journal article·2004-09

Silicon carbide ceramics through temperature-induced gelation and pressureless sintering

X. Xu, S. Mei, J.M.F. Ferreira, T. Nishimura, N. Hirosaki

Materials Science and Engineering: A· Volume 382· Issue 1-2
Publisher page

Abstract

Temperature-induced gelation is a novel near-net-shape method for forming ceramic green bodies from homogeneous high-solids-loaded suspensions. It is based on the change of the solubility of dispersant in solvent with changing temperature. Stable and low-viscosity suspensions of SiC, Y2O3 and Al2O3 powder mixtures were prepared in methyl ethyl keton (MEK)/ ethanol (E) solvent with solid loading as high as 60 vol.% using hypermer KD1 (a polyester/polyamine condensation polymer) as dispersant. The solubility of the dispersant in MEK/E decreased dramatically on cooling. Thus, the suspension displayed a reversible temperature-induced gelation process, being a stable and free flowing fluid at 20 ◦ C, and being completely solidified at 5 ◦ C. The obtained green body showed uniform microstructure, and it was possible to obtain almost theoretical density (≥0.98) upon pressureless sintering without special dispersant burn-out procedure. The possibilities of fabricating homogeneous and complex SiC green parts that can achieve high sintered densities by pressureless sintering are demonstrated. © 2004 Elsevier B.V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Injection Molding Process and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Dapkunas · Am. Ceram. Soc. Bull. · 1988 · 65 · 388
2. Takeda · Am. Ceram. Soc. Bull. · 1988 · 67 · 1961
3. Lange · J. Am. Ceram. Soc. · 1989 · 72 · 310.1111/j.1151-2916.1989.tb05945.x ↗
4. Lewis · J. Am. Ceram. Soc. · 2000 · 83 · 234110.1111/j.1151-2916.2000.tb01560.x ↗
5. Cameron · J. Am. Ceram. Soc. · 1990 · 73 · 203210.1111/j.1151-2916.1990.tb05263.x ↗
6. Sigmund · J. Am. Ceram. Soc. · 2000 · 83 · 155710.1111/j.1151-2916.2000.tb01432.x ↗
7. Ferreira · J. Am. Ceram Soc. · 1999 · 82 · 199310.1111/j.1151-2916.1999.tb02031.x ↗
8. Hirata · J. Mater. Res. · 1997 · 12 · 314610.1557/JMR.1997.0411 ↗
9. Nieto · Am. Ceram. Soc. Bull. · 1998 · 77 · 62
10. J.S. Reed, Introduction to the Principles of Ceramic Processing, Wiley, New York, 1994, pp. 477–491.
11. B.C. Mutsuddy, R.G. Ford, Ceramic Injection Molding, Chapman and Hall, London, UK, 1995, pp. 1–26.
12. Mangels · Am. Ceram. Soc. Bull. · 1994 · 73 · 37
13. Young · J. Am. Ceram. Soc. · 1991 · 74 · 61210.1111/j.1151-2916.1991.tb04068.x ↗
14. Nunn · Ceram. Eng. Sci. Proc. · 1996 · 17 · 20910.1002/9780470314821.ch24 ↗
15. Janney · J. Am. Ceram. Soc. · 1998 · 81 · 58110.1111/j.1151-2916.1998.tb02377.x ↗
16. Omatete · Am. Ceram. Soc. Bull. · 1991 · 70 · 1641
17. Wang · Ceram. Int. · 2002 · 28 · 86510.1016/S0272-8842(02)00066-4 ↗
18. Fanelli · J. Am. Ceram. Soc. · 1989 · 72 · 183310.1111/j.1151-2916.1989.tb05987.x ↗
19. Chen · J. Eur. Ceram. Soc. · 1999 · 19 · 27110.1016/S0955-2219(98)00201-5 ↗
20. Schilling · J. Am. Ceram. Soc. · 1999 · 82 · 5710.1111/j.1151-2916.1999.tb01723.x ↗
21. Graule · Ind. Ceram. · 1996 · 16 · 31
22. Graule · Ind. Ceram. · 1996 · 16 · 36
23. Hruschka · J. Aust. Ceram. Soc. · 1997 · 33 · 21
24. Si · J. Am. Ceram. Soc. · 1999 · 82 · 112910.1111/j.1151-2916.1999.tb01886.x ↗
25. L. Bergström, US Patent 534053223, August 1994.
26. Bergström · J. Eur. Ceram. Soc. · 1999 · 19 · 211710.1016/S0955-2219(99)00021-7 ↗
27. D.H. Napper, Polymeric Stabilisation of Colloidal Dispersions, Academic Press, London, 1982.
28. Th.F. Thadros (Ed.), The Effect of Polymers on Dispersion Properties, Academic Press, London, 1982.
29. Xu · J. Colloid Interface Sci. · 2003 · 259 · 39110.1016/S0021-9797(02)00223-0 ↗
30. Xu · J. Eur. Ceram. Soc. · 2003 · 23 · 152510.1016/S0955-2219(02)00349-7 ↗
31. Xu · Mater. Sci. Forum · 2003 · 442 · 10310.4028/www.scientific.net/MSF.442.103 ↗
32. X. Xu, S. Mei, J.M.F. Ferreira, T. Nishimura, N. Hirosaki, Temperature induced gelation of concentrated silicon carbide suspensions, J. Colloid Interface Sci. 277 (2004) 111–115.10.1016/j.jcis.2004.04.012 ↗