journal article·2021-08-03Open access

Alloy design against the solidification cracking in fusion additive manufacturing: an application to a FeCrAl alloy

Bogdan Dovgyy, Marco Simonelli, Minh-Son Pham

Materials Research Letters· Volume 9· Issue 8

Abstract

This study developed a design methodology against liquid-state cracking by combining the Scheil–Gulliver solidification simulations and Machine Learning analysis to design alloys for Fusion Additive Manufacturing. Applying this design approach resulted in a Fe–20Cr–7Al–4Mo–3Ni. The alloy was successfully printed with relative densities of over 99%. Microstructure of printed material was extensively characterised through scanning and transmission electron microscopy, energy dispersive spectroscopy and x-ray diffraction, confirming a single-phase material with low texture and negligible chemical segregation. Neither solidification nor liquation cracks were detected, supporting the validity of the methodology, however, the alloy suffered from solid-state cracking, hindering the ductility.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Fusion materials and technologies · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials, Imperial College London, London, UK

Centre for Additive Manufacturing, University of Nottingham, Nottingham, UK

Funding

EPSRC

References (33)

Show source-provided references
1. 10.1016/j.addma.2021.10185310.1016/j.addma.2021.101853 ↗
2. 10.1016/j.addma.2020.10170610.1016/j.addma.2020.101706 ↗
3. 10.1016/j.matdes.2020.10876210.1016/j.matdes.2020.108762 ↗
4. 10.1016/S1468-6996(01)00047-X10.1016/S1468-6996(01)00047-X ↗
5. 10.1007/BF0267259310.1007/BF02672593 ↗
6. 10.1038/s41467-020-14453-310.1038/s41467-020-14453-3 ↗
7. 10.1007/s11661-018-4870-210.1007/s11661-018-4870-2 ↗
8. 10.1007/s11665-019-04275-w10.1007/s11665-019-04275-w ↗
9. 10.1016/j.dental.2015.09.00310.1016/j.dental.2015.09.003 ↗
10. Letenneur M · J Manuf Mater Process · 2019 · 3 · 21
11. 10.1016/j.msea.2016.04.04210.1016/j.msea.2016.04.042 ↗
12. 10.1016/j.actamat.2019.10.04710.1016/j.actamat.2019.10.047 ↗
13. 10.1179/1743280413Y.000000002010.1179/1743280413Y.0000000020 ↗
14. Kou S. · Weld J · 2015 · 94 · 374s
15. Feurer U. Influence of alloy composition and solidification conditions on dendrite arm spacing, feeding and hot tearing properties of aluminium alloys. Proc Int Symp Delft; 1977. p. 131–145.
16. 10.1016/j.actamat.2015.01.03410.1016/j.actamat.2015.01.034 ↗
17. 10.1007/s11661-999-0334-z10.1007/s11661-999-0334-z ↗
18. 10.1007/BF0266458310.1007/BF02664583 ↗
19. 10.1016/j.addma.2018.05.03210.1016/j.addma.2018.05.032 ↗
20. 10.1179/13621710322500563310.1179/136217103225005633 ↗
21. 10.1007/s00170-018-2095-610.1007/s00170-018-2095-6 ↗
22. 10.1016/j.matdes.2015.10.15510.1016/j.matdes.2015.10.155 ↗
23. 10.1533/9780857098771.2.33210.1533/9780857098771.2.332 ↗
24. 10.1038/s41586-019-1702-510.1038/s41586-019-1702-5 ↗
25. 10.2172/147458110.2172/1474581 ↗
26. 10.1016/j.msea.2018.07.07410.1016/j.msea.2018.07.074 ↗
27. 10.1016/j.jnucmat.2015.10.01910.1016/j.jnucmat.2015.10.019 ↗
28. 10.1007/s11837-017-2705-z10.1007/s11837-017-2705-z ↗
29. 10.1016/j.jmatprotec.2020.11680210.1016/j.jmatprotec.2020.116802 ↗
30. 10.1016/j.matdes.2020.10884510.1016/j.matdes.2020.108845 ↗
31. 10.1016/j.matlet.2018.04.05210.1016/j.matlet.2018.04.052 ↗
32. 10.1038/nmat502110.1038/nmat5021 ↗
33. 10.1016/j.actamat.2017.02.00710.1016/j.actamat.2017.02.007 ↗