Effect of grain size changes on corrosion behavior of copper produced by accumulative roll bonding process
Source abstract
Abstract
The effect of changes in grain size on corrosion resistance of the pure tough pitch copper stripwas investigated in acidic and alkaline NaCl solutions. Accumulative roll bonding as sever plastic process was applied up to 8 cycles to produce the ultrafine graincopper. Polarization and electrochemical impedance tests were used for corrosion resistance investigations. Corrosion morphologies were analyzed by FE-SEM. Results showed that the corrosion resistance decreased up to cycle 2 and increased after rolled for the fourth time due to UFG grain formation after cycle 4. The corrosion degradation in cycle 8 was uniformand it was more intergranular for the sample of cycle 2 and the unrolled counterpart.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Petroleum University of Technology, Iran
ShahidChamran University, Iran
Isfahan University of Technology, Iran
References (33)
Show source-provided references
1. Materials with ultrafine microstructures: Retrospectives and perspectives10.1016/0965-9773(92)90045-Y ↗
2. Materials processing by simple shear10.1016/0921-5093(95)09705-8 ↗
3. A comparison of the properties of SPD-processed AA-6061 by equal-channel angular pressing, multi-axial compressions/forgings and accumulative roll bonding
4. Improving corrosion resistance of RE-containing magnesium alloy ZE41A through ECAP10.1016/S1002-0721(08)60348-8 ↗
5. Corrosion behavior of ultra-fine grained industrial pure Al fabricated by ECAP10.1016/S1003-6326(08)60407-0 ↗
6. Effect of the number of ECAP pass time on the electrochemical properties of 1050 Al alloys10.1016/j.msea.2003.08.056 ↗
7. Impact of ultrafine-grained microstructure on the corrosion of aluminium alloy AA202410.1016/j.corsci.2011.12.016 ↗
8. Novel ultra-high straining process for bulk materials-development of the accumulative roll-bonding (ARB) process10.1016/S1359-6454(98)00365-6 ↗
9. Huang X · 2001
10. ARB (Accumulative Roll-Bonding) and other new Techniques to Produce Bulk Ultrafine Grained Materials10.1002/adem.200310077 ↗
11. Nano-grained copper strip produced by accumulative roll bonding process10.1016/j.msea.2007.03.065 ↗
12. Reciprocating wear resistance of Al-SiC nano-composite fabricated by accumulative roll bonding process10.1016/j.matdes.2013.03.047 ↗
13. Gordo PM · 2009
14. Corrosion and ion release behavior of ultra-fine grained bulk pure copper fabricated by ECAP in Hanks solution as potential biomaterial for contraception10.1016/j.matlet.2009.11.065 ↗
15. Corrosion of ultra-fine grained copper fabricated by equal-channel angular pressing10.1016/j.corsci.2008.01.024 ↗
16. Effect of equal-channel angular pressing on pitting corrosion resistance of anodized aluminum-copper alloy10.1016/S1003-6326(08)60374-X ↗
17. Corrosion investigation of Al-SiC nano-composite fabricated by accumulative roll bonding (ARB) process10.1016/j.jallcom.2012.10.069 ↗
18. Evaluation of corrosion properties of Al/nanosilica nanocomposite sheets produced by accumulative roll bonding (ARB) process10.1016/j.jallcom.2013.04.090 ↗
19. Mechanical and corrosion resistance of a new nanostructured Ti-Zr-Ta-Nb alloy10.1016/j.jmbbm.2011.05.012 ↗
20. Corrosion and tensile behaviors of ultra-fine grained Al-Mn alloy produced by accumulative roll bonding
21. On the chloride-induced pitting of ultra fine grains 5052 aluminum alloy produced by accumulative roll bonding process10.1016/j.jallcom.2011.01.066 ↗
22. On the corrosion behaviour of ultra-fine grain copper10.1016/S1359-6462(99)00170-0 ↗
23. Stress corrosion cracking susceptibility of ultra-fine grain copper produced by equal-channel angular pressing10.1016/S0921-5093(01)01332-6 ↗
24. The influence of microstructure on the corrosion properties Cu polycrystals prepared by ECAP
25. Kinetics and mechanism of palladium electrodeposition on graphite electrode by impedance and noise measurements10.1016/j.jelechem.2011.09.012 ↗
26. Note on the parameterization of the constant-phase admittance element10.1016/0167-2738(84)90049-3 ↗
27. Effect of trace phosphorous on tensile behavior of accumulative roll bonded oxygen-free copper10.1016/j.scriptamat.2004.09.005 ↗
28. Mechanical Properties of SPD (Severe Plastic Deformation) Processed Copper
29. Effects of two fungicides on the corrosion resistance of copper in 3.5% NaCl solution under various conditions10.1016/j.corsci.2010.11.006 ↗
30. Electrochemical corrosion of unalloyed copper in chloride media: a critical review10.1016/S0010-938X(02)00257-3 ↗
31. The Influence of pH on Electrochemical Behavior of Copper in Presence of Chloride Ions10.1016/S1452-3981(23)15159-5 ↗
32. Corrosion behavior of AISI 4130 steel alloy in ethylene glycol-water mixture in presence of molybdate10.1016/j.matchemphys.2012.05.041 ↗
33. Kinetics of the hydrogen evolution reaction on NiMn graphite modified electrode10.1016/j.ijhydene.2011.06.106 ↗