Effect of Hydrogen on the Mechanical Properties of ASTM A182 F22 and ASTM A36 Steels Welded Joint Using Inconel 625 as Filler and Buttering Metal
Source abstract
Abstract
ASTM A 182 F22 steel, used in components subsea for oil extraction, are previously buttered with ductile metal such as Inconel 625, before being welded to steel pipes similar to ASTM A36 steels. The thermal buttering weld cycle provides the formation of high hardness micro-phases and carbides at the interface between F22 steel and the buttering with Inconel, which when in contact with hydrogen, originating from the cathodic protection applied to these equipment, can lead to the embrittlement of this region, causing fragile fractures. In this work, ASTM A 182 F22 steel, buttered with Inconel 625 and welded to A36 steel, submitted to post-weld heat treatment without hydrogenation and subjected to cathodic protection for hydrogen permeation were submitted to fracture toughness test. The welds and buttering were done using GMAW process with AWS ERNiCrMo-3 wire as filler and buttering metal and a mixture of Ar and He as shield gas. The results indicated a 56% of area reduction, and 15% in the elongation values in the tensile tests, in addition to a 13.3% reduction in the CTOD value, for welded joints subjected to hydrogen permeation, which showed a quasi-cleavage fracture mechanism.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Universidade Federal Rural do Semi-Árido, Brasil
Universidade Federal da Paraíba, Brasil
References (28)
Show source-provided references
1. In-situ neutron diffraction measurement of stress redistribution in a dissimilar joint during heat treatment10.1016/j.msea.2014.12.095 ↗
2. Sulphide stress cracking behaviour of the dissimilar metal welded joint of X60 pipeline steel and Inconel 625 alloy10.1016/j.corsci.2016.04.044 ↗
3. Dissimilar metal welding of P91 steel-AISI 316L SS with Incoloy 800 and Inconel 600 interlayers by using activated TIG welding process and its effect on the microstructure and mechanical properties10.1016/j.jmatprotec.2019.116280 ↗
4. Effect of buffer-layered buttering on microstructure and mechanical properties of dissimilar metal weld joints for nuclear plant application10.1016/j.msea.2016.04.053 ↗
5. Hydrogen embrittlement: the game changing factor in the applicability of nickel alloys in oilfield technology
6. Fenske JA · 2010
7. Olden V · 2003 · 1
8. de Oliveira GLG · 2013
9. Dodge MF · 2014
10. 2009 · 1
11. Silva AN · 2018
12. 2010
13. 2013
14. Beaugrand VCM · 2009 · 1
15. Dodge MF · 2014 · 1
16. Bourgeois D · 2015
17. Microstructure and hydrogen-induced failure mechanisms in Fe and Ni alloy weldments10.1007/s11661-012-1129-1 ↗
18. Butter-weld interface microstructural analysis employing NCS and LAMS sections10.1590/1980-5373-mr-2019-0018 ↗
19. Low heat input gas metal arc welding for dissimilar metal weld overlays part II: the transition zone
20. The effect of postweld heat treatment on hydrogen-assisted cracking of F22/Alloy 625 overlays10.29391/2018.97.007 ↗
21. Fenske JA · 2011 · 1
22. 2003
23. Influence of hydrogen and low temperature on pipeline steels mechanical behaviour10.1016/j.proeng.2011.04.533 ↗
24. Hydrogen-enhanced localized plasticity--a mechanism for hydrogenrelated fracture10.1016/0921-5093(94)90975-X ↗
25. The influence of ductile tearing on fracture energy in the ductile-to-brittle transition temperature range10.1016/S0921-5093(01)01913-X ↗
26. Effect of hydrogen and low temperature on fatigue crack growth of pipeline steels10.1016/j.engfracmech.2012.09.023 ↗
27. Tempering effect on the fusion boundary region of alloy 625 weld overlay on 8630 steel10.1007/s40194-018-0560-3 ↗
28. Gittos MF · 2008 · 19