Abstract

The solidification behavior of the Al-12.6% Si (A1), the hypereutectic Al-20%Si (A2) and the Al-20%Si-1.5% Fe-0.5%Mn (A3) (in wt. (%)) alloys, at different cooling rates is reported and discussed. The cooling rates ranged between 0.93 °C/s and 190 °C/s when cast in sand and copper wedge-shaped molds, respectively. A spheroidization heat treatment was carried out to the alloys in the as-cast condition at 540 °C for 11 hours and quench in water with a subsequent heat treatment at 170 °C for 5 hours with the purpose of improving the mechanical properties. The samples were characterized by optical microscopy, scanning electron microscopy and mechanically by tensile test, in order to evaluate the response of the heat treatment on the different starting microstructures and mechanical properties. It was found that alloys cooled at rates greater than 10.8 °C/s had a smaller particle size and better distribution, also showed a greater response to spheroidization heat treatment of all silicon (Si) phases. The spheroidization heat treatment caused an increase in the ultimate tensile stress (UTS) and elongation when compared with the alloys in the as-cast condition. The highest UTS value of 174 MPa was obtained for the (A1) alloy.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Instituto Politécnico Nacional, México

Universidad Nacional Autónoma de México, México

References (25)

Show source-provided references
1. Mechanical Properties and Fracture Behavior of an Ultrafine-Grained Al-20 Wt Pct Si Alloy10.1007/s11661-005-0187-z ↗
2. Precipitation of Si particles in a super rapidly solidified Al-Si hypereutectic alloy10.1016/S0254-0584(03)00030-0 ↗
3. Development of High Wear Resistance Al-Si Alloy10.2320/materia1962.24.307 ↗
4. Solidification behavior of Al-Si-Fe alloys and phase transformation of metaestable intermetallic compound by heat treatment10.1023/A:1004584415196 ↗
5. Modeling of Irregular Eutectic Microstructures in Solidification of Al-Si Alloys10.1007/s11661-004-0262-x ↗
6. Inhibited Coarsening of a Spray-Formed and Extruded Hypereutectic Aluminum-Silicon Alloy in the Semisolid State10.1007/s11661-005-0147-7 ↗
7. Influence of modification, solidification conditions and heat treatment on the microstructure and mechanical properties of A356 aluminum alloy10.1023/B:JMSC.0000017764.20609.0d ↗
8. Impact toughness in Al-12Si and Al-12Si-3Cu cast alloys-Part 1: effect of process variables and microstructure10.1016/j.ijimpeng.2007.03.002 ↗
9. Silicon morphology modification in the eutectic Al-Si alloy using mechanical mold vibration10.1016/j.msea.2004.09.038 ↗
10. Influence of Silicon Morphology and Mechanical Properties of Piston Alloys10.1081/AMP-200055138 ↗
11. On the silicon spheroidization in Al-Si alloys10.1016/S1471-5317(03)00010-5 ↗
12. Vacuum assisted high pressure die casting of aluminum alloys10.1016/S0924-0136(00)00545-8 ↗
13. Rapid solidification processing with specific application to aluminum alloys10.1179/imr.1992.37.1.1 ↗
14. Property improvement in Al-Si alloys through rapid solidification processing10.1016/S0924-0136(97)00198-2 ↗
15. The microstructure and mechanical properties of spray deposited hypereutectic Al-Si-Fe alloy10.1016/S0924-0136(02)01074-9 ↗
16. The effect of iron and manganese on the formation of intermetallic compounds in aluminum-silicon alloys10.1016/S0921-5093(04)00832-9 ↗
17. Fasm, The principles of Materials Selection for Engineering Design
18. Belov NA · 2002
19. Characterization of microstructures obtained in wedge shaped Al-Zn-Mg alloys10.1016/j.jallcom.2009.11.106 ↗
20. Rapidly Solidified Al-6Si-3Cu alloy10.4028/www.scientific.net/MSF.570.103 ↗
21. Microstructural evolution of Al-20Si-5Fe alloy during rapid solidification and hot consolidation10.1007/s12598-009-0122-3 ↗
22. Microstructure and phase formation in spray-deposited Al-18%Si-5%Fe-1.5%Cu alloy10.1016/S0167-577X(02)00616-X ↗
23. Effet des conditions de solidification sur la qualité des alliage de fonderie de A-U5 G T et A-S7 G, estimation des caractéristiques mécaniques
24. The mutual effect of iron and manganese on microstructure and mechanical properties of aluminum-silicon alloys
25. The effect of Mn additions on the microstructure and mechanical properties of Al-Si-Cu casting alloys10.1016/j.msea.2007.12.026 ↗