Effect of SiC on the antioxidant properties of Al-containing composites Ti3SiC2/SiC and its oxidation mechanism analysis
Source abstract
Abstract
• Preparation of Ti 3 SiC 2 /SiC composites with different contents of SiC. • SiC reduces oxidation weight gain and increases oxidation activation energy. • SiC improves the structure of the oxide layer and increases oxidation resistance. • Atomic migration is an important factor in the formation of oxidized delamination. This study aims at improving the oxidation resistance of ceramics intended for high-temperature applications by examining the quantitative SiC-reinforced aluminum-containing composites Ti 3 SiC 2 /SiC that were synthesized through a powder metallurgy method. The high-temperature antioxidant properties of these composites were evaluated at temperatures between 900 °C and 1300 °C. The findings reveal that an increase in SiC content elevates the activation energy associated with oxidation, mitigates oxidation behavior, and decreases the weight gain attributable to oxidation of the material. Additionally, the formation of the oxide layer and atomic diffusion were investigated through the analysis of surface micro-morphology and the distribution of the oxide layer at the interface. It was found that the addition of SiC modifies the oxide layer structure of the material, which primarily consists of an outer mixed oxide layer of TiO 2 and Al 2 O 3 , an intermediate oxide layer of TiO 2 with a small amount of SiO 2 , and an inner homogeneous mixed oxide layer of TiO 2 and SiO 2 . Finally, the high-temperature oxidation mechanism of Ti 3 SiC 2 /SiC composites is systematically illustrated through experimental results.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: MXene and MAX Phase Materials · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Materials for high temperature electrochemical applications: Automotive sensors, catalysts and traps10.1016/j.snb.2012.09.069 ↗
2. Designing VxNbMoTa refractory high-entropy alloys with improved properties for high-temperature applications10.1016/j.scriptamat.2020.09.027 ↗
3. Experimental investigation and mathematical modelling of water vapour corrosion of Ti3SiC2 and Ti2AlC ceramics and their mechanical behaviour10.1016/j.jeurceramsoc.2021.03.045 ↗
4. Advanced Materials for High-Temperature Thermal Transport10.1002/adfm.201904815 ↗
5. Advances in ultra-high temperature ceramics, composites, and coatings10.1007/s40145-021-0550-6 ↗
6. Progress in Nb-Si ultra-high temperature structural materials: A review10.1016/j.jmst.2022.11.022 ↗
7. Cyclic-Oxidation Behavior of Ti3Al0.7Si0.3C2 Compounds Between 900 and 1100°C in Air10.1007/s11085-009-9163-0 ↗
8. On the oxidation of Ti2GeC in air10.1016/j.jallcom.2013.06.103 ↗
9. Anodized Ti3SiC2 As an Anode Material for Li-ion Microbatteries10.1021/acsami.6b03528 ↗
10. Ti3SiC2 has negligible thermopower10.1038/35036686 ↗
11. Synthesis of Ti3AuC2, Ti3Au2C2 and Ti3IrC2 by noble metal substitution reaction in Ti3SiC2 for high-temperature-stable Ohmic contacts to SiC10.1038/nmat4896 ↗
12. The Ti3SiC2 max phases as promising materials for high temperature applications: Formation under various synthesis conditions10.1016/j.matchemphys.2021.124625 ↗
13. Cyclic Fatigue-Crack Growth and Fracture Properties in Ti3SiC2 Ceramics at Elevated Temperatures10.1111/j.1151-2916.2001.tb01115.x ↗
14. Oxidation and hot corrosion behaviors of MAX-phase Ti3SiC2, Ti2AlC, Cr2AlC10.1016/j.ceramint.2022.05.356 ↗
15. In-situ fabrication and characterization of TiC matrix composite reinforced by SiC and Ti3SiC210.1016/j.ceramint.2023.03.218 ↗
16. High temperature oxidation behavior of Ti3SiC2-based material in air10.1016/S1359-6454(01)00247-6 ↗
17. Oxidation behavior of Ti3SiC2 at high temperature in air10.1016/S0921-5093(02)00210-1 ↗
18. Fabrication of nearly stoichiometric polycrystalline SiC fibers with excellent high-temperature stability up to 1900°C10.1111/jace.15366 ↗
19. Interfacial reaction mechanism and high temperature stability of heat-resistant steel and SiC under a vacuum environment10.1016/j.jmrt.2023.06.078 ↗
20. Synthesis, fabrication, and applications of Ti3SiC2/SiC ceramics: a review10.1007/s10853-024-09962-1 ↗
21. Mechanical performance and oxidation resistance of SiC castables with lamellar Ti3SiC2 coatings on SiC aggregates prepared by SPS10.1016/j.jallcom.2019.03.358 ↗
22. Constructing hierarchical Ti3SiC2 layer and carbon nanotubes on SiC fibers for enhanced electromagnetic wave absorption10.1016/j.ceramint.2022.10.323 ↗
23. Fabrication of SiCw/Ti3SiC2 composites with improved thermal conductivity and mechanical properties using spark plasma sintering10.1007/s40145-020-0389-2 ↗
24. Effect of positioning impregnation on the oxidation behaviour of Ti3SiC2/SiC functionally graded materials at 1400 °C10.1016/j.jallcom.2018.01.310 ↗
25. The morphology of oxides and oxidation behavior of Ti3SiC2-based composite at high-temperature10.1016/S0266-3538(02)00285-3 ↗
26. High temperature oxidation resistance behavior of Ti3SiC2/Cu composites under migration of Ti and Cu atomic
27. General Relationship for the Thermal Oxidation of Silicon10.1063/1.1713945 ↗
28. Oxidation kinetics of hot-pressed silicon carbide10.1007/BF00545142 ↗
29. SPS preparation and mechanical properties of Ti3SiC2/SiC composites reinforced with quantitative SiC10.1016/j.jallcom.2024.178167 ↗
30. The effect of Ta on the kinetics and mechanisms of high-temperature oxidation of the (Hf,Ta)B2–SiC ceramics10.1016/j.corsci.2023.111721 ↗
31. Synthesis and oxidation resistance of different Ti3SiC2–TiC composites10.1016/j.ceramint.2024.04.232 ↗
32. Oxidation mechanism of Al–Si–SiC composite at elevated temperature10.1016/j.ceramint.2024.03.279 ↗
33. High-temperature performance in Al2O3–Cr2O3 refractories: Effect of Al2TiO510.1016/j.ceramint.2021.10.178 ↗
34. High-temperature oxidation behaviour of Ti65 titanium alloy fabricated by laser direct energy deposition10.1016/j.corsci.2024.111866 ↗
35. Oxidation behaviour of SiC/SiC ceramic matrix composites in air10.1016/j.jeurceramsoc.2016.05.051 ↗
36. Investigation on the effect of Nb doping on the oxidation mechanism of Ti3SiC210.1016/j.corsci.2018.05.028 ↗
37. Oxidation behavior of Al-doped Ti3SiC2-20wt.%Ti5Si3 composite10.1016/j.ceramint.2021.08.272 ↗
38. Fabrication and characterization of B4C–ZrB2–SiC ceramics with simultaneously improved high temperature strength and oxidation resistance up to 1600°C10.1016/j.ceramint.2016.01.202 ↗
39. Preparation and anti-oxidation performance of TaC-SiC nanocomposites by precursor-derived ceramic method10.1016/j.ceramint.2024.08.407 ↗