Enhanced hot-hardness in nanograined Nb with stable grain boundary at small grain size
Source abstract
Abstract
Nanograined pure Nb samples with two types of grain sizes (15 nm and 59 nm) were prepared by high-pressure torsion. The 15-nm-grained sample has a higher fraction of low-angle grain boundaries and CSL boundaries compared with the 59-nm-grained sample. These structures significantly reduce the grain boundary energy and suppress the grain coarsening rate under thermomechanical conditions, endowing the 15-nm-grained sample with an ultra-high hot-hardness of 6.3 GPa at 800 °C, which is threefold higher than that of the 59-nm-grained specimen. This provides a novel strategy for designing high-performance heat-resistant BCC refractory metals with stable grain boundaries at small grain sizes.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Microstructure and mechanical properties · Surface Treatment and Residual Stress · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Chinese Academy of Sciences
University of Science and Technology of China
Funding
Chinese Academy of Sciences · National Science Foundation of China · Youth Innovation Promotion Association CAS
References (59)
Show source-provided references
1. 10.1007/978-3-319-69743-710.1007/978-3-319-69743-7 ↗
2. Prasad N, Wanhill R. Aerospace materials and material technologies: volume 2: Aerospace Material Technologies. Singapore: Springer; 2017.
3. 10.1080/21663831.2025.256432610.1080/21663831.2025.2564326 ↗
4. 10.13182/FST11-A1273610.13182/FST11-A12736 ↗
5. 10.2320/jinstmet1952.64.7_55910.2320/jinstmet1952.64.7_559 ↗
6. 10.1080/21663831.2024.241947510.1080/21663831.2024.2419475 ↗
7. 10.1007/s11661-003-0269-810.1007/s11661-003-0269-8 ↗
8. 10.1016/j.jmst.2022.11.02210.1016/j.jmst.2022.11.022 ↗
9. 10.1016/j.msea.2015.07.06310.1016/j.msea.2015.07.063 ↗
10. 10.1016/S0079-6425(99)00007-910.1016/S0079-6425(99)00007-9 ↗
11. 10.1021/accountsmr.0c0007510.1021/accountsmr.0c00075 ↗
12. 10.1016/j.actamat.2012.10.03810.1016/j.actamat.2012.10.038 ↗
13. 10.1126/science.aar694110.1126/science.aar6941 ↗
14. 10.1038/natrevmats.2016.1910.1038/natrevmats.2016.19 ↗
15. 10.1080/21663831.2023.221372910.1080/21663831.2023.2213729 ↗
16. 10.1016/j.msea.2016.01.02710.1016/j.msea.2016.01.027 ↗
17. 10.1016/j.actamat.2004.07.04410.1016/j.actamat.2004.07.044 ↗
18. 10.1016/j.actamat.2022.11764010.1016/j.actamat.2022.117640 ↗
19. 10.1126/science.abq773910.1126/science.abq7739 ↗
20. 10.1021/accountsmr.0c0007510.1021/accountsmr.0c00075 ↗
21. 10.1016/j.jmst.2024.03.02210.1016/j.jmst.2024.03.022 ↗
22. Vítek V. Intrinsic stacking faults in body-centred cubic crystals. Philos Mag J Theoret Exp Appl Phys. 1968;18(154):773–786.
23. 10.1016/j.msea.2010.10.05210.1016/j.msea.2010.10.052 ↗
24. 10.1126/science.abh070010.1126/science.abh0700 ↗
25. 10.1016/j.matlet.2020.12881910.1016/j.matlet.2020.128819 ↗
26. 10.4028/www.scientific.net/MSF.667-669.78510.4028/www.scientific.net/MSF.667-669.785 ↗
27. 10.1016/j.actamat.2011.12.01910.1016/j.actamat.2011.12.019 ↗
28. 10.1016/j.msea.2011.12.08210.1016/j.msea.2011.12.082 ↗
29. 10.2320/matertrans.MD20113110.2320/matertrans.MD201131 ↗
30. 10.1016/j.matpr.2020.08.42610.1016/j.matpr.2020.08.426 ↗
31. 10.1080/21663831.2024.235676110.1080/21663831.2024.2356761 ↗
32. 10.1007/s10853-013-7210-310.1007/s10853-013-7210-3 ↗
33. 10.1134/S0031918X1611005310.1134/S0031918X16110053 ↗
34. 10.1016/j.actamat.2018.07.03010.1016/j.actamat.2018.07.030 ↗
35. 10.1016/j.actamat.2006.07.01310.1016/j.actamat.2006.07.013 ↗
36. 10.1109/TASC.2023.324853310.1109/TASC.2023.3248533 ↗
37. 10.1016/j.msea.2010.02.04310.1016/j.msea.2010.02.043 ↗
38. 10.1126/science.124257810.1126/science.1242578 ↗
39. 10.1016/j.scriptamat.2018.05.03610.1016/j.scriptamat.2018.05.036 ↗
40. 10.1016/j.scriptamat.2023.11582110.1016/j.scriptamat.2023.115821 ↗
41. 10.1016/j.actamat.2023.11907410.1016/j.actamat.2023.119074 ↗
42. 10.1016/0001-6160(73)90026-610.1016/0001-6160(73)90026-6 ↗
43. 10.1080/14786435.2010.48127210.1080/14786435.2010.481272 ↗
44. 10.1016/j.actamat.2014.03.06310.1016/j.actamat.2014.03.063 ↗
45. 10.1016/S1359-6454(99)00418-810.1016/S1359-6454(99)00418-8 ↗
46. 10.1016/j.actamat.2011.11.03510.1016/j.actamat.2011.11.035 ↗
47. Zheng S, Beyerlein IJ, Carpenter JS, et al. High-strength and thermally stable bulk nanolayered composites due to twin-induced interfaces. Nat. Com. 2013;4(1):1696.
48. 10.1073/pnas.131943611110.1073/pnas.1319436111 ↗
49. 10.1016/S1359-6454(01)00212-910.1016/S1359-6454(01)00212-9 ↗
50. 10.1016/j.msea.2016.08.04510.1016/j.msea.2016.08.045 ↗
51. 10.1016/j.actamat.2020.05.05710.1016/j.actamat.2020.05.057 ↗
52. 10.1016/j.msea.2014.10.01610.1016/j.msea.2014.10.016 ↗
53. 10.1016/j.jnucmat.2007.03.02510.1016/j.jnucmat.2007.03.025 ↗
54. 10.1016/j.ijrmhm.2019.02.00510.1016/j.ijrmhm.2019.02.005 ↗
55. 10.1016/0502-8205(49)90004-010.1016/0502-8205(49)90004-0 ↗
56. 10.1016/j.actamat.2012.10.00810.1016/j.actamat.2012.10.008 ↗
57. Michaluk CA, Huber LE, Ford RB. Niobium and ni obium 1% zirconium for high pressure sodium (HPS) discharge lamps. In: Proceedings of the International Symposium Niobium 2001; 2001 Dec 2–5; Orlando, FL. Bridgeville (PA): Niobium Limited; 2001. p. 1–12.
58. 10.1016/j.ijplas.2008.06.00510.1016/j.ijplas.2008.06.005 ↗
59. 10.1063/1.182821310.1063/1.1828213 ↗