Effect of friction stir processing and subsequent annealing on microstructure and mechanical properties of a metastable β-Zr alloy
Source abstract
Abstract
Abstract In this work, an effective method to improve the local mechanical properties of β-ZrTiAlV alloy via friction stir processing (FSP) was proposed. A good strength-ductility synergy with high yield strength (896 MPa) and elongation (18.3%) was achieved in the FSPed alloy compared to that of the base material (BM) with low elongation (2.9%) owing to the grain refinement by dynamic recrystallization (DRX) during FSP and the transformation induced plasticity (TRIP) effect caused by deformation-induced α′ martensite transformation. Moreover, FSPed alloy can be further strengthened by annealing treatment. A higher yield strength (1003 MPa) was obtained following 650 °C anneal while a higher ultimate tensile strength (1276 MPa) was acquired in 600 °C annealed samples. The microstructure-properties relationship and underlying deformation mechanisms were also investigated.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Titanium Alloys Microstructure and Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Texture development and anisotropic deformation of zircaloys10.1016/j.pnucene.2005.09.011 ↗
2. Effect of predeformation on microstructural evolution of a Zr alloy during 550-700°C aging after β quenching10.1016/j.actamat.2013.02.001 ↗
3. Reassessment of oxidation-induced amorphization and dissolution of Nb precipitates in Zr-Nb nuclear fuel cladding tubes10.1016/j.actamat.2017.01.032 ↗
4. Achieving high strength and toughness in a Zr-2.3Nb alloy by the formation of duplex microstructure10.1016/j.matdes.2012.04.012 ↗
5. Formation of duplex microstructure in Zr-2.3Nb alloy and its plastic behaviour at various strain rates10.1016/j.ijplas.2013.08.013 ↗
6. Microstructure and mechanical properties of hot-rolled ZrTiAlV alloys10.1016/j.msea.2011.10.053 ↗
7. Structural evolution and mechanical properties of Zr-45Ti-5Al-3V alloy by heat treatments10.1016/j.msea.2012.02.003 ↗
8. Influence of the high pressure torsion die geometry on the allotropic phase transformations in pure Zr10.1016/j.msea.2010.02.066 ↗
9. High strength and ductility in multimodal-structured Zr10.1016/j.matdes.2011.08.002 ↗
10. Investigation of structure, phase composition, and mechanical properties of Zr-2.5% Nb alloy after ECAP10.1016/j.matlet.2016.01.148 ↗
11. Effect of annealing on structural and phase transformations and mechanical properties of ultrafine-grained E125 zirconium alloy obtained by high-pressure torsion10.1016/j.matlet.2017.06.107 ↗
12. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
13. Friction-stir welding and processing of Ti-6Al-4V titanium alloy: a review10.1016/j.jmst.2017.10.018 ↗
14. Achieving ultrafine dual-phase structure with superior mechanical property in friction stir processed plain low carbon steel10.1016/j.msea.2013.03.033 ↗
15. Microstructure and mechanical properties of friction stir processed Cu with an ideal ultrafine-grained structure10.1016/j.matchar.2016.10.009 ↗
16. Achieving an excellent strength-ductility synergy in Zircaloy-4 by FSW with rapid cooling10.1080/02670836.2017.1320861 ↗
17. Microstructure, texture evolution and mechanical properties of pure Ti by friction stir processing with slow rotation speed10.1016/j.matchar.2018.12.006 ↗
18. Microstructural refinement and property enhancement of cast light alloys via friction stir processing10.1016/j.scriptamat.2007.09.062 ↗
19. Microstructural studies of friction stir welded Zircaloy-410.1016/j.scriptamat.2012.04.029 ↗
20. Twinning behaviors and grain refinement mechanisms during friction stir processing of Zr alloy10.1016/j.matchar.2020.110277 ↗
21. Microstructures and mechanical properties of friction stir welded joints of Zr-Ti alloy10.1179/1362171814Y.0000000229 ↗
22. Microstructural and mechanical properties of a beta-type titanium alloy joint fabricated by friction stir welding10.1016/j.msea.2017.11.006 ↗
23. Investigation of early stage deformation mechanisms in a metastable β titanium alloy showing combined twinning-induced plasticity and transformation-induced plasticity effects10.1016/j.actamat.2013.07.019 ↗
24. The effects of increasing deformation strain on the microstructural evolution of a metastable β-Zr alloy10.1016/j.jallcom.2019.05.334 ↗
25. {332}<113> Twinning system selection in a β-type Ti-15Mo-5Zr polycrystalline alloy10.1016/j.msea.2013.04.119 ↗
26. A new titanium alloy with a combination of high strength, high strain hardening and improved ductility10.1016/j.scriptamat.2014.09.005 ↗
27. Evidence for deformation-induced phase transformation in a high Sn content zirconium alloy10.1016/j.actamat.2018.09.034 ↗
28. Changeable Young's modulus with large elongation-to-failure in β-type titanium alloys for spinal fixation applications10.1016/j.scriptamat.2014.03.014 ↗
29. Anisotropic pitting of single-phase β-Zr alloy and isotropic pitting of α+β double-phase Zr alloy10.1016/j.corsci.2017.08.006 ↗
30. Tailoring elastic admissible strain of TiZr alloy by cold rolling deformation10.1016/j.jallcom.2018.11.388 ↗
31. Abnormal martensitic transformation of high Zr-containing Ti alloys10.1016/j.jallcom.2014.07.041 ↗
32. Development of grain structure during friction stir welding of pure titanium10.1016/j.actamat.2009.06.020 ↗
33. Stacking-fault energy, mechanical twinning and strain hardening of Fe-18Mn-0.6C-(0, 1.5)Al twinning-induced plasticity steels during friction stir welding10.1016/j.actamat.2018.02.004 ↗
34. Fabrication of high-quality Ti joint with ultrafine grains using submerged friction stirring technology and its microstructural evolution mechanism10.1016/j.actamat.2018.12.059 ↗
35. A review of dynamic recrystallization phenomena in metallic materials10.1016/j.matdes.2016.09.012 ↗
36. Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions10.1016/j.pmatsci.2013.09.002 ↗
37. Elucidation of microstructural evolution of beta-type titanium alloy joint during friction stir welding using liquid CO2 cooling10.1016/j.matchar.2018.09.005 ↗
38. Microstructural evolution of pure copper during friction-stir welding10.1080/14786435.2015.1006293 ↗
39. Deformation mechanism and mechanical properties of a thermomechanically processed β Ti-28Nb-35.4Zr alloy10.1016/j.jmbbm.2017.11.025 ↗
40. Mechanical properties and deformation mechanisms of Ti-3Al-5Mo-4.5 V alloy with varied β phase stability10.1016/j.jmst.2018.04.004 ↗
41. A multi-deformation mechanisms assisted metastable β-ZrTiAlV alloy exhibits high yield strength and high work hardening rate10.1016/j.jallcom.2019.152642 ↗
42. Deformation mechanisms in a metastable beta titanium twinning induced plasticity alloy with high yield strength and high strain hardening rate10.1016/j.actamat.2018.04.035 ↗
43. Microstructure evolution and superelastic behavior in Ti-35Nb-2Ta-3Zr alloy processed by friction stir processing10.1016/j.actamat.2017.03.079 ↗
44. Microstructure evolution and electrochemical properties of TiO2/Ti-35Nb-2Ta-3Zr micro/nano-composites fabricated by friction stir processing10.1016/j.matdes.2019.107680 ↗
45. Tensile and superelastic behaviors of Ti-35Nb-2Ta-3Zr with gradient structure10.1016/j.matdes.2020.108961 ↗
46. The influence of β phase stability on deformation mode and compressive mechanical properties of Ti-10V-3Fe-3Al alloy10.1016/j.actamat.2014.10.043 ↗
47. Influence of α morphology and volume fraction on the stress-induced martensitic transformation in Ti-10V-2Fe-3Al10.1016/j.msea.2011.03.107 ↗