Effect of particle size and high-energy ball milling time on microstructure and mechanical properties of WC-10Co cemented carbides with plate-like WC grains
Source abstract
Abstract
The effect of particle size and high-energy ball milling time on microstructure and mechanical properties of WC-10Co cemented carbides with plate-like WC grains were studied using a scanning electron microscope, x-ray diffraction and mechanical properties tests. The results show that coarsening W particle size seemed to be beneficial for the increase of the plate-like WC content due to the easy acquirement of the thin W flake with high-density defects. Additionally, increasing the ball milling time could first increase the content of plate-like WC grains, and then decrease with 96 h ball milling. The high amount of defects and activity of fine W particles from fracturing with long ball milling time could enhance the formation of plate-like WC grains. However, the oxygen content could be increased with the excess ball milling time, which reduced the content of liquid Co and thus impeded the formation of plate-like WC grains. As the content of plate-like WC grains increased, the intergranular fracture gradually transformed into the main fracture mode. Additionally, crack bridging and crack path deflection could be seen in the alloy with plate-like WC grains. The high fracture surface area and energy required for crack propagation could improve the strength of WC-10Co cemented carbides with plate-like WC.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Tunneling and Rock Mechanics · Orthopaedic implants and arthroplasty
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. 10.1016/j.ijrmhm.2018.12.00410.1016/j.ijrmhm.2018.12.004 ↗
2. Tu X · Mater. Res. Express · 2019 · 6
3. Shoufa L · Mater. Res. Express · 2018 · 510.1088/2053-1591/aad535 ↗
4. 10.1016/j.ijrmhm.2017.10.00510.1016/j.ijrmhm.2017.10.005 ↗
5. 10.1016/j.jallcom.2018.03.19710.1016/j.jallcom.2018.03.197 ↗
6. 10.1016/j.ceramint.2018.03.17410.1016/j.ceramint.2018.03.174 ↗
7. Shang Y · Mater. Res. Express · 2019 · 610.1088/2053-1591/ab1553 ↗
8. 10.1016/j.ceramint.2016.08.11910.1016/j.ceramint.2016.08.119 ↗
9. 10.1016/j.msea.2016.02.02110.1016/j.msea.2016.02.021 ↗
10. 10.1016/j.jeurceramsoc.2014.05.04510.1016/j.jeurceramsoc.2014.05.045 ↗
11. 10.1016/j.matdes.2018.04.02510.1016/j.matdes.2018.04.025 ↗
12. Feng Q · Nanotechnology · 2017 · 28
13. 10.2497/jjspm.47.52610.2497/jjspm.47.526 ↗
14. 10.1111/j.1551-2916.2006.01218.x10.1111/j.1551-2916.2006.01218.x ↗
15. 10.2320/matertrans.M201038010.2320/matertrans.M2010380 ↗
16. 10.1016/j.msea.2012.01.00510.1016/j.msea.2012.01.005 ↗
17. 10.1016/j.matchemphys.2017.01.01010.1016/j.matchemphys.2017.01.010 ↗
18. 10.1016/j.ijrmhm.2014.06.02410.1016/j.ijrmhm.2014.06.024 ↗
19. 10.1016/j.matdes.2017.02.01010.1016/j.matdes.2017.02.010 ↗
20. 10.1016/j.actamat.2018.02.01810.1016/j.actamat.2018.02.018 ↗
21. 10.1016/j.ijrmhm.2009.05.00610.1016/j.ijrmhm.2009.05.006 ↗
22. 10.1016/j.ijrmhm.2013.09.00610.1016/j.ijrmhm.2013.09.006 ↗
23. 10.1016/j.actamat.2011.03.01810.1016/j.actamat.2011.03.018 ↗
24. 10.1016/0039-6028(76)90190-410.1016/0039-6028(76)90190-4 ↗
25. 10.1016/S0263-4368(01)00069-510.1016/S0263-4368(01)00069-5 ↗
26. 10.1016/S0921-5093(02)00246-010.1016/S0921-5093(02)00246-0 ↗
27. 10.1016/j.jallcom.2019.06.32810.1016/j.jallcom.2019.06.328 ↗
28. 10.1016/j.actamat.2003.12.02410.1016/j.actamat.2003.12.024 ↗
29. 10.1016/j.actamat.2004.12.01710.1016/j.actamat.2004.12.017 ↗
30. 10.1016/j.msea.2006.10.15710.1016/j.msea.2006.10.157 ↗
31. 10.1016/j.ijrmhm.2005.11.00410.1016/j.ijrmhm.2005.11.004 ↗
32. 10.1016/j.jeurceramsoc.2015.04.02110.1016/j.jeurceramsoc.2015.04.021 ↗
33. 10.1016/j.ceramint.2015.07.08610.1016/j.ceramint.2015.07.086 ↗