Effect of voltage and spray–off distance of electric-arc spray technique on surface properties of nickel–chrome (Ni–Cr) coating developed on 304L stainless steel
Source abstract
Abstract
Abstract Nickel–chrome coatings are widely used to improve surface properties and service life of engineering components made from different ferrous and non–ferrous alloys. Herein, an attempt has been made to investigate the impact of various voltages ranging from 26–30 V and spray–off distances ranging from 100–300 mm of electric-arc spray technique on the surface properties of Ni–Cr coating developed on 304L stainless steel. Thickness, porosity, surface morphology, surface roughness, and hardness of Ni–Cr coatings were determined to study the impact of deposition parameters. Coating deposition at 26 V exhibited the lowest porosity and the highest percentage of Cr nodules among all samples. The comparison study showed that coating deposit developed at 26 V and 100 mm spray–off distance has a maximum thickness, followed by coating developed at 30 V and 100 mm spray–off distance. This indicated that coating deposit developed at 100 mm spray–off distance results in thicker coatings. Maximum hardness was achieved at 30 V and 300 mm spray–off distance. The shorter spray–off distance revealed that coatings tend to be thicker and harder resulting in longer coating life.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Surface Treatment and Coatings
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Effect of La2O3 addition on the microstructure, hardness and abrasive wear behavior of flame sprayed Ni based coatings10.1016/j.wear.2008.12.029 ↗
2. Davis · 2004
3. Microstructure of Ni–Cr–based coating for corrosive conditions10.1007/s11666-019-00936-3 ↗
4. Effect of flame spray deposition parameters on the microstructure of Al2O3-13% TiO2 coatings applied onto 7075 aluminum alloy10.1590/1980-5373-mr-2018-0038 ↗
5. Influence of process parameters on the quality of thermally sprayed X46Cr13 stainless steel coatings10.1590/S1678-58782004000100016 ↗
6. Post-processing of Ni–Cr–Al2O3 Thermal spray coatings through friction stir processing for enhanced erosion–corrosion performance10.1007/s11666-019-00891-z ↗
7. High velocity oxygen fuel sprayed Cr3C2–Ni–Cr–B–Si coatings on inconel 718 using design of experiments
8. Evaluation of corrosion resistance and characterization of Ni-Cr coated structure using plasma spray coating for marine hulls10.1007/s11468-018-0838-8 ↗
9. Studies on the properties of high-velocity oxy-fuel thermal spray coatings for higher temperature applications10.1007/s11003-006-0047-z ↗
10. Stokes · 2005
11. Stern · 1996
12. Grainger · 1998
13. Influence of the thermal-spray procedure on the properties of a nickel-chromium coating10.1023/A:1013742213115 ↗
14. Electroless deposition of silver nano particles on thionyl chloride and hydrazine monohydrate treated multi walled carbon nano-tubes10.1088/2053-1591/aac5be ↗
15. A review-study of thermal spray coatings for corrosive wear
16. 2001A comparative study of high-temperature erosion wear of plasma-sprayed NiCrBSiFe and WC–NiCrBSiFe coatings under simulated coal-fired boiler conditions10.1016/S0301-679X(00)00146-8 ↗
17. Review of applications of thermal spraying in the printing industry in respect to OEMs
18. Coatings for gas turbine materials and long term stability issues10.1016/j.matdes.2004.02.005 ↗
19. Effect of surface profile of mild steel substrate upon adhesion strength of WC-11% Co flame spray coating
20. Mechanical properties of CNT reinforced hybrid functionally graded materials for bioimplants10.1016/S1003-6326(14)63293-3 ↗
21. Wear behavior of flame sprayed NiCrBSi coating remelted by flame or by laser10.1016/j.wear.2006.05.009 ↗
22. The thermal spray roadmap10.1007/s11666-016-0473-x ↗
23. Mechanical characterization of copper coated carbon nanotubes reinforced aluminum matrix composites10.1016/j.matchar.2013.09.006 ↗
24. Tribological behavior of thermal spray coatings, deposited by HVOF and APS techniques, and Composite Electrodeposits Ni/SiC at Both Room Temperature and 300 °C
25. NiCr coatings on stainless steel by HVOF technique10.1016/S0257-8972(03)00367-0 ↗
26. Mechanical and metallurgical properties of plasma sprayed and laser remelted Ni–20Cr and Stellite-6 coatings10.1016/j.jmatprotec.2004.05.023 ↗