Numerical interpretation of cone crack initiation trends in a brittle coating on a compliant substrate
Source abstract
Abstract
Abstract Finite element analysis is used to interpret trends in experimentally observed critical loads for contact damage in a brittle (porcelain) coating on a compliant (polymeric) substrate. Different forms of cracking in the brittle layer—both “cone” cracking initiating at the surface, and “radial” cracking at the layer/substrate interface—are considered, with varying coating thicknesses. The resulting predicted critical loads agree qualitatively with the experimentally observed figures. It is postulated that a previously unexplained peak in critical loads for the onset of cone cracking is caused by a transition between differing modes of cone cracking.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Mechanical stress and fatigue analysis · Mechanical Behavior of Composites · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Peterson · J. Dent. Res. · 1998 · 77 · 58910.1177/00220345980770041201 ↗
2. Knight · Thin Solid Films · 1989 · 177 · 11710.1016/0040-6090(89)90561-0 ↗
3. Katz · Int. J. High Technol. Ceram. · 1985 · 1 · 6910.1016/0267-3762(85)90025-6 ↗
4. Kelly · Annu. Rev. Mater. Sci. · 1997 · 27 · 44310.1146/annurev.matsci.27.1.443 ↗
5. Jung · J. Dent. Res. · 1999 · 78 · 88710.1177/00220345990780040901 ↗
6. Burns · J. Am. Ceram. Soc. · 1995 · 78 · 232110.1111/j.1151-2916.1995.tb08664.x ↗
7. Fischer-Cripps · J. Mater. Sci. · 1999 · 34 · 12910.1023/A:1004490230078 ↗
8. Chan · Annu. Rev. Mater. Sci. · 1997 · 27 · 24910.1146/annurev.matsci.27.1.249 ↗
9. An · J. Mater. Res. · 1996 · 11 · 20410.1557/JMR.1996.0025 ↗
10. Pajares · Mater. Sci. Eng. A · 1996 · 208 · 15810.1016/0921-5093(95)10071-7 ↗
11. Lardner · J. Am. Ceram. Soc. · 1997 · 80 · 185110.1111/j.1151-2916.1997.tb03060.x ↗
12. Hu · Thin Solid Films · 1998 · 322 · 22510.1016/S0040-6090(97)00919-X ↗
13. Lee · J. Am. Ceram. Soc. · 1998 · 81 · 239410.1111/j.1151-2916.1998.tb02635.x ↗
14. Lawn · J. Am. Ceram. Soc. · 1998 · 81 · 197710.1111/j.1151-2916.1998.tb02580.x ↗
15. Chai · J. Mater. Res. · 1999 · 14 · 380510.1557/JMR.1999.0514 ↗
16. Zhao · J. Mater. Res. · 2000 · 15 · 67610.1557/JMR.2000.0100 ↗
17. Tsai · Int. J. Prosthodont. · 1998 · 11 · 27
18. Zhao · J. Mater. Res. · 2001 · 16 · 147110.1557/JMR.2001.0205 ↗
19. Lee · J. Mater. Res. · 2000 · 15 · 165310.1557/JMR.2000.0237 ↗
20. Rhee · J. Am. Ceram. Soc. · 2001 · 84 · 106610.1111/j.1151-2916.2001.tb00791.x ↗
21. C. Ford, M. Bush, X.-Z. Hu, H. Zhao, Mater. Sci. Eng. A 364 (1–2) 202–206.10.1016/j.msea.2003.08.019 ↗
22. E.J. Hearn, Mechanics of Materials, 2, 3rd ed., Butterworths-Heinemann, Oxford, 1997.
23. Scherrer · Dent. Mater. · 1998 · 14 · 24610.1016/S0109-5641(98)00032-3 ↗
24. Scherrer · Dent. Mater. · 1999 · 15 · 34210.1016/S0109-5641(99)00055-X ↗
25. Zhao · J. Mater. Res. · 2002 · 17 · 110210.1557/JMR.2002.0163 ↗
26. A. Koller (Ed.), Structure and Properties of Ceramics, Elsevier, Amsterdam, 1994.