: ‘Improvement of weld HAZ toughness at low heat input by controlling the distribution of M-A constituents’, C234, University of Oulu, Oulu, Finland, 2006.
11. Matsuda F · Trans. JWRI · 1994 · 23 · 231
12. 10.1007/BF0265235110.1007/BF02652351 ↗
13. 10.1007/BF0265159810.1007/BF02651598 ↗
14. 10.1016/0001-6160(84)90234-710.1016/0001-6160(84)90234-7 ↗
15. Hrivnak I · Trans. JWRI · 1992 · 21 · 241
16. Matsuda F · Weld. World · 1991 · 29 · 307
17. 10.1016/0026-0800(79)90041-710.1016/0026-0800(79)90041-7 ↗
18. Hrivnak I · Trans. JWRI · 1992 · 21 · 9
19. 10.1179/mst.1993.9.1.810.1179/mst.1993.9.1.8 ↗