journal article·2025-11Open access

Research on the microstructure and properties of Cu-Ni-Si-Ti alloys with micro-nano hybrid systems

Xiao Zhang, Qing Liu, Xiangfang Liu, Xiaocui Zhang, Huanyu Liu, Desheng Zhao, Fugong Qi, Jinchuan Jie, Chong Li, Haimin Ding

Materials & Design· Volume 259

Abstract

• Micron/nanoscale Ni 16 Ti 6 Si 7 and nanoscale Ni 2 Si precipitate in Cu-Ni-Si-Ti alloys. • Cu-Ni-Si-(Ti) alloys are mainly strengthened by fine nanoscale Ni 2 Si phases. • The micron Ni 16 Ti 6 Si 7 promotes the recrystallization nucleation of Cu. • Cu-4.84Ni-1.04Si-0.5Ti shows higher HDI stress from GNDs at G phase/Cu interfaces. The Cu-Ni-Si-Ti alloys with micron Ni 16 Ti 6 Si 7 phase and nano δ-Ni 2 Si dual-scale reinforcement particles were prepared and their microstructures, properties as well as strengthening mechanism were studied. It is found that micron-sized Ni 16 Ti 6 Si 7 particles (∼8μm) formed during alloy solidification, along with submicron Ni 16 Ti 6 Si 7 and Ni 2 Si precipitates (∼200 nm). This behavior differed from that observed in conventional Cu-Ni-Si alloys. After heat treatment, the micron and submicron Ni 16 Ti 6 Si 7 particles form semi-coherent interfaces with the α-Cu matrix, promoting recrystallization nucleation during hot rolling and thereby effectively refining the grain size of the alloy. Meanwhile, the nanoscale Ni 2 Si precipitates (∼30 nm) act as the primary strengthening phase, pinning grain boundaries and dislocations during deformation. Due to the significant elasticity modulus mismatch between Cu matrix and Ni 16 Ti 6 Si 7 phase, a large strain gradient during the tensile process will lead to HDI strengthening, and improve the overall performance of the material through the storage and induction of dislocations at the Cu grain boundaries and the Ni 16 Ti 6 Si 7 -Ni 2 Si/Cu interface. Therefore, compared with Cu-3.2Ni-0.7Si alloy, Cu-4Ni-0.9Si-0.5Ti alloy exhibits higher elastoplasticity while maintaining similar strength and conductivity. Its peak-aged conductivity reaches 35.0 ± 0 %IACS, with elastic modulus of 142 ± 4GPa, tensile strength of 747 ± 7 MPa, and elongation of 12.1 ± 0.3 %.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and mechanical properties · Intermetallics and Advanced Alloy Properties · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (85)

Show source-provided references
1. Achieving high strength and high-electrical-conductivity of Cu-Ni-Si alloys via regulating nanoprecipitation behavior through simplified process10.1016/j.jmst.2024.07.039 ↗
2. Microstructure and properties of TiC-Ti5Si3 reinforced copper matrix composites10.1016/j.ceramint.2023.08.114 ↗
3. Revealing the high strength and high thermal stability of a nano-lamellar Cu-0.1at.%Zr alloy10.1016/j.actamat.2024.120163 ↗
4. The precipitation behaviours and strengthening mechanism of a Cu-0.4wt%Sc alloy10.1016/j.jmst.2020.12.081 ↗
5. Effects of microelements on the microstructure evolution and properties of ultrahigh strength Cu-Ti alloys10.1016/j.msea.2021.141581 ↗
6. Strength-ductility synergy in a hierarchical Cu-Cr-Zr alloy processed via laser powder bed fusion10.1016/j.jmst.2023.12.042 ↗
7. Balanced strength and ductility in B4C/SiC/2024Al composite with multimodal grain structure achieved by multistep ball milling and powder metallurgy10.1016/j.matchar.2023.112896 ↗
8. Enhancing strength-ductility synergy of AlNp/Al composite by regulating heterostructure of matrix grain and particle distribution10.1016/S1003-6326(23)66453-2 ↗
9. The two-step nucleation of G-phase in ferrite10.1016/j.actamat.2016.06.013 ↗
10. On the crystal structure of the Mn-Ni-Si G-phase10.1016/j.jallcom.2008.01.142 ↗
11. Development of novel ferritic steels strengthened by the Co16X6Si7-G phase: a theoretical and experimental study10.1016/j.matdes.2022.111021 ↗
12. New insights into the precipitation strengthening of ferritic steels: nanoscale G-phase particle10.1016/j.matlet.2017.07.078 ↗
13. Microstructural evolution and precipitation strengthening in a new 20Cr ferritic trial steel10.1016/j.msea.2018.05.027 ↗
14. Effect of Ni, Mo and Mn content on spinodal decomposition kinetics and G-phase precipitation of aged model cast austenitic stainless steels10.1016/j.jnucmat.2021.153123 ↗
15. Simultaneous enhancement of mechanical and electrical properties of Cu-Ni-Si alloys via thermo-mechanical process10.1016/j.msea.2022.142815 ↗
16. Effect of cryogenic rolling on the microstructure and properties of C70250 copper alloy
17. Minor-alloyed Cu-Ni-Si alloys with high hardness and electric conductivity designed by a cluster formula approach10.1016/j.pnsc.2017.06.006 ↗
18. Metall. Effects of small addition of Ti on strength and microstructure of a Cu-Ni-Si alloy10.1007/s11661-015-2870-z ↗
19. Effect of Ti addition on tensile properties of Cu-Ni-Si alloys10.1007/s12540-011-0807-7 ↗
20. Microstructure and properties of high-strength Cu-Ni-Si-(Ti) alloys10.1007/s12598-020-01699-5 ↗
21. Growth and evolution of Ni-Ti-Si type G phase Ni16Ti6Si7 in Cu alloys10.1016/j.matchar.2024.114304 ↗
22. The microstructures and properties of diamond reinforced Cu-Ni-Si-Ti alloys10.1016/j.msea.2022.144478 ↗
23. The intergranular precipitation behavior of G phase in a high-performance complex cast Cu-Ni-Al alloy10.1016/j.matchar.2022.112611 ↗
24. Effect of inclusion on strength and conductivity of Cu-Ni-Si alloys with discontinuous precipitation10.1016/j.jallcom.2020.156006 ↗
25. Physical background of significant increase in mechanical properties and fatigue strength of groove-rolled Cu-Ni-Si alloy with discontinuous precipitates10.1016/j.jallcom.2023.169569 ↗
26. Dislocation densities in some annealed and cold-worked metals from measurements on the X-ray debye-scherrer spectrum10.1080/14786435608238074 ↗
27. Strengthening mechanisms in a high-strength bulk nanostructured Cu-Zn-Al alloy processed via cryomilling and spark plasma sintering10.1016/j.actamat.2012.09.036 ↗
28. Effect of indentation defects on fatigue crack propagation behavior of weld and base material: an in-situ fatigue study10.1016/j.tafmec.2025.104982 ↗
29. Revealing the deformation behavior and resultant texture evolution in extruded dilute Mg-Bi-Sn-Ca alloy during hot compression10.1016/j.msea.2022.143788 ↗
30. Analysis of microstructure and strengthening in CuMg alloys deformed by equal channel angular pressing10.1016/j.jallcom.2014.12.043 ↗
31. A review of dynamic recrystallization phenomena in metallic materials10.1016/j.matdes.2016.09.012 ↗
32. Tailoring bimodal grain structure of Mg-9Al-1Zn alloy for strength-ductility synergy: Co-regulating effect from coarse Al2Y and submicron Mg17Al12 particles10.1016/j.jma.2021.01.008 ↗
33. Co effects on Cu-Ni-Si alloys microstructure and physical properties10.1016/j.jallcom.2019.05.135 ↗
34. Relationship and mechanism between double cold rolling-aging process, microstructure and properties of Cu-Ni-Si alloy prepared by two-phase zone continuous casting10.1016/j.msea.2020.140148 ↗
35. Lattice misfit design and characterisation in BCC superalloys10.1016/j.scriptamat.2025.116802 ↗
36. Influence of γ'-Ni3(Al, Ti) precipitate morphology and lattice misfit on the oxidation behavior of Ni-based superalloy IN740H
37. Inverse Hall-Petch behavior in diamantane stabilized bulk nanocrystalline aluminum10.1016/j.actamat.2012.07.026 ↗
38. Small-volume aluminum alloys with native oxide shell deliver unprecedented strength and toughness10.1016/j.actamat.2016.12.055 ↗
39. Effect of G-phase and heterogeneous deformation-induced strengthening on the mechanical properties of Cu-20Ni-20Mn-2Fe-1Si alloy10.1016/j.matchar.2023.113325 ↗
40. G-phase strengthened iron alloys by design10.1016/j.actamat.2019.11.007 ↗
41. Property and thermal stability of in situ composite Cu-Cr alloy contact cable10.1016/j.jmatprotec.2004.08.013 ↗
42. Annealing hardening and deformation behavior of layered gradient Zr-Ti composite10.1016/S1003-6326(21)65659-5 ↗
43. R. Monzen, C. Watanabe, Microstructure and mechanical properties of Cu-Ni-Si alloys, Mater. Sci. Eng.: A 483-484 (2008) 117-119. https://doi.org/10.1016/j.msea.2006.12.163.10.1016/j.msea.2006.12.163 ↗
44. Tensile and electrical properties of direct aged Cu-Ni-Si-x% Ti alloys10.1007/s12540-013-2007-0 ↗
45. Effects of Nb addition on the properties and microstructure of Cu-Ni-Si-Mg alloy10.1016/j.matchar.2022.112451 ↗
46. Microstructure and properties of a high-strength Cu-Ni-Si-Co-Zr alloy10.1007/s11665-013-0482-6 ↗
47. Enhancing the comprehensive properties of as-cast Cu-Ni-Si alloys by continuous extrusion combined with subsequent thermomechanical treatment10.1016/j.matdes.2022.111033 ↗
48. Effects of Cr and Zr additions on microstructure and properties of Cu-Ni-Si alloys10.1016/j.msea.2016.07.021 ↗
49. Effect of aluminum on microstructure and property of Cu-Ni-Si alloys10.1016/j.msea.2013.02.024 ↗
50. Effect and mechanism of room temperature rolling, cryogenic rolling and heat treatment on mechanical properties and electrical conductivity of Cu-Ni-Si alloy with continuous directional solidification10.1016/j.jallcom.2023.169748 ↗
51. Enhanced combination of mechanical and electrical properties of a Cu-Cr-Zr alloy by optimized two-step thermomechanical treatment
52. Modeling the electrical resistivity of deformation processed metal-metal composites10.1016/j.actamat.2014.06.013 ↗
53. Mechanical and electrical properties of mechanically alloyed nanocrystalline Cu-Nb alloys10.1016/j.actamat.2006.03.021 ↗
54. J.R. Davis. Copper and Copper Alloys, ASM International, 2001.
55. Effect of electron concentration on electrical conductivity in in situ Al-TiB2 nanocomposites10.1063/1.5129817 ↗
56. Properties and precipitates of the high strength and electrical conductivity Cu-Ni-Co-Si-Cr alloy10.1016/j.jmst.2021.03.049 ↗
57. Bulk Cu-NbC nanocomposites with high strength and high electrical conductivity10.1016/j.jallcom.2018.02.215 ↗
58. The electrical resistivity of dislocations10.1080/14786436308209092 ↗
59. X-ray line broadening from filed aluminium and wolfram10.1016/0001-6160(53)90006-6 ↗
60. Effects of Fe content on properties and microstructure of Cu-Ti alloys during aging10.1016/j.jmrt.2023.10.211 ↗
61. Microstructure and properties of Cu-Cr-Nb alloy with high strength, high electrical conductivity and good softening resistance performance at elevated temperature10.1016/j.msea.2019.02.036 ↗
62. K. Maex, M. Van Rossum, Properties of Metal Silicides, IET 1995.
63. Crystal structures of some intermetallic compounds
64. Studies of electrical resistivity of an annealed Cu-Fe composite10.1063/1.4803716 ↗
65. S. Nagarjuna, K. Balasubramanian, D.S. Sarma, Effect of Ti additions on the electrical resistivity of copper, Mater. Sci. Eng.: A 225(1-2) (1997) 118-124. https://doi.org/10.1016/S0921-5093(96)10578-5.10.1016/S0921-5093(96)10578-5 ↗
66. Correlations between microstructures and properties of Cu-Ni-Si-Cr alloy10.1016/j.msea.2018.06.075 ↗
67. Achieving simultaneous enhancement of strength and ductility in Al matrix composites by employing the synergetic strengthening effect of micro- and nano-SiCps10.1016/j.compositesb.2022.110350 ↗
68. Microstructural evolution and strain-hardening in TWIP Ti alloys10.1016/j.actamat.2019.11.009 ↗
69. Effects of different Cr contents on microstructure, mechanical and electrical properties of Cu-Zr-Cr alloy
70. Effects of multiple trace alloying elements on the microstructure and properties of Cu-4wt% Ti alloys10.1016/j.msea.2017.09.072 ↗
71. Optimization of strength and ductility in an as-extruded Cu-15Ni-8Sn alloy by the additions of Si and Ti10.1016/j.jallcom.2020.153759 ↗
72. Some applications of the Taylor theory of polycrystal plasticity10.1002/crat.19700050112 ↗
73. A review on copper alloys with high strength and high electrical conductivity10.1016/j.jallcom.2024.174456 ↗
74. Effects of pre-deformation on precipitation behaviors and properties in Cu-Ni-Si-Cr alloy10.1016/j.msea.2018.11.045 ↗
75. Courtney · 2005
76. Effect of Ti additions on microstructure and mechanical properties of Cu-Cr-Zr alloy10.1016/j.jmst.2023.04.012 ↗
77. Effect of aging temperature on microstructure and softening property of the Cu-Cr-Zr-Nb alloy10.1016/j.jallcom.2024.173818 ↗
78. Superior strength-toughness synergy of heterogeneous TiB2p/AZ91 composites containing hard/soft zones via tailoring bimodal grain structure10.1016/j.msea.2023.145775 ↗
79. Generalized shear-lag model for load transfer in SiC/Al metal-matrix composites10.1557/JMR.2003.0398 ↗
80. Perspective on hetero-deformation induced (HDI) hardening and back stress10.1080/21663831.2019.1616331 ↗
81. Back stress in strain hardening of carbon nanotube/aluminum composites10.1080/21663831.2017.1405371 ↗
82. Bauschinger effect in thin metal films10.1016/j.scriptamat.2005.03.048 ↗
83. Emergence of enhanced strengths and Bauschinger effect in conformally passivated copper nanopillars as revealed by dislocation dynamics10.1016/j.actamat.2012.12.008 ↗
84. Enhanced dislocation obstruction in nanolaminated graphene/Cu composite as revealed by stress relaxation experiments10.1016/j.scriptamat.2017.01.015 ↗
85. About the determination of the thermal and athermal stress components from stress-relaxation experiments10.1016/j.actamat.2007.09.027 ↗