journal article·2016-03

Improving mechanical strength and thermal shock resistance of SiC/zinc aluminum silicate joint by electrophoretic deposited multi-walled carbon nanotubes

Lei Feng, Kezhi Li, Caifeng Zheng, Yewei Fu, Zhigang Zhao, Qiang Song

Materials & Design· Volume 94
Publisher page

Abstract

Abstract Improving the SiC/zinc aluminum silicate (SiC/ZAS) interface was essential for increasing the mechanical strength of SiC/ZAS joints that were used to join carbon/carbon (C/C) composites and lithium aluminum silicate (LAS) glass ceramics. In this work, well-dispersed multi-walled carbon nanotubes (MWCNTs) were introduced at the SiC/ZAS interface in the joints by electrophoretic deposition, which changed the fracture feature of the bonded C/C-LAS from SiC/ZAS interface fracture to C/C fracture, resulting in significant improvements of the shear strength. Results showed that the average shear strength of the joints was increased by 94.8% after introducing MWCNTs, which was attributed to the obviously decreased micro-defects at the SiC/ZAS interface in the joints. MWCNT-reinforced joints also exhibited better thermal shock resistance evidenced by higher residual shear strengths than those of neat joints after thermal shock tests from 800 °C to room temperature and 1000 °C to room temperature, respectively, which was primarily attributed to the positive role of MWCNTs in alleviating thermal stress.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Fitzer · 1998
2. Mechanical property and failure mechanism of 3D carbon–carbon braided composites bolted joints under unidirectional tensile loading10.1016/j.matdes.2014.08.073 ↗
3. Carbon/carbon composites
4. The relationship between structure and transparency in glass-ceramic materials10.1016/S0925-3467(00)00017-3 ↗
5. MAS-NMR studies of lithium aluminum silicate (LAS) glasses and glass-ceramics having different Li2O/Al2O3 ratio10.1016/j.jssc.2009.10.006 ↗
6. Sol–gel synthesis of lithium aluminum silicate powders: the effect of silica source10.1016/j.ceramint.2005.03.033 ↗
7. A gradient LMAS interlayer joint of SiC coated C/C composites to LAS glass ceramics10.1016/j.ceramint.2013.08.021 ↗
8. Improvement of SiC–Si/MAS interface in the joints via in situ synthesizing SiC nanowires10.1111/jace.12612 ↗
9. Joining of surface modified carbon/carbon composites using a barium-aluminum-boro-silicate glass10.1016/S0955-2219(97)00203-3 ↗
10. Vitreous joining of SiC-coated carbon/carbon composites10.1016/j.matlet.2007.11.100 ↗
11. Microstructural studies of the interfacial zone of a SiC-fiber-reinforced lithium aluminum silicate glass-ceramic10.1111/j.1151-2916.1989.tb06210.x ↗
12. Influence of interlayer's thickness on strength of joints between LAS glass-ceramic and carbon/carbon composites10.3724/SP.J.1077.2011.00847 ↗
13. High strength, high fracture toughness fibre composites with interface control—a review10.1016/0266-3538(91)90072-W ↗
14. Hierarchical composites reinforced with carbon nanotube grafted fibers: the potential assessed at the single fiber level10.1021/cm702782j ↗
15. Effect of carbon nanotubes on the strength of adhesive lap joints of C/C and C/C-SiC ceramic fibre composites10.1016/j.ijadhadh.2011.03.006 ↗
16. A multi-wall carbon nanotube-reinforced high-temperature resistant adhesive for bonding carbon/carbon composites10.1016/j.carbon.2012.06.021 ↗
17. Enhancement of C/C-LAS joint using aligned carbon nanotubes prepared by injection chemical vapor deposition10.1016/j.msea.2015.10.003 ↗
18. Microstructure and thermal shock resistance of SiC/CNT-SiC double-layer coating for carbon/carbon composites10.1016/j.ceramint.2014.04.127 ↗
19. CNT-PyC-SiC/SiC double-layer oxidation-protection coating on C/C composite10.1016/j.carbon.2008.07.014 ↗
20. A carbon nanotube-enhanced SiC coating for the oxidation protection of C/C composite materials10.1016/j.compositesb.2011.05.012 ↗
21. Electrophoretic deposition of carbon nanotubes10.1016/j.carbon.2006.06.021 ↗
22. SiC nanowires reinforced MAS joint of SiC coated carbon/carbon composites to LAS glass ceramics10.1016/j.msea.2011.10.088 ↗
23. Electrophoretic deposition of SiC nanowires onto carbon/carbon composites to improve the interface bonding of Ti–Ni–Si joint10.1016/j.matdes.2015.04.042 ↗
24. Thermal shock resistance of SiC/MAS-LAS multilayer joint of carbon/carbon composites to LAS glass-ceramic10.1016/j.msea.2012.07.034 ↗
25. Partial transient liquid phase bonding of carbon/carbon composites using Ti–Ni–Al2O3–Si compound as interlayer10.1016/j.jallcom.2012.09.048 ↗
26. Carbon-fiber-reinforced YMAS glass-ceramic-matrix composites—IV. Thermal residual stresses and fiber/matrix interfaces10.1016/S0266-3538(97)00139-5 ↗
27. Process and mechanical properties of carbon/carbon-silicon carbide composite reinforced with carbon nanotubes grown in situ10.1016/j.compositesa.2013.01.014 ↗