Effect of the flyer material on the interface phenomena in aluminium and copper explosive welds

G.H.S.F.L. Carvalho, R. Mendes, R.M. Leal, I. Galvão, A. Loureiro

Materials & Design· Volume 122
Publisher page

Abstract

Abstract The effect of physical and mechanical properties of three different flyers on the interface phenomena of partially overlapped explosive welds, using the same base plate material, was studied. Flyers of Copper Cu-DHP and aluminium alloy 6082 (tempers T6 and O) were welded to AA6082-T6 base plates. The morphology of the weld interface is strongly influenced by the physical and mechanical properties of the flyer. In the interface of the aluminium welds, the use of a flyer of lower hardness and yield strength than the base plate results in asymmetrical waves, with bigger amplitude and smaller wavelength than the weld series of similar temper, and higher mechanical properties. The copper-aluminium welds presented flat interfaces, mainly because of the significant differences in melting temperature and density between the copper flyer and the aluminium base plate. Considering these results and analysing several dissimilar welds carried out by other authors it was found that when the product of density and melting temperature ratios between the flyer and the base plate exceeds a certain value, there is no formation of waves at the interface of the metals. Furthermore, for the Cu-Al welds, the CuAl 2 (θ) intermetallic phase was formed on the bond zone.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Effect of explosive mixture on quality of explosive welds of copper to aluminium10.1016/j.matdes.2016.01.116 ↗
2. Comparison of Cu, Ti and Ta interlayer explosively fabricated aluminum to stainless steel transition joints for cryogenic pressurized hydrogen storage10.1016/j.ijhydene.2014.11.038 ↗
3. Intermetallic phase formation in explosively welded Al/Cu bimetals10.1007/s11663-016-0682-1 ↗
4. Explosion welding
5. Blazynski · 1987
6. Analysis of explosive bonding parameters10.1080/10426910600611136 ↗
7. Review of the weldability window concept and equations for explosive welding10.1088/1742-6596/500/5/052038 ↗
8. Enhancement of explosive welding possibilities by the use of emulsion explosive10.2478/amm-2014-0269 ↗
9. Limiting conditions for jet formation in high velocity collisions10.1063/1.1721278 ↗
10. Mechanism of bond zone wave formation in explosion-clad metals10.1007/BF02814967 ↗
11. Surface effects with oblique collisions between metallic plates10.1007/BF01463767 ↗
13. Explosion welding of steel with aluminum10.1023/A:1015674407898 ↗
14. Effect of interlayer thickness on shear deformation behavior of AA5083 aluminum alloy/SS41 steel plates manufactured by explosive welding10.1023/A:1021197328946 ↗
15. Investigation of interface properties and weldability of aluminum and copper plates by explosive welding method10.1016/j.matdes.2006.11.001 ↗
16. Weldability window and the effect of interface morphology on the properties of Al/Cu/Al laminated composites fabricated by explosive welding10.1016/j.matdes.2015.07.114 ↗
17. Joining of titanium/stainless steel by explosive welding and effect on interface10.1016/j.jmatprotec.2005.06.045 ↗
18. Handbook · 1990
19. Dissimilar metals
20. Cu-Al
21. Explosive scarf welding of aluminum to copper plates and their interface properties10.1002/mawe.200900415 ↗
22. Quality of bimetal Al-Cu joint after explosive cladding
23. The analysis of the impact relative rolling reduction at the area connector bimetallic plate after the rolling process10.4028/www.scientific.net/SSP.199.514 ↗
24. Kennedy · 1970
25. Cooper · 1996
26. Kennedy · 1972
27. Thermochemical estimation of explosive energy output10.1016/0010-2180(77)90007-4 ↗
28. Mendes · 2012 · Vol. 1426 · 267
29. Differences between the detonation behavior of emulsion explosives sensitized with glass or with polymeric micro-balloons10.1088/1742-6596/500/5/052030 ↗
30. Kah · 2010 · 373
31. Mathers · 2002
32. On the transition from a waveless to a wavy interface in explosive welding10.1016/0025-5416(87)90300-4 ↗
33. Flow configurations in colliding plates: explosive bonding10.1063/1.1729565 ↗
34. The aluminium-copper system10.1179/imr.1985.30.1.211 ↗
35. Effect of annealing on the interfacial structure of aluminum-copper joints10.2320/matertrans.MER2006371 ↗
36. Microstructural evolution in the friction stir welded 6061 aluminum alloy (T6-temper condition) to copper10.1016/j.jmatprotec.2005.09.013 ↗
37. Analysis of Al-Cu bimetallic bars properties after explosive welding and rolling in modified passes10.1515/amm-2015-0070 ↗
38. Intermetallic phase formation in diffusion-bonded Cu/Al laminates10.1007/s10853-010-5093-0 ↗
39. Investigation of interdiffusion and intermetallic compounds in Al–Cu joint produced by continuous drive friction welding
40. Properties of joint in the bimetallic rods Cu-Al and Cu-steel after explosive cladding and the process of rolling
41. Interface phenomena and bonding mechanism in magnetic pulse welding10.1007/s11665-014-1143-0 ↗
42. Bonding zone formation in magnetic pulse welds10.1179/136217102225002673 ↗
43. Development of an explosive welding process for producing high-strength welds between niobium and 606-T651 aluminum
44. The problem of intermixing of metals possessing no mutual solubility upon explosion welding (Cu-Ta, Fe-Ag, Al-Ta)10.1016/j.matchar.2012.10.011 ↗
45. The effect of annealing on the interface microstructure and mechanical characteristics of AZ31B/AA6061 composite plates fabricated by explosive welding10.1016/j.matdes.2014.08.025 ↗
46. Nobili · 1999 · 83
47. Effect of explosive characteristics on the explosive welding of stainless steel to carbon steel in cylindrical configuration10.1016/j.matdes.2013.03.069 ↗
48. An investigation on the explosive cladding of 316L stainless steel-din-P355GH steel10.1016/j.jmatprotec.2004.03.012 ↗
49. Examination of copper/stainless steel joints formed by explosive welding10.1016/j.matdes.2004.07.021 ↗
50. Investigation of effect of the stand-off distance on interface characteristics of explosively welded copper and stainless steel10.1016/j.matdes.2007.07.012 ↗
51. Characterization of explosively bonded iron and copper plates10.1007/BF01233153 ↗
52. Microstructural and mechanical properties of Cu-Ti plates bonded through explosive welding process10.1016/j.jmatprotec.2005.02.264 ↗
53. Experimental investigation of explosive welding of cp-titanium/AISI 304 stainless steel10.1016/j.matdes.2008.06.016 ↗
54. Experimental investigation of explosion-welded CP-Ti/Q345 bimetallic sheet filled with Cu/V based flux-cored wire10.1016/j.matdes.2014.11.008 ↗
55. The use of lead in explosive welding10.1002/prep.19760010506 ↗