Abstract

We analyze stresses and the degree of plastic deformation at the contours of cracks of two types, namely, a sharp crack and a crack with slip lines. We show that at the tip of a crack of the second type, at the contour of the bottom–walls of the crack galvanic couple, there appear two symmetric microgalvanic couples at the slip lines. Microinhomogeneities of a metal (grain boundaries, nonmetallic inclusions, etc.) are submicrogalvanic couples whose activity increases due to inhomogeneity of microplastic deformations of their vicinities. We distinguished the mechanisms of corrosion-cyclic fracture and corrosion-static cracking. Under cyclic loading, breaking of grains occurs and grain boundaries and nonmetallic inclusions fail, which levels the influence of currents of submicrogalvanic couples on the growth rate of a crack. Under static loading, micro- and submicrogalvanic couples are permanently operating, the cold work of the surfaces of the metal of the walls of the crack is lower than that under cyclic loading, while the difference of potentials and the current of the bottom–walls of the crack galvanic couple are greater than those under cyclic loading. This explains both the phenomenon of branching and the higher growth rate of a crack of corrosion-static cracking with time. In addition to the electrode potential and pH of the medium, we propose to consider the following parameters as defining factors of the growth of a crack: currents of a galvanic couple, micro-, and submicrogalvanic couples and the time of repassivation of freshly formed metal surfaces appearing in the process of the growth of a crack. According to analysis of the literature data, these parameters cannot be experimentally determined. For this reason, we propose to use methods of simulation to investigate distributions of the potentials and currents of corrosion at the tip of a crack. We propose certain structures of physical and mechanoelectrochemical models of a crack and methods for measurement of distributions of the current density and the electrode potential at their surfaces.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Material Properties and Failure Mechanisms · Engineering Diagnostics and Reliability · Industrial Engineering and Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. V. V. Panasyuk, L. V. Ratych, and I. N. Dmytrakh, “Determination of cyclic crack resistance of structural materials in a corrosive medium,” Dokl. Akad. Nauk SSSR, 269, No. 1, 109–112 (1983).
2. V. V. Panasyuk, L. V. Ratych, and I. N. Dmytrakh, “Fatigue crack growth in corrosive environments,” Fatigue Eng. Mater. Struct., No. 1, 1–11 (1984).10.1111/j.1460-2695.1984.tb00355.x ↗
3. V. V. Panasyuk, L. V. Ratych, and I. N. Dmytrakh, “Cyclic crack resistance of metals in corrosive media,” Uspekhi Mekh., No. 3, 37–50 (1984).
4. V. V. Panasyuk, L. V. Ratych, and I. N. Dmytrakh, “Determination of basic diagrams of corrosion-cyclic crack resistance of steels with regard for extremal electrochemical conditions in a crack,” Dokl. Akad. Nauk SSSR, 266, No. 5, 1128–1131 (1986).
5. Yu. Ya. Iossel' and G. É. Klenov, Mathematical Methods for Analysis of Electrochemical Corrosion and Protection of Metals [in Russian], Metallurgiya, Moscow (1984).
6. V. N. Tkachenko, M. V. Getmanskii, and V. N. Ryabukhina, “Calculation of the geometry of a developing corrosion pit,” Zashch. Met., No. 2, 209–213 (1985).
7. R. N. Parkins, “Factor of corrosive medium under cyclic loading of metals,” in: Ya. M. Kolotyrkin (editor), Corrosion Fatigue of Metals. Proceedings of the First Soviet-English Seminar [in Russian], Naukova Dumka, Kiev (1982), pp. 337–339.
8. R. A. H. Edvards, “Conversion of potential as dept seans inside crack into plots of current density on the walls,” Corrosion (USA), 42, No. 4, 245–247 (1986).10.5006/1.3586005 ↗
9. A. Turnbull and J. G. N. Thomas, “A model of crack electrochemistry for steels on mass transport by diffusion and ion migration,” J. Electrochem. Soc., 129, No. 7, 1412–1422 (1982).10.1149/1.2124176 ↗
10. G. I. Bignold, “Cyclic voltammetry at the iron electrode in high temperature sodium hydroxide solution,” Corros. Sci., 12, No. 6, 145–153 (1972).10.1016/S0010-938X(72)90874-8 ↗
11. W. Fu John and Chan Sin-Kee, “A finite element method for modeling localized corrosion cells,” Corrosion, 40, No. 10, 540–544 (1984).10.5006/1.3593890 ↗
12. Yu. A. Popov and Yu. V. Alekseev, “Kinetics of the growth of pitting,” Élektrokhimiya, 23, No. 1, 79–84 (1981).
13. I. P. Gnyp, É. I. Lychkovskii, and V. F. Kondrat, “Calculation of the distribution of the electric field in metallic crevices with corrosive medium,” Fiz.-Khim. Mekh. Mater., 23, No. 1, 14–19 (1987).
14. V. V. Panasyuk (editor), Fracture Mechanics and Strength of Materials. A Handbook [in Russian], Vols. 1-4, Naukova Dumka, Kiev (1990).
15. V. G. Karpenko, V. N. Loboiko, S. I. Mikitishin, and I. I. Vasilenko, “Dependence of the ultimate strength of a metal on the character of interaction with medium,” Dokl. Akad. Nauk SSSR, 211, No. 4, 833–835 (1973).
16. N. N. Dmytrakh, L. V. Ratych, and V. V. Panasyuk, Electrochemical Capillary for Electrochemical Investigation of Crack Resistance of Materials [in Russian], Inventor's Certificate 934345 SSSR MKI3 G01N27/52, Published 07.06.82, Bull. No. 21 (1982).
17. G. Gabetta, “A method to measure electrochemical potential at the tip of growing crack during environmental fatigue test,” Fatigue Eng. Mater. Struct., No. 3, 215–220 (1982).10.1111/j.1460-2695.1982.tb01248.x ↗
18. A. V. Saakiyan, L. Ya. Efremov, L. Ya. Ropyak, and A. V. Gorbatskii, “On the method of microelectrochemical investigations,” Fiz.-Khim. Mekh. Mater., 23, No. 3, 40–43 (1987).
19. V. A. Makarov, G. M. Florianovich, and Ya. M. Kolotyrkin, “Theoretical aspects of electrochemical protection of metals in corrosive medium,” Fiz.-Khim. Mekh. Mater., 22, No. 6, 3–11 (1986).
20. L. V. Ratych, Methods for the Estimation of Crack Resistance of Metals in Corrosive Media [in Russian], Author's Abstract of the Doctoral-Degree Thesis (Technical Sciences), Lviv (1991).
21. L. N. Petrov and A. Yu. Kalinkov, “On the electrochemical situation in corrosion-mechanical cracks,” Fiz.-Khim. Mekh. Mater., 30, No. 4, 54–60 (1994).
22. V. S. Bagotskii, Fundamentals of Electrochemistry [in Russian], Khimiya, Nauka (1988).
23. A. V. Ryabchenkov, Corrosion-Fatigue Strength of Steel [in Russian], Mashgiz, Moscow (1953).
24. G. V. Karpenko, É. M. Gutman, I. E. Zamostyanik, and L. M. Gavrilenko, “Corrosion microelements of deformed iron,” Dokl. Akad. Nauk SSSR, 187, No. 2, 389–390 (1969).
25. M. Ya. Barnyak, I. P. Gnyp, V. F. Kondrat, and E. V. Kartysh, “Projection method for calculation of distribution of electric fields and currents in volumes filled with electrolyte,” Fiz.-Khim. Mekh. Mater., 26, No. 3, 101–105 (1990).
26. M. H. Stashchuk, “Determination of the electrode potential and corrosion currents along surfaces of stress concentrators,” in: Fracture Mechanics and Strength of Structures (Issue 2) [in Ukrainian], Vol. 2, Kamenyar, Lviv (1996), pp. 213–219.
27. S. M. Shariand and P. W. Tasker, “A mathematical model of crevice and pitting corrosion,” Corros. Sci., 28, No. 6, 603–630 (1991).10.1016/0010-938X(88)90027-3 ↗
28. O. N. Romaniv and G. N. Nikiforchin, Mechanics of Corrosion Fracture of Structural Alloys [in Russian], Metallurgiya, Moscow (1986).
29. Pu Su Yun and Zhao Wen Li, “Stress corrosion cracking behaviour of implant titanium alloy in physiological solution,” in: Proc. Techn. Program. Int. Conf. “Titanium 1990: Production and Application,” Vol. 2, Dayton, Ohio, pp. 693-699.
30. I. P. Gnyp, “Phenomenological aspects of the influence of parameters of cyclic loading on the corrosion-fatigue growth of cracks,” Fiz.-Khim. Mekh. Mater., 20, No. 4, 40–44 (1984).
31. V. A. Shtoff, Simulation and Knowledge [in Russian], Nauka i Tekhnika, Minsk (1974).
32. Simulation of Processes of Deformation and Fracture of Solids. A Collection of Scientific Transactions [in Russian], Academy of Sciences of the USSR, Ural Scientific Center, Sverdlovsk (1987).
33. Simulation and Diagnostics of Complicated Processes and Systems. A Collection of Scientific Transactions of the Ukrainian Academy of Sciences. Institute of Problems of Simulation in Energetics, Intersectional Scientific and Engineering Complex “Impulse” [in Russian], Naukova Dumka, Kiev (1997).
34. É. I. Lychkovskii, “On the simulation of electrochemical processes at the tip of a crack,” Fiz.-Khim. Mekh. Mater., 23, No. 3, 33–35 (1987).
35. L. N. Petrov and A. Yu. Kalinkov, “On the electrochemical situation in corrosion-mechanical cracks,” Fiz.-Khim. Mekh. Mater., 30, No. 4, 54–60 (1994).
36. H. H. Uhlig and R. W. Revie, Corrosion and Corrosion Control. An Introduction to Corrosion Science and Engineering, Wiley, New York (1985).
37. R. O. Ritchie, J. F. Knott, and J. R. Rice, “On the relationship between critical tensile steels and fracture toughness in mild steel,” J. Mech. Phys. Solids, 21, 395–410 (1973).10.1016/0022-5096(73)90008-2 ↗
38. G. H. Bulloch and P. Alexander, “Corrosion fatigue behavior of A508-III steel in a simulated PRW water environment at 525°C,” Int. G. Pressure Vessels Pip., 24, No. 4, 283–302 (1986).10.1016/0308-0161(86)90003-7 ↗
39. G. P. Ray, R. A. Garman, and G. R. Thomas, “The influence of non-metallic inclusions on the corrosion fatigue of mild steel,” Corros. Sci., 75, No. 3, 171–184 (1985).10.1016/0010-938X(85)90093-9 ↗
40. D. D. Hicks and F. P. A. Robinson, “Fatigue crack growth rates in a pressure vessel steel under various conditions of loading and the environment,” Mat. Trans., A17, No. 7-12, 1837–1849 (1986).10.1007/BF02817280 ↗
41. H. Hanhinen, K. Soarinen, and K. Ehrnsten, “Determination of the threshold potential for stress corrosion cracking of low alloy steels in PRW primary water,” in: Proceedings of the Third International Atomic Energy Specialists Meeting on the Subcritical Crack Growth [in Russian], Vol. 1, (Moscow, May 1990), NUREG/CP0112, ANL (1990), pp. 271–278.
42. F. P. Ford and P. L. Andersen, “Corrosion fatigue of A533B/A508 - pressure vessel in 288°C water,” in: Proceedings of the Third International Atomic Energy Specialists Meeting on the Subcritical Crack Growth [in Russian], Vol. 2, (Moscow, May 1990), NUREG/CP0112, ANL (1990), pp. 37–56.
43. F. P. Ford, “Status of research of environmentally assisted cracking in LWR pressure vessel steels,” Trans. ASME: G. Pressure Vessel Technol., 10, No. 2, 113–128 (1988).
44. I. P. Gnyp, V. I. Pokhmurs'kyi, and I. M. Antoshchak, “Analysis of the influence of nonmetallic inclusions on corrosion crack resistance of steels,” Fiz.-Khim. Mekh. Mater., 28, No. 4, 28–35 (1992).
45. I. P. Gnyp and I. M. Antoshchak, “Influence of metallurgical and electrochemical factors on cracking of steels of nuclear power stations at a high temperature,” Probl. Prochn., No. 3, 63–71 (1996).
46. A. N. Orlov (editor), Atomic Structure of Intergranular Boundaries, News of Physics of Solid [in Russian], Issue 8, Mir, Moscow (1978).
47. V. I. Pokhmurskii, É. I. Lychkovskii, V. M. Filatov, and I. P. Gnyp, “Distribution of potentials in narrow crevices simulating the electrochemical situation in spaces of a corrosion crack,” Fiz.-Khim. Mekh. Mater., 23, No. 4, 27–30 (1987).
48. D. V. Sivukhin, General Course in Physics. Electricity [in Russian], Nauka, Moscow (1983).