Abstract

In the present work, TiCNp/Al–11Si composites have been fabricated upon addition of TiCN nanoparticles to the molten alloy, which are dispersed via ultrasonic vibration method. Two distribution types of nanoparticles in the matrix are observed and systematically investigated using SEM and TEM, including intragranular distribution (within the interior of α-Al dendrite) and intergranular distribution (along the grain boundary or the eutectic Si on the grain boundary). During solidification, large quantities of NPs distributed along grain boundaries and then along the eutectic interfaces can form NP layers to physically restrict the growth of primary α-Al and eutectic Si. The refined microstructure and the reinforcing particles with no brittle intermetallics precipitating at the interface can be responsible for the significant improvement in the mechanical properties of the composites. The 2 vol.% TiCNp/Al–11Si composite exhibits the most excellent performance with its hardness, ultimate tensile strength, yield strength and elongation higher by 45%, 22%, 16% and 108%, respectively, as compared to the matrix alloy.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Microstructure and mechanical properties of 6061 Al alloy based composites with SiC nanoparticles10.1016/j.jallcom.2014.01.134 ↗
2. Investigation of microstructure, hardness and wear properties of Al–4.5wt.% Cu–TiC nanocomposites produced by mechanical milling10.1016/j.matdes.2011.03.056 ↗
3. Overview of wear performance of aluminum matrix composites reinforced with ceramic materials under the influence of controllable variables10.1016/j.ceramint.2015.08.150 ↗
4. Fabrication of in situ AlN–TiN/Al inoculant and its refining efficiency and reinforcing effect on pure aluminum10.1016/j.jallcom.2012.08.082 ↗
5. Reinforcement fracture and tensile ductility in sphere-reinforced metal-matrix composites10.1111/j.1460-2695.1997.tb00301.x ↗
6. Effects of Sr on the microstructure and mechanical properties of in situ TiB2 reinforced A356 composite10.1016/j.matdes.2014.07.040 ↗
7. Effects of nano-TiCp on the microstructures and tensile properties of TiCp/Al–Cu composites10.1016/j.matchar.2014.05.012 ↗
8. Enhanced properties of Mg-based nano-composites reinforced with Al2O3 nano-particles10.1016/j.msea.2009.05.001 ↗
9. Processing-microstructure relationships in compocast magnesium/SiC10.1007/BF00541578 ↗
10. Processing, microstructure and tensile properties of nano-sized Al2O3 particle reinforced aluminum matrix composites10.1016/j.matdes.2011.11.064 ↗
11. Scaling laws for van der Waals interactions in nanostructured materials10.1038/ncomms3341 ↗
12. Wetting improvement of carbon or silicon carbide by aluminum alloys based on a K2ZrF6 surface treatment: application to composite material casting10.1007/BF02385613 ↗
13. The K2ZrF6 wetting process: effect of surface chemistry on the ability of a SiC-fiber preform to be impregnated by aluminum10.1007/BF02669881 ↗
14. Perfect wettability of carbon by liquid aluminum achieved by a multifunctional flux10.1007/s10853-010-4555-8 ↗
15. Production of natural and synthesized aluminum-based composite materials with the aid of ultrasonic (cavitation) treatment of the melt10.1016/S1350-4177(02)00158-X ↗
16. Application of ultrasonic vibration to in situ MMC process by electromagnetic melt stirring10.1016/S0261-3069(00)00079-0 ↗
17. Structure and amorphization of the oxide on the silicon carbide surface in an SiCp/Al composite10.1016/S1359-6462(99)00006-8 ↗
18. The interfacial characterization of oxidized SiC(p)/2014 Al composites10.1016/S0921-5093(00)01943-2 ↗
19. Mechanical and fracture behaviour of aluminium-based discontinuously reinforced composites at hot working temperatures10.1016/j.compscitech.2005.04.045 ↗
20. An analysis of the factors affecting strengthening in carbon nanotube reinforced aluminum composites10.1016/j.carbon.2010.09.054 ↗
21. Prediction of Si contents to suppress the formation of Al4C3 in the SiCp/Al composite10.1016/S1359-6454(97)00265-6 ↗
22. Observation of three-dimensional interfacial morphologies in SiCp/Al composites and its characterization10.1007/BF00625016 ↗
23. Effect of aging on interface characteristics of Al–Mg–Si/SiC composites10.1016/j.jallcom.2015.07.033 ↗
24. Phase constituents and mechanical properties of laser in-situ synthesized TiCN/TiN composite coating on Ti–6Al–4V10.1016/j.surfcoat.2010.07.058 ↗
25. Wetting of porous titanium carbonitride by Al–Mg–Si alloys10.1016/S1359-6454(99)00198-6 ↗
26. Ti (C,N) coatings using the arc process10.1016/0257-8972(91)90148-P ↗
27. Charged nanoparticles as supramolecular surfactants for controlling the growth and stability of microcrystals10.1038/nmat3202 ↗
28. Rapid control of phase growth by nanoparticles10.1038/ncomms4879 ↗
29. Nanoparticle-inhibited growth of primary aluminum in Al–10Si alloys10.1016/j.actamat.2015.10.005 ↗
30. Effect of grain refiner on the tensile and impact properties of Al–Si–Mg cast alloys10.1016/j.matdes.2013.11.058 ↗
31. Development of an efficient grain refiner for Al–7Si alloy10.1016/S0921-5093(99)00656-5 ↗
32. Dahle AK. Segregation of particles and its influence on the morphology of the eutectic silicon phase in Al–7wt.% Si alloys10.1016/j.scriptamat.2005.10.016 ↗
33. Villars · 1985
34. An analytical model for the interaction between an insoluble particle and an advancing solid/liquid interface10.1007/BF02801184 ↗
35. Particle engulfment and pushing by solidifying interfaces: part 1. Ground experiments10.1007/s11661-998-0091-4 ↗
36. Stefanescu DM, Uretzko FR, Dhindaw BK, Catalina A, Sen S, Curreri PA. Particle engulfment and pushing by solidifying interfaces: part II. Microgravity experiments and theoretical analysis. Metall. Mater. Trans. A 1998;29:1697.10.1007/s11661-998-0092-3 ↗
37. Temperature-dependent viscosities of eutectic Al–Si alloys modified with Sr and P10.1016/j.jallcom.2009.01.028 ↗
38. 1986
39. Cottrell · 1988
40. Interfacial phenomena and microstructure evolution during solidification of binary and ternary Al–Mg–Si alloys cast with titanium carbonitride10.1016/S0921-5093(01)01485-X ↗
41. A simple model for grain refinement during solidification10.1016/0001-6160(75)90188-1 ↗
42. Dendritic growth into undercooled alloy melts10.1016/0025-5416(84)90199-X ↗
43. Modeling equiaxed solidification with melt convection and grain sedimentation-I: model description10.1016/j.actamat.2009.07.056 ↗
44. Modelling of inoculation of metallic melts application to grain refinement of aluminum by Al–Ti–B10.1016/S1359-6454(00)00094-X ↗
45. A quantitative study of solute diffusion field effects on heterogeneous nucleation and the grain size of alloys10.1016/j.actamat.2010.12.014 ↗
46. Eutectic grains in unmodified and strontium-modified hypoeutectic aluminum-silicon alloys10.1007/s11661-004-0091-y ↗
47. The growth temperature and interflake spacing in aluminium silicon eutectic alloys10.1016/0001-6160(80)90049-8 ↗
48. Al2O3 nanoparticle addition to concentrated magnesium alloy AZ81: enhanced ductility10.1016/j.jallcom.2012.08.020 ↗
49. Effects of Sr-modification, iron-based intermetallics and aging treatment on the impact toughness of 356 Al-Si-Mg alloy10.1007/s10853-010-5181-1 ↗
50. Interpretation of tensile results by means of quality index and probable yield strength
51. Nanomechanics of Hall–Petch relationship in nanocrystalline materials10.1016/j.pmatsci.2009.03.008 ↗
52. Ultrafine grains and the Hall–Petch relationship in an Al–Mg–Si alloy processed by high-pressure torsion10.1016/j.msea.2011.10.074 ↗
53. Development of TiB2 reinforced aluminum foundry alloy based in situ composites-part II: enhancing the practical aluminum foundry alloys using the improved Al–5 wt%TiB2 master composite upon dilution10.1016/j.msea.2014.03.021 ↗