Sinter-hipped silicon nitride with additions of ceria and alumina has been subjected to oxidation for up to 72 h at various temperatures. Within the experimental temperature range (1250–1425°C), a parabolic weight gain was observed with an activation energy of 350 kJ mol−1 for the process. On oxidation there formed an oxide scale whose morphology depended on temperature and cooling rate, and a subscale, at the interface between the substrate and the oxide scale, consisting of β3-Si3MN4 grains, a Ce-rich silicate glass, and Si2N20. The morphology and phase content of the oxide products were characterised by X-ray diffractometry and electron microscopy. Detailed analyses by SEM showed that the oxide scales were not homogeneous, but exhibited several layers with important microstructural and compositional variations through their thickness.MST/1107
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Energetic Materials and Combustion
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. 10.1111/j.1151-2916.1975.tb18972.x10.1111/j.1151-2916.1975.tb18972.x ↗
2. 10.1111/j.1151-2916.1980.tb10770.x10.1111/j.1151-2916.1980.tb10770.x ↗
3. 10.1007/BF0239679410.1007/BF02396794 ↗
4. 1974 · 6 · 17
5. 10.1111/j.1151-2916.1979.tb12749.x10.1111/j.1151-2916.1979.tb12749.x ↗
6. 1985 · 68 · 1974
7. 10.1111/j.1151-2916.1981.tb10221.x10.1111/j.1151-2916.1981.tb10221.x ↗
8. 10.1007/BF0102630810.1007/BF01026308 ↗
9. 1980 · 59 · 533
10. 10.1111/j.1151-2916.1978.tb16130.x10.1111/j.1151-2916.1978.tb16130.x ↗
11. 10.1007/BF0054093110.1007/BF00540931 ↗
12. 10.1007/BF0054473910.1007/BF00544739 ↗