Self-flux synthesis and photoluminescent properties of LiAl5O8
Source abstract
Abstract
Abstract Pure-phase LiAl5O8 was selected as an oxide ceramic red phosphor material without dopants (color centers) and was synthesized using a self-flux method. The LiAl5O8 was formed by heating a powder mixture consisting of γ-Al2O3:Li2SO4 = 1:2 (molar ratio) at over 1100 °C for 1 h. Photoluminescence (PL) properties for the synthesized LiAl5O8 were investigated. The maximum intensity of the excitation spectrum for the photoluminescent emission of LiAl5O8 synthesized was at 274 nm. The peak intensity of the emission spectrum was at a wavelength of 667 nm (red color). The intensity of the peak emission spectrum increased with the heating temperature, i.e., the maximum peak intensity of the red emission spectrum was detected for the LiAl5O8 synthesized by heating at 1500 °C for 1 h.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Luminescence Properties of Advanced Materials · Microwave Dielectric Ceramics Synthesis · Advanced Photocatalysis Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. R.S. Roth, Phase Equilibria Diagrams, Ed. by National Institute of Standards and Technology, vol. 8, Am. Ceram. Soc., Columbus Ohio, USA (2001) Fig.10335 (A).
2. Kutty · J. Alloy Compd. · 1998 · 269 · 7510.1016/S0925-8388(98)00159-5 ↗
3. Inoue · J. Mater. Sci. · 2006 · 41 · 126910.1007/s10853-005-4232-5 ↗
4. Inoue · J. Ceram. Soc. Jpn. · 2006 · 114 · 62010.2109/jcersj.114.620 ↗
5. Tang · Ceram. Int. · 2000 · 26 · 34110.1016/S0272-8842(99)00061-9 ↗
6. Okamoto · J. Appl. Phys. · 1999 · 86 · 559410.1063/1.371565 ↗
7. Park · Appl. Phys. Lett. · 2000 · 77 · 216210.1063/1.1315341 ↗
8. Brain · 1995
9. JCPDS card: 38-1425, JCPDS International Centre for Diffraction Data.