Abstract

This study investigates the effect of hydrothermal aging on the properties of glass fiber reinforced polymer (GFRP) rebars manufactured with isophthalic polyester or vinylester resin and glass fiber type E. The GFRP rebars were immersed in an alkaline solution (pH 12.6) for 1000 h at different temperatures (23 and 60 ºC), and their deterioration was evaluated based on microstructural and chemical changes (using SEM, DSC, XRF, and FTIR techniques), moisture absorption, and variation in mechanical properties. The results indicated an increase in the presence of voids and water absorption of the rebars with accelerated aging, with a reduction in the glass transition temperature of the resin and alteration of the chemical composition of the glass fiber. The comparison between the experimental results indicates that the rebars with matrix in vinylester resin present greater chemical resistance than the rebars with a polyester matrix. The degradation of the rebar also resulted in a reduction of approximately 6% in the tensile strength of the rebar and 2% in the modulus of elasticity. Using the damage model, it was possible to identify that the reduction in mechanical strength was associated with the simultaneous degradation of the resin and glass fiber due to the alkaline attack.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Structural Behavior of Reinforced Concrete · Concrete Corrosion and Durability · Innovative concrete reinforcement materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Universidade Federal da Bahia, Brasil

Universidade Estadual de Feira de Santana, Brasil

References (50)

Show source-provided references
1. Statistical study of corrosion types in constructions in south region of Rio de Janeiro – Brasil
2. Effect of the environment on the performance of GFRP reinforcing bars10.1016/j.compositesb.2017.12.037 ↗
3. Durability of glass fibre-reinforced polymer (GFRP) bars embedded in concrete under various environments. I: experiments and analysis
4. A mechanical and environmental assessment and comparison of basalt fibre reinforced polymer (BFRP) bar and steel bar in concrete beams10.1016/j.egypro.2017.03.005 ↗
5. Glass fibre sizing: a review10.1016/j.compositesa.2019.105619 ↗
6. Durability and degradation mechanisms of GFRP reinforced subjected to severe environments and sustained stress10.1016/j.conbuildmat.2018.03.092 ↗
7. Kinetics of processes modeling corrosion of glass fibers mixed into concrete10.13168/cs.2017.0012 ↗
8. Water absorption and distribution in a pultruded unidirectional carbon/glass hybrid rod under hydraulic pressure and elevated temperatures
9. Water absorption, hydrothermal expansion, and thermomechanical properties of a vinylester resin for fiber-reinforced polymer composites subjected to water or alkaline solution immersion
10. 2006
11. Degradation of glass fiber-reinforced plastic composites containing nanoclay in alkaline environment10.1177/0021998311401064 ↗
12. Durability of glass polymer composites subject to stress corrosion
13. Properties of aged GFRP reinforcement grids relared to fatigue life and alkaline environment10.3390/app7090897 ↗
14. Effect of alkaline conditioning and temperature on the properties of glass fiber polymer composite bar
15. Statistical analysis and theorical predictions of the tensile-strength retention of glass fiber-reinforced polymer bars based on resin type10.1177/0021998318755866 ↗
16. Laboratory assessment and durability performance of vinyl-ester, polyester, and epoxy glass-FRP bars for concrete structures10.1016/j.compositesb.2017.02.002 ↗
17. 2015
18. 2007
19. FRP reinforced bars – designs and methods of manufacture10.1007/s11029-013-9355-1 ↗
20. 2020
21. 2015
22. 2016
23. 2019
24. 2018
25. Durability of FRP rods for concrete structures10.1016/j.conbuildmat.2004.04.012 ↗
26. Durability characteristics of nano-GFRP composites reinforcing bars for concrete structures in moist and alkaline environments10.1016/j.compstruct.2011.11.006 ↗
27. Duncan C · 2007
28. 2008
29. Pansart S · 2013
30. Microstructural investigation of glass fiber reinforced polymer bars10.1016/j.compositesb.2016.11.029 ↗
31. Accelerated aging tests for evaluations of durability performance of FRP reinforcing bars for concrete structures10.1016/j.compstruct.2005.08.015 ↗
32. Padmavathi SV · 2006
33. The water ageing of unsaturated polyester-based composites: influence of resin chemical structure10.1016/0010-4361(83)90160-X ↗
34. Effects of water, salt solution and simulated concrete pore solution on the properties of composite matrix resins used in civil engineering applications10.1002/pc.10538 ↗
35. Laboratory characterization and evaluation of durability performance of new polyester and vinylester E-glass GFRP dowels for jointed concrete pavement10.1061/(ASCE)CC.1943-5614.0000317 ↗
36. Shear properties and durability of GFRP reinforcement bar aged in seawater10.1016/j.polymertesting.2019.02.033 ↗
37. Sorption and diffusion of water, salt water, and concrete pore solution in composite matrices10.1002/(SICI)1097-4628(19990118)71:3<483::AID-APP15>3.0.CO;2-S ↗
38. Aging in water and in an alkaline medium of unsaturated polyester and epoxy resins: experimental study and modeling
39. Modified one-dimensional fickean solution for moisture absorption in composites10.1177/073168449000900402 ↗
40. Long term durability of pultruded polymer composite bar in concrete environment10.1016/j.matdes.2014.01.049 ↗
41. Durability of GFRP rebars in simulated concrete solutions under accelerated aging conditions10.1061/(ASCE)CC.1943-5614.0000168 ↗
42. Water absorption and distribution in a pultruded unidirectional carbon/glass hybrid rod under hydraulic pressure and elevated temperatures
43. Effects of environmental exposure on Fiber-Reinforced Plastic (FRP) materials used in construction10.1520/CTR10120J ↗
44. Comparative durability of GFRP composite reinforcing bars in concrete and simulated concrete environments10.1016/j.cemconcomp.2020.103564 ↗
45. Weitsman YJ · 2012
46. Chemical resistance of carbon, basalt and glass fibers used in FRP reinforcing bars10.1177/0021998319844306 ↗
47. Residual tensile strength of dry and impregnated fibres after exposure to alkaline environments10.1016/j.compositesb.2017.03.005 ↗
48. Combined effects of saline solution and moist concrete on long-term durability of GFRP reinforcing bars10.1016/j.conbuildmat.2012.08.021 ↗
49. 2006
50. Long-term durability of basalt and glass fiber reinforced polymer (BFRP/GFRP) bars in seawater and sea sand concrete environment10.1016/j.conbuildmat.2017.02.038 ↗