Simultaneous and different nucleation modes in undercooled Pd–Cu–Ni–P melts
Source abstract
Abstract
Abstract Both Pd 40 Cu 30 Ni 10 P 20 alloys with a slightly off-eutectic composition and Pd 42.5 Cu 30 Ni 7.5 P 20 alloys with a eutectic composition exhibit high glass-forming ability and a low critical cooling rate for glass formation of 0.100 and 0.067 K/s, respectively. Due to the difference in the critical cooling rate, an incubation time for crystallization at 683 K for the eutectic alloy is 2.5 times longer than that for the off-eutectic alloy. In order to clarify the reason for the difference, nucleation and crystal grain growth behaviors of the undercooled off-eutectic and eutectic melts were investigated. Nucleation frequency was evaluated as 3.00×10 10 nuclei/m 3 s for the off-eutectic alloy and 4.77×10 9 nuclei/m 3 s for the eutectic alloy. In addition, it is found that the nucleation behavior changes from internal homogeneously dispersed mode to surface one. On the contrary, the crystal grain growth rates have almost the same value of about 3.20×10 −7 m/s for the crystallized phases in both alloys. Based on these results, the compositional effect on the stability of undercooled melt is discussed in the present study.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Solidification and crystal growth phenomena · Fashion and Cultural Textiles
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. Inoue · Mater. Trans. JIM · 1996 · 37 · 18110.2320/matertrans1989.37.181 ↗
2. Nishiyama · Mater. Trans. JIM · 1996 · 37 · 153110.2320/matertrans1989.37.1531 ↗
3. Inoue · Mater. Trans. JIM · 1997 · 38 · 17910.2320/matertrans1989.38.179 ↗
4. Nishiyama · Mater. Trans. JIM · 1997 · 38 · 46410.2320/matertrans1989.38.464 ↗
5. Nishiyama · Acta Mater · 1999 · 47 · 148710.1016/S1359-6454(99)00030-0 ↗
6. Nishiyama · Mater. Trans. JIM · 2001 · 42 · 320110.2320/matertrans.42.1068 ↗
7. Nishiyama · Appl. Phys. Lett · 2000 · 76 · 391410.1063/1.126819 ↗
8. Nishiyama · Mater. Trans. JIM · 1999 · 40 · 6410.2320/matertrans1989.40.64 ↗
9. Nishiyama · Mater. Trans. JIM · 2000 · 41 · 143210.2320/matertrans1989.41.1432 ↗
10. Nishiyama · Appl. Phys. Lett · 2001 · 78 · 198510.1063/1.1359490 ↗
11. Schroers · Appl. Phys. Lett · 2000 · 77 · 115810.1063/1.1289033 ↗
12. Schroers · Acta Mater · 2001 · 49 · 277310.1016/S1359-6454(01)00159-8 ↗
13. Nishiyama · Appl. Phys. Lett · 2002 · 80 · 56810.1063/1.1445475 ↗
14. Kui · Appl. Phys. Lett · 1984 · 45 · 61510.1063/1.95330 ↗
15. N. Nishiyama, M. Matsushita, A. Inoue, in: A. Inoue, et al. (Eds.), Proceedings of MRS Fall Meeting, vol. 644, Boston, 2000, L3.1.10.1557/PROC-644-L3.1 ↗
16. N.Nishiyama, A. Inoue, Intermetallics 10 (2002) 1141.10.1016/S0966-9795(02)00151-6 ↗
17. Ma · Mater. Trans · 2002 · 43 · 116110.2320/matertrans.43.1161 ↗