journal article·2020-11Open access

Localised creep cavitation on boron nitride in the heat affected zone of 9% Cr tempered martensitic steel welds

X. Xu, J.A. Siefert, J.D. Parker, R.C. Thomson

Materials & Design· Volume 196

Abstract

An excessive concentration of boron in the 9% Cr tempered martensitic steels alloyed with nitrogen has a detrimental effect on creep performance, as relatively large boron nitride phases are formed and can act as the preferred sites for cavity nucleation. In the current research, a systematic investigation has been performed documenting details of creep damage in the heat affected zone of a weld joint constructed by using a 9% Cr Grade 92 steel. A combination of correlative characterisation techniques has been applied to monitor and quantify the evolution of creep damage within the heat affected zone through the entire creep life. The utilisation of cryo-fractography, two-dimensional electron-based microscopic characterisation and three-dimensional tomography based on focused ion beam microscopy have confirmed the close association between creep cavities and boron nitride phases from the initial stage of creep. It is revealed that the thermal transients imposed during welding result in the decohesion at the interface of boron nitrides with the surrounding matrix. This decohesion is a result of significant thermo-mechanical mismatch between boron nitrides and the tempered martensitic matrix. The voids initiated at these locations grow and eventually link-up during creep exposure, leading to cracking and fracture.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Richardot · 2000
2. The influence of thermal cycles on the microstructure of grade 92 steel10.1007/s11661-017-4306-4 ↗
3. Review of type IV cracking of weldments in 9-12% Cr creep strength enhanced ferritic steels10.1179/1743280412Y.0000000016 ↗
4. Review Type IV cracking in ferritic power plant steels10.1179/174328406X148778 ↗
5. Microstructural characterization of the heat-affected zones in grade 92 steel welds: double-pass and multi-pass welds10.1007/s11661-017-4446-6 ↗
6. X. Xu, J.A. Siefert, J.D. Parker, R.C. Thomson, Influence of microstructure on cavitation in the heat affected zone of a 9% Cr steel weld during long-term high temperature creep, Manuscript submitted to Materials & Characterization.
7. Y. Gu, G.D. West, R.C. Thomson, J. Parker, Investigation of creep damage and cavitation mechanisms in P92 steels, in: D. Gandy, J. Shingledecker, (eds.), Advances in materials technology for fossil power plants: proceedings from the seventh international conference (EPRI 2013), 22nd-25th October 2013, Waikoloa, Hawaii, USA. ASM International, pp. 596–606.10.31399/asm.cp.am-epri-2013p0596 ↗
8. J.D. Parker, Creep cavitation in CSEF steels, in: D. Gandy, J. Shingledecker, (eds.), Advances in Materials Technology for Fossil Power Plants: Proceedings from the Seventh International Conference (EPRI 2013), 22nd-25th October 2013, Waikoloa, Hawaii, USA. ASM International, pp. 714–733.10.31399/asm.cp.am-epri-2013p0714 ↗
9. BN type inclusions formed in high Cr ferritic heat resistant steel
10. Gu · 2017
11. Segregation of boron at prior austenite grain boundaries in a quenched martensitic steel studied by atom probe tomography10.1016/j.scriptamat.2014.09.031 ↗
12. The influence of boron on the microstructure of a 9 wt% Cr ferritic steel10.1179/096034011X13059091965585 ↗
13. F. Abe, Precipitate design for creep strengthening of 9% Cr tempered martensitic steel for ultra-supercritical power plants, Sci. Technol. Adv. Mater. 9 (2008) 13002 1–15.10.1088/1468-6996/9/1/013002 ↗
14. ASME/BPVC-2179-6 Seamless 9Cr-2W Material, Section I and section VIII, division 1 supplement 11. ASME International, 2004.
15. Factors affecting Type IV creep damage in grade 91 steel welds10.1016/j.msea.2013.04.045 ↗
16. Cross-weld creep performance in Grade 91 steel: macro-based assessment10.29391/2019.98.005 ↗
17. Cryo-cracking: a technique for creep damage assessment in high temperature components10.1080/09603409.1998.11689596 ↗
18. Focused ion beam microscopy and micromachining10.1557/mrs2007.62 ↗
19. Quantification of Laves phase particle size in 9CrW steel10.1016/S1044-5803(01)00159-0 ↗
20. Metallurgical and stress state factors which affect the creep and fracture behavior of 9% Cr steels10.1155/2018/6789563 ↗
21. Samuels · 2003
22. Large volume serial section tomography by Xe plasma FIB dual beam microscopy10.1016/j.ultramic.2015.11.001 ↗
23. The theory of metal-ceramic interfaces10.1088/0953-8984/8/32/003 ↗
24. The application of the Eshelby method of internal stress determination to short fibre metal matrix composites10.1016/0001-6160(89)90341-6 ↗
25. Separation of macroscopic, elastic mismatch and thermal expansion misfit stresses in metal matrix composite quenched plates from neutron diffraction measurements10.1016/S1359-6454(97)00209-7 ↗
26. Calibration of the differential dilatometric measurement signal upon heating and cooling; thermal expansion of pure iron10.1016/j.tca.2003.10.005 ↗
27. Properties of high-purity iron10.6028/jres.028.027 ↗
28. W. Paszkowicz, J.B. Pelka, M. Knapp, T. Szyszko, S. Podsiadlo, Lattice parameters and anisotropic thermal expansion of hexagonal boron nitride in the 10–297.5 K temperature range, Appl. Phys. A. 75 (2002) 431–435.10.1007/s003390100999 ↗
29. A. Bosak, J. Serrano, M. Krisch, K. Watanabe, T. Taniguchi, H. Kanda, Elasticity of hexagonal boron nitride: inelastic x-ray scattering measurements, Phys. Rev. B. 73 (2006) 041402 1–4.10.1103/PhysRevB.73.041402 ↗
30. On the properties of α-MnS and MnS210.3891/acta.chem.scand.19-1405 ↗
31. First-principles study of structural stability, elastic and dynamical properties of MnS10.1016/j.commatsci.2014.07.022 ↗
32. Richerson · 2005
33. Influence of porosity on Young’s modulus and Poisson’s ratio in alumina ceramics10.1016/S0955-2219(00)00314-9 ↗
34. Direct observation of thermal stability of M23C6 carbides during reheating using in situ synchrotron X-ray diffraction10.1080/09500839.2012.728296 ↗
35. The electronic, mechanical properties and theoretical hardness of chromium carbides by first-principles calculations10.1016/j.jallcom.2011.02.009 ↗
36. Toth · 2014
37. Elastic moduli of niobium carbide and tantalum carbide at high temperature10.1016/0022-5088(71)90046-4 ↗
38. B.D. Fulcher, X.Y. Cui, B. Delley, C. Stampfl, Hardness analysis of cubic metal mononitrides from first principles, Phys. Rev. B. 85 (2012) 184106 1–9.10.1103/PhysRevB.85.184106 ↗
39. Effect of laser spot weld energy and duration on melting and absorption10.1179/136217102225004293 ↗
40. H. Hongo, M. Tabuchi, T. Watanabe, Type IV creep damage behaviour in Gr. 91 steel welded joints, Metall. Mater. Trans. A. 43 (2012) 1163–1173.10.1007/s11661-011-0967-6 ↗
41. Thermal cycle measurement of P92 welded joints
42. Honeycombe · 1995
43. A. Yaghi, D. Tanner, T. Hyde, A. Becker, W. Sun, Abaqus thermal analysis of the fusion welding of a P92 steel pipe, Report of 2011 SIMULIA Customer Conference, 2012.10.5194/ms-3-33-2012 ↗
44. Mayr · 2009
45. Abe · 2008
46. Creep cavitation in metals10.1016/S0749-6419(02)00111-0 ↗
47. Formation mechanism of Type IV failure in high Cr ferritic heat-resistant steel-welded joint10.1007/s11661-013-1801-0 ↗