Study on the microstructures of Al-2.5%Mn alloy
Source abstract
Abstract
Abstract The effect of Sr and cooling rate on the microstructure of Al-2.5%Mn alloy was studied by OM, SEM and XRD. The results showed that Sr not only refined the primary phase, but also refined eutectic microstructures. However, there was obvious delamination in the alloy. When the content of Sr was 0.2%–0.65%, the primary phase in the upper part of alloy changed from coarse needle and lath-shaped to fine block and needle-like. With the Sr content increased, the needle-like structure in the alloy tended to be more and longer, but the size of α-Al tended to be finer. At the bottom, there were many large massive phases, which were much more refined than the primary phase without Sr With the cooling rate increased, the primary phase was refined greatly and almost all of them transformed into eutectic microstructure. Besides, the delamination of microstructure disappeared.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Formation and microstructure of quasicrystals in suction cast Al-6 wt% Mn alloys with additions of nickel and iron elements10.1002/mawe.201700128 ↗
2. Research present situation of Al–Mn alloys
3. Improvement in the mechanical properties and creep resistance of Al–Mn–Mg 3004 alloy with Sc and Zr addition10.1016/j.msea.2018.05.055 ↗
4. Effects of homogenisation treatment on microstructure and grain refinement of Al–1.2Mn alloy10.1080/02670836.2017.1407565 ↗
5. Evolution of microstructure in Al–Mn alloy with a low ratio of Fe/Si during homogenization10.1016/S1875-5372(18)30200-5 ↗
6. Improved strength and enhanced pitting corrosion resistance of Al–Mn alloy with Zr addition10.1016/j.matlet.2019.126535 ↗
7. The effects of Mn concentration on the tribocorrosion resistance of Al–Mn alloys10.1016/j.wear.2017.03.017 ↗
8. Effect of Fe, Si and cooling rate on the formation of Fe- and Mn-rich intermetallics in Al–5Mg–0.8Mn alloy10.1016/j.jmst.2015.10.010 ↗
9. The effect of heating rate on the softening behaviour of a deformed Al–Mn alloy with strong and weak concurrent precipitation10.1016/j.matchar.2015.10.033 ↗
10. Microstructure control and high temperature performance of Al–Mn alloys
11. Influence of TiB2 nanoparticles on elevated-temperature properties of Al–Mn–Mg 3004 alloy10.1016/S1003-6326(17)60088-8 ↗
12. Structure and properties studies of rapidly solidified Al–Mn alloys10.4028/www.scientific.net/KEM.682.199 ↗
13. Effect of Zr addition on microstructure and properties of Al−Mn−Si−Zn-based alloy10.1016/S1003-6326(14)63545-7 ↗
14. Effect of magnesium on the dispersion phase of Al–Mn–Mg–Si(3xxx) alloy dispersion
15. Effect of high magnetic fields on the solidification microstructure of an Al-Mn alloy10.1007/s12598-009-0059-6 ↗
16. Microstructure control and high temperature properties of Al–Mn-based alloys10.11900/0412.1961.2017.00010 ↗
17. Evolution of microstructure and elevated-temperature properties with Mn addition in Al–Mn–Mg alloys10.1557/jmr.2017.239 ↗
18. Effect of Cr content and cooling rate on the primary phase of Al-2.5Mn alloy10.1007/s12613-019-1862-1 ↗
19. Effect of cooling rate on solidification structure of Mg_8Gd_1Er alloy