Investigation of tensile creep behavior of Mg–Gd–Y–Zr alloy based on creep constitutive model

Yaocheng Zhang, Zheng Liu, Song Pang, Tao Meng, Yating Zhi, Yuling Xu, Lv Xiao, Ruifeng Li

Publisher page

Abstract

Abstract The tensile creep behavior of as-extruded and T6 treated Mg–8Gd–3Y–0.3Zr (GW83) alloy was estimated under temperature at 170–200 °C and stress at 40–70 MPa. The results showed that the primary creep strain and steady state creep rate increased, while the duration of steady state creep decreased with increasing temperature and stress. The primary creep constitutive model of GW83 alloy kept an Andrade power law e = βtk with k value of 0.24–0.6 for as-extruded alloy and 0.13–0.49 for T6 alloy, respectively. The steady state creep plastic deformation of as-extruded and T6 state alloys can be expressed by Arrhenius constitutive equations with stress exponents 5.6–5.9 and 8.9–9.8, creep activity energy 124.9–135.6 kJ/mol and 152.2–195.8 kJ/mol, respectively. The tensile creep resistance of GW83 alloy improved significantly by T6 heat treatment, the effect of temperature on steady state creep rate was relatively moderate, and the tensile creep plastic deformation of GW83 alloy mainly was controlled by applied stress. The steady state creep deformation mechanism of as-extruded GW83 alloy was regulated by Mg self-diffusion conducted by dislocation climb before heat treatment, and then transformed to dislocation cross-slip after T6 treated. The recrystallization and texture evolution of (10) , (10) played a non-ignorable effect on the tensile creep deformation. The creep rupture life can be predicted by steady state creep rate that will be controlled by temperature under low and intermediate stress and by stress under larger applied stress, respectively. The creep fracture surfaces with coarse dimples and tear ridges presented as ductile transgranular fracture features with the secondary cracks occurred.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (63)

Show source-provided references
1. Critical Assessment 6: magnesium sheet alloys: viable alternatives to steels?10.1179/1743284714Y.0000000596 ↗
2. Magnesium and its alloys applications in automotive industry10.1007/s00170-007-1279-2 ↗
3. Precipitation and hardening in magnesium alloys10.1007/s11661-012-1217-2 ↗
4. What is going on in magnesium alloys?10.1016/j.jmst.2017.07.019 ↗
5. Microstructural stability and high-temperature mechanical properties of AZ91 and AZ91+2RE magnesium alloys10.1016/j.matdes.2011.01.040 ↗
6. Microstructure evolution of semi-solid Mg–10Gd–3Y–0.5Zr alloy during isothermal heat treatment10.1016/j.jma.2013.02.004 ↗
7. Development of heat resistant Mg-Zn-Al-based magnesium alloys by addition of La and Ca: microstructure and tensile properties10.1016/j.jallcom.2016.05.137 ↗
8. Deteriorated tensile creep resistance of a high-pressure die-cast Mg–4Al–4RE–0.3Mn alloy induced by substituting part RE with Ca10.1016/j.msea.2018.01.027 ↗
9. Effect of Ca and Sr on the compressive creep behavior of Mg–4Al–RE based magnesium alloys10.1016/j.matdes.2014.06.027 ↗
10. Effect of Nd on the microstructure, mechanical properties and corrosion behavior of die-cast Mg–4Al-based alloy10.1016/j.jallcom.2007.10.056 ↗
11. Creep behavior of high-pressure die-cast Mg-4Al-4La-0.4Mn alloy under medium stresses and at intermediate temperatures10.1016/j.msea.2015.09.061 ↗
12. Effect of Y and Ca addition on the creep behaviors of AZ61 magnesium alloys10.1016/j.jallcom.2016.06.015 ↗
13. Effect of substituting cerium-rich mischmetal with lanthanum on microstructure and mechanical properties of die-cast Mg–Al–RE alloys10.1016/j.matdes.2008.10.028 ↗
14. Effect of Si on the creep properties of AZ61 cast magnesium alloy10.1016/j.matdes.2015.03.021 ↗
15. Microstructure characterization and high-temperature shear strength of the Mg–10Gd–3Y–1.2Zn–0.5Zr alloy in the as-cast and aged conditions10.1016/j.jallcom.2014.09.102 ↗
16. Microstructure evolution and mechanical properties of an ultra-high strength casting Mg–15.6Gd–1.8Ag–0.4Zr alloy10.1016/j.jallcom.2014.07.028 ↗
17. Influence of stress on γ″ precipitation behavior in Inconel 718 during aging10.1016/j.jallcom.2018.01.030 ↗
18. Solute segregation and texture modification in an extruded magnesium alloy containing gadolinium10.1016/j.scriptamat.2011.08.012 ↗
19. Precipitation in a Mg–10Gd–3Y–0.4Zr (wt.%) alloy during isothermal ageing at 250°C10.1016/j.jallcom.2005.11.046 ↗
20. Precipitation reactions in magnesium-rare earth alloys containing yttrium, gadolinium or dysprosium10.1016/S1359-6462(02)00596-1 ↗
21. Effect of Gd content on high temperature mechanical properties of Mg–Gd–Y–Zr alloy10.1016/j.msea.2015.11.047 ↗
22. Microstructure and thermal stability of nanocrystalline Mg-Gd-Y-Zr alloy processed by high pressure torsion10.1016/j.jallcom.2017.05.164 ↗
23. Microstructure and mechanical properties of Mg-Gd-Y-Zn-Mn alloy sheets processed by large-strain high-efficiency rolling10.1016/j.msea.2019.01.080 ↗
24. Characterization of hot deformation behavior of as-extruded Mg–Gd–Y–Zn–Zr alloy10.1016/j.jallcom.2014.04.210 ↗
25. A super high-strength Mg-Gd-Y-Zn-Mn alloy fabricated by hot extrusion and strain aging10.1016/j.matdes.2019.107666 ↗
26. Annealing behavior of a cast Mg-Gd-Y-Zr alloy with necklace fine grains developed under hot deformation10.1016/j.msea.2017.02.008 ↗
27. Annealing-induced microstructural evolution and mechanical anisotropy improvement of the Mg-Gd-Y-Zr alloy processed by hot ring rolling10.1016/j.matchar.2018.08.022 ↗
28. Effect of Zn content on the microstructure and mechanical properties of Mg-Gd-Y-Zr alloys10.1016/j.msea.2018.12.088 ↗
29. Alloying Mg with Gd and Y: increasing both plasticity and strength10.1016/j.commatsci.2016.01.003 ↗
30. Effect of Gd content on microstructure and mechanical properties of Mg–Gd–Y–Zr alloys under peak-aged condition10.1016/j.msea.2014.07.056 ↗
31. Microstructure and creep behaviour of Mg-12Gd-3Y-1Zn-0.4Zr alloy10.1016/S1002-0721(12)60256-7 ↗
32. The impression creep behavior and microstructure evolution of cast and cast-then-extruded Mg–10Gd–3Y–0.5Zr (wt%)10.1016/j.msea.2015.10.001 ↗
33. Effects of repetitive upsetting-extrusion parameters on microstructure and texture evolution of Mg–Gd–Y–Zn–Zr alloy10.1016/j.jallcom.2019.03.207 ↗
34. Effect of Zn addition on microstructure and mechanical properties of cast Mg-Gd-Y-Zr alloys10.1016/S1003-6326(19)64982-4 ↗
35. Effect of Y and Gd content on the microstructure and mechanical properties of Mg–Y–RE alloys10.1016/j.jma.2019.03.002 ↗
36. Kassner · 2009
37. Characterisation of low-temperature creep deformation and primary creep stage of TA2 using small punch creep test10.1016/j.engfracmech.2018.11.010 ↗
38. Work hardening during primary creep of copper10.1016/j.msea.2008.07.076 ↗
39. Creep rupture behavior of Grade 91 steel10.1016/j.msea.2012.12.031 ↗
40. A comparative study of the role of Ag in microstructures and mechanical properties of Mg-Gd and Mg-Y alloys10.1016/j.msea.2018.06.084 ↗
41. Creep behavior and microstructure evolution of sand–cast Mg–4Y–2.3Nd–1Gd–0.6Zr alloy crept at 523–573 K10.1016/j.jmst.2016.08.016 ↗
42. Effects of Zr addition on the multi-scale second-phase particles and fracture behavior for Mg-3Gd-1Zn alloy10.1016/j.jallcom.2018.02.328 ↗
43. Low-temperature creep behavior of commercially pure titanium TA210.1016/S1875-5372(10)60008-2 ↗
44. Phenomenological and microstructural analysis of room temperature creep in titanium alloys10.1016/S1359-6454(99)00426-7 ↗
45. The temperature and stress dependent primary creep of CP-Ti at low and intermediate temperature10.1016/j.msea.2014.05.094 ↗
46. Microstructure and impression creep characteristics of squeeze-cast AZ91 magnesium alloy containing Ca and/or Bi10.1016/j.msea.2018.12.067 ↗
47. A primary creep model for Class M materials10.1016/j.msea.2011.03.069 ↗
48. Evolution of superdislocation structures during tertiary creep of a nickel-based single-crystal superalloy at high temperature and low stress10.1016/j.actamat.2016.12.072 ↗
49. Mechanical behavior of crystalline solids at elevated temperature10.1016/0079-6425(68)90024-8 ↗
50. Diffusion-creep in magnesium alloys10.1016/0022-3115(67)90198-5 ↗
51. Recent magnesium alloy development for elevated temperature applications10.1179/095066004225010497 ↗
52. Five-power-law creep in single phase metals and alloys10.1016/S0079-6425(99)00006-7 ↗
53. Creep mechanism of as-cast Mg-6Al-6Nd alloy10.1007/s12598-010-0164-6 ↗
54. Effect of Ca and rare earth elements on impression creep properties of AZ91 magnesium alloy10.1007/s11661-010-0238-y ↗
55. Tensile creep anisotropy of a Mg-2Y alloy extruded sheet with a splitted texture10.1016/j.jallcom.2020.153754 ↗
56. Influence of grain size on the compressive deformation of wrought Mg–3Al–1Zn10.1016/j.actamat.2004.07.015 ↗
57. Investigation of deformation twinning in a fine-grained and coarse-grained ZM20 Mg alloy: combined in situ neutron diffraction and acoustic emission10.1016/j.actamat.2009.10.057 ↗
58. On the evolution of β' precipitate during creep in a Mg–3.3Y–0.1Zr(at.%) alloy10.1016/j.matchar.2018.11.028 ↗
59. Investigation on the impression creep properties of a cast Mg–6Al–1Zn magnesium alloy10.1016/j.matdes.2013.04.045 ↗
60. Texture evolution and deformation activity of an extruded magnesium alloy: effect of yttrium and deformation temperature10.1016/j.jallcom.2016.07.150 ↗
61. The effects of grain size and heat treatment on the deformation heterogeneities and fatigue behaviors of GW83K magnesium alloys10.1016/j.msea.2019.03.063 ↗
62. Microstructures and tensile properties of Mg–8Gd–0.6Zr–xNd–yY (x+y=3, mass%) alloys10.1016/j.msea.2006.06.043 ↗
63. Role of initial {10-12} twin in the fatigue behavior of rolled Mg–3Al–1Zn alloy10.1016/j.scriptamat.2010.01.021 ↗