Effects of Pre-Strain on the Evolution of Microstructure and Strain Hardening of Extruded Az31 Magnesium Alloy
Source abstract
Abstract
Pre-compression 3% and pre-stretch 3% subsequent annealing at 200ºC for 2h are conducted on AZ31 magnesium alloys, then inverse tensile and compressive deformation are carried out at room temperature, respectively. During inverse tension 3% deformation on 1st pre-compression samples, detwinning behavior happens; after 2nd pre-compression 3%, the volume fraction of {10-12} extension twins decreases comparing with 1st pre-compression. Due to the interaction of dislocation and induced twinning lamellas, strain hardening rate (θ) increases on 1st and 2nd pre-compression samples. {10-12} tensile twinning is restrained during inverse compressive deformation by pre-stretch process. Owing to the decreasing amount of twins, the texture strengthening in compressive deformation weakens. So the slop of stage III in strain hardening rate sustaining reduces after 1st pre-stretch 3% and 2nd pre-stretch 3% deformation during inverse compression deformation.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Shanxi ley laboratory of advanced magnesium-based materials, China; Taiyuan University of Technology, China; Taiyuan University of Technology, China
Shanxi ley laboratory of advanced magnesium-based materials, China
National University of defense technology, China
Taiyuan University of Technology, China
References (24)
Show source-provided references
1. Deep drawability and drawing behaviour of AZ31 alloy sheets with different initial texture10.1016/j.jallcom.2014.06.199 ↗
2. The effect of high yttrium solute concentration on the twinning behaviour of magnesium alloys10.1016/j.actamat.2014.09.022 ↗
3. Influence of aluminum content on twinning and texture development of cast Mg-Al-Zn alloy during compression10.1016/j.jallcom.2014.10.096 ↗
4. Effects of texture and grain size on mechanical properties of AZ80 magnesium alloys at lower temperatures10.1016/j.matdes.2015.09.153 ↗
5. Influence of grain orientation on twinning during warm compression of wrought Mg-3Al-1Zn10.1179/174328405X71710 ↗
6. Grain size effect on deformation twinning in Mg-Al-Zn alloy10.1179/1743284713Y.0000000237 ↗
7. Improving tensile and compressive properties of magnesium alloy plates by pre-cold rolling10.1016/j.scriptamat.2012.02.047 ↗
8. Reducing the tension-compression yield asymmetry in a hot-rolled Mg-3Al-1Zn alloy via multidirectional pre-compression10.1016/j.msea.2012.11.127 ↗
9. Improved strength and ductility of magnesium alloy below micro-twin lamellar structure
10. The effect of pre-compressive strain on the fatigue life of the AZ31 magnesium alloy10.1016/j.msea.2014.03.027 ↗
11. Tailoring the texture of magnesium alloy by twinning deformation to improve the rolling capability10.1016/j.scriptamat.2011.02.010 ↗
12. Improved formability of Mg-3Al-1Zn alloy by pre-stretching and annealing10.1016/j.scriptamat.2012.06.017 ↗
13. Influence of pre-deformation and subsequent annealing on strain hardening and anisotropy of AM30 magnesium alloy10.1016/j.jallcom.2014.05.133 ↗
14. Understanding low-cycle fatigue life improvement mechanisms in a pre-twinned magnesium alloy10.1016/j.jallcom.2015.09.247 ↗
15. Dependence of compressive deformation on pre-strain and loading direction in an extruded magnesium alloy: Texture, twinning and de-twinning10.1016/j.msea.2013.12.038 ↗
16. Strengthening and toughening of magnesium alloy by {10 −12} extension twins10.1016/j.scriptamat.2011.09.033 ↗
17. Role of {10-12} twinning characteristics in the deformation behavior of a polycrystalline magnesium alloy10.1016/j.actamat.2010.07.002 ↗
18. Microstructure evolution and mechanical properties of twinned AZ31 alloy plates at lower elevated temperature10.1016/j.jallcom.2014.07.045 ↗
19. Plastic anisotropy and the role of non-basal slip in magnesium alloy AZ31B10.1016/j.ijplas.2004.05.018 ↗
20. Research of Bauschinger Effect of AZ31 Magnesium Alloy
21. Effect of crystal orientation on the mechanical properties and strain hardening behavior of magnesium alloy AZ31 during uniaxial compression10.1016/j.msea.2011.12.013 ↗
22. Influence of {10-12} extension twinning on the flow behavior of AZ31 Mg alloy10.1016/j.msea.2006.09.069 ↗
23. Internal strain and texture evolution during deformation twinning in magnesium10.1016/j.msea.2005.02.016 ↗
24. The effect of twinning and detwinning on the mechanical property of AZ31 extruded magnesium alloy during strain-path changes10.1016/j.matdes.2014.05.056 ↗