Correlations of microstructure and mechanical properties of the ternary Sn-9wt%Zn-2wt%Cu solder alloy
Source abstract
Abstract
The microstructure length-scales (dendritic and eutectic), morphologies and tensile properties of a ternary Sn-9wt.%Zn-2wt.%Cu alloy are compared with those of a binary eutectic Sn-9wt.%Zn alloy. The following experimental/analytical steps were performed: transient directional solidification experiments of the Sn-9wt.%Zn-2wt.%Cu alloy; measurements of secondary dendrite arm (λ2) and interphase spacing (λ); morphology of the eutectic α-Zn phase; determination of thermal parameters such as cooling rate (ṪL) and their evolutions during solidification; and, finally, interrelations of microstructure vs. tensile properties. The addition of 2wt.%Cu causes significant refinement of the eutectic structure. Hall-Petch type experimental expressions outlined the variations of strength and ductility with both λ2 and λ. Very fine Zn globules and needles forming the eutectic in the ternary alloy seems to cause a reversal on ductility behavior, as compared to the tendency observed for the binary Sn-9wt.%Zn alloy. Here, for the ternary Sn-9wt.%Zn-2wt.%Cu alloy ductility increases with decreasing interphase spacing.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloy Microstructure Properties · Solidification and crystal growth phenomena
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Universidade Federal do Rio Grande do Norte - UFRN, Brazil
Universidade Federal de São Carlos - UFSCar, Brazil
References (21)
Show source-provided references
1. Mechanical properties of Sn-Zn lead-free solder alloys based on the microstructure array10.1016/j.matchar.2009.11.012 ↗
2. Microstructure and mechanical properties of Sn-Bi, Sn-Ag and Sn-Zn lead-free solder alloys10.1016/j.jallcom.2013.03.234 ↗
3. Investigations of interfacial reactions of Sn-Zn based and Sn-Ag-Cu lead-free solder alloys as replacement for Sn-Pb solder10.1016/j.jallcom.2005.03.053 ↗
4. Wetting and interface microstructure between Sn-Zn binary alloys and Cu10.1557/JMR.1998.0391 ↗
5. Influence of small amount of Al and Cu on the microstructure, microhardness and tensile properties of Sn-9Zn binary eutectic solder alloy10.1016/j.jallcom.2009.03.017 ↗
6. Elastic properties and thermal behavior of Sn-Zn based lead-free solder alloys10.1016/j.jallcom.2010.06.142 ↗
7. Effects of small addition of Ag and/or Cu on the microstructure and properties of Sn-9Zn lead-free solders10.1016/j.msea.2010.04.078 ↗
8. Rahman M · 2009 · 1
9. Kurz W · 1992
10. Garcia A · 2011
11. Effects of Ag and Cu addition on microstructural properties and oxidation resistance of Sn-Zn eutectic alloy10.1016/j.jallcom.2006.12.037 ↗
12. Directional solidification of aluminium-copper alloys10.1016/S0921-5093(01)01649-5 ↗
13. Effects of Solidification Thermal Parameters on Microstructure and Mechanical Properties of Sn-Bi Solder Alloys10.1007/s11664-016-5225-7 ↗
14. Mathematical model for the unidirectional solidification of metals: I. cooled molds10.1007/BF02654420 ↗
15. Mathematical model for the unidirectional solidification of metals: II. Massive molds10.1007/BF02653977 ↗
16. Garcia LR · 2008
17. Lamellar and Rod Eutectic Growth
18. Enhancing mechanical response of hypoeutectic Sn-6. 5Zn solder alloy using Ni and Sb additions10.1016/j.matdes.2013.06.023 ↗
19. Dendritic Growth, Eutectic Features and Their Effects on Hardness of a Ternary Sn-Zn-Cu Solder Alloy10.1007/s40195-017-0572-9 ↗
20. Dieter GE · 1988
21. Meyers M · 2009