Effect of combined rolling with subsequent aging on the structure, mechanical and fatigue properties of β titanium alloy
Source abstract
Abstract
Abstract In the paper the effect of radial-shear and groove rolling with subsequent aging on the structure, mechanical and fatigue properties of the Ti-15V-3Al-3Sn-3Cr-1Mo-1Zr alloy has been studied. It is shown that the specified processing leads to the formation in the alloy of a homogeneous hierarchical structure with lamellar precipitates of the α″-phase 20–30 nm thick in the volume of grains of the β phase with an average size of 10 μm. As a result, it is more than double increase in ultimate strength of the alloy (from 800 to 1630 MPa) while maintaining satisfactory plasticity (5.3%) It was found that such treatment also significantly increases the resistance to the development of fatigue fracture of the alloy at stress amplitudes above 500 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Intermetallics and Advanced Alloy Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Lütjering · 2007
2. Moiseyev · 2005
3. Mouritz · 2012
4. Thermomechanical processing of beta titanium alloys – an overview
5. Potential of rapid heat treatment of titanium alloys and steels
6. A comparative study of the mechanical properties of high-strength β-titanium alloys10.1016/j.jallcom.2007.03.070 ↗
7. Mechanical properties of nanocrystalline materials10.1016/j.pmatsci.2005.08.003 ↗
8. Bulk nanostructured materials: fundamentals and applications, Wiley
9. The effect of alpha-case formation on plastic deformation and fracture of near β titanium alloy10.1016/j.msea.2019.138495 ↗
10. Fatigue and fracture behavior of ultrafine-grained near β titanium alloy produced by radial shear rolling and subsequent aging10.1016/j.msea.2021.140968 ↗
11. Influence of combined helical and pass rolling on structure and residual porosity of an AA6082-0.2 wt % Al2O3 composite produced by casting with ultrasonic processing10.3390/met7120544 ↗
12. Microstructure and texture development in Ti-15V-3Cr-3Sn-3Al alloy – possible role of strain path10.1016/j.matchar.2019.109884 ↗
13. Mean stress dependence of fatigue strength and subsurface crack initiation in Ti-15Mo-5Zr-3Al alloy10.1016/S0921-5093(99)00710-8 ↗
14. High cycle fatigue and fracture behavior of Ti-5Al-5Mo-5V-3Cr alloy with BASCA and double aging treatments10.1016/j.msea.2016.02.004 ↗