journal article·2019-07-04

On the Ultra-Precision Fabrication of Damage-Free Optical KDP Components: Mechanisms and Problems

Ning Hou, Liangchi Zhang, Yong Zhang, Feihu Zhang

Publisher page

Abstract

Potassium dihydrogen phosphate (KDP) crystals have excellent optical properties such as high nonlinear conversion efficiency, superior photoelectric and piezoelectric properties, transparency in a wide range of optical spectra, and good optical homogeneity. Therefore, KDP crystals have been used in many advanced fields, such as in the laser ignition facilities as large aperture crystals for optical switching and frequency conversion. However, extensive trials in the past decades showed that a KDP crystal is an extremely difficult-to-handle material for its high sensitivity to external stresses and environmental conditions, such as contact stresses, temperature variation and moisture invasion. It is also a soft material yet easy to fracture. A critical challenge is that it is unclear about the underlying physics of the damages which have been frequently observed after the ultra-precision surfacing of an optical KDP lens. As a result, when it is used in a Pockels photoelectric switch in a high-density laser system, for instance, its optical performance (e.g., its laser-induced damage threshold) is unexpectedly low. These have hindered significantly the development of high performance laser systems. This paper aims to provide a comprehensive review on the critical integrity issues of KDP components and their characterization methods, from the points of view of microstructure, micro/nano-mechanics, deformation mechanisms and laser-induced damage associated with the most commonly used surfacing technology––ultra-precision machining.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Laser Material Processing Techniques · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Mechatronics Engineering, Harbin Institute of Technology

Ministry of Education Key Laboratory of Micro-systems and Micro-structures Manufacturing, Harbin Institute of Technology

Laboratory for Precision and Nano Processing Technologies, School of Mechanical and Manufacturing Engineering, The University of New South Wales

Funding

NSFC · Error! Hyperlink reference not valid. · ARC

References (100+)

Show source-provided references
1. M. E. Lines and A. M. Glass, Principles and Applications of Ferroelectrics and Related Materials, Oxford University Press, Oxford (1977).
2. 10.1103/PhysRev.69.17310.1103/PhysRev.69.173 ↗
3. 10.1109/JQE.1981.107134910.1109/JQE.1981.1071349 ↗
4. 10.1080/0015019870801794210.1080/00150198708017942 ↗
5. 10.1016/S0960-8974(01)00004-310.1016/S0960-8974(01)00004-3 ↗
6. 10.1016/S0022-0248(97)00223-610.1016/S0022-0248(97)00223-6 ↗
7. 10.1016/S0022-0248(98)01095-110.1016/S0022-0248(98)01095-1 ↗
8. R. L. Hibbard, M. A. Norton, and P. J. Wegner, Design of Precision Mounts for Optimizing the Conversion Efficiency of KDP Crystals for The National Ignition Facility, Lawrence Livermore National Lab, Livermore, CA (1998).
9. 10.1179/09506600122500108510.1179/095066001225001085 ↗
10. 10.1103/PhysRevLett.24.59210.1103/PhysRevLett.24.592 ↗
11. 10.1063/1.37352110.1063/1.373521 ↗
12. 10.13182/FST94-A4024610.13182/FST94-A40246 ↗
13. 10.1016/j.fusengdes.2005.06.25110.1016/j.fusengdes.2005.06.251 ↗
14. 10.1063/1.87200510.1063/1.872005 ↗
15. 10.1080/0950034980823066010.1080/09500349808230660 ↗
16. 10.3788/HPLPB20132512.307710.3788/HPLPB20132512.3077 ↗
17. 10.1117/12.53848210.1117/12.538482 ↗
18. A. K. Burnham, H. F. Robey, N. P. Zaitseva, J. J. De, R. A. Yoreo, M. Runkel, M. Yan, M. Staggs, S. A. Couture, R. L. Combs, and R. C. Montesanti, Producing KDP and DKDP crystals for the NIF laser, ICF. Quart. Rep. 9, 135 (1999).
19. 10.1117/12.77336510.1117/12.773365 ↗
20. 10.1016/S0022-3697(99)00294-210.1016/S0022-3697(99)00294-2 ↗
21. 10.1103/PhysRevB.65.02410810.1103/PhysRevB.65.024108 ↗
22. 10.1103/PhysRevB.64.10010110.1103/PhysRevB.64.100101 ↗
23. 10.1103/PhysRevLett.80.222910.1103/PhysRevLett.80.2229 ↗
24. D. B. Sirdeshmukh, L. Sirdeshmukh, and K. G. Subhadra, Micro- and Macro-Properties of Solids Thermal, Mechanical and Dielectric Properties, Springer, New York, (2006).
25. 10.1016/S0167-577X(01)00415-310.1016/S0167-577X(01)00415-3 ↗
26. 10.1007/BF0274764210.1007/BF02747642 ↗
27. 10.1007/BF0167205710.1007/BF01672057 ↗
28. H. X. Wang, J. H. Wang, E. C. Ma, T. Sun, and S. Gao, Hardness indentation size effect of KDP crystals for ultra-precision machining surface, J. Harbin Inst. Technol. 6, 856 (2006).
29. 10.1002/crat.1980015062110.1002/crat.19800150621 ↗
30. 10.1111/j.1151-2916.2002.tb00062.x10.1111/j.1151-2916.2002.tb00062.x ↗
31. H. X. Wang, S. Gao, E. C. Ma, Q. Xu, X. H. Chen, and J. Hou, Near-surface mechanical properties of KDP crystals in single point diamond turning, Mater. Sci. Technol. 15, 133 (2007).
32. X. Cao, D. Wu, B. Wang, H. Gao, and R. Kang, Analysis on mechanical property of anisotropy of KDP crystal, J. Synth. Cryst. 3, 704 (2008).
33. 10.1063/1.169086710.1063/1.1690867 ↗
34. 10.1557/jmr.2016.9110.1557/jmr.2016.91 ↗
35. 10.1088/1674-4926/34/3/03400110.1088/1674-4926/34/3/034001 ↗
36. 10.1080/1042691090312484510.1080/10426910903124845 ↗
37. 10.3901/JME.2010.17.19210.3901/JME.2010.17.192 ↗
38. J. Peng, L. C. Zhang, and X. C. Lu, Elastic-plastic deformation of KDP crystals under nanoindentation, Mater. Sci. Forum. 773, 705 (2014).
39. 10.3901/JME.2010.13.17910.3901/JME.2010.13.179 ↗
40. D. Wang, P. Feng, C. Zhang, and J. Zhang, Experimental research on the influence of the KDP crystal anisotropy on scratch characteristics, J. Synthetic Crystals. 41, 568 (2012).
41. 10.3901/JME.2013.19.11910.3901/JME.2013.19.119 ↗
42. 10.1016/j.wear.2014.11.03210.1016/j.wear.2014.11.032 ↗
43. 10.1016/S0301-679X(99)00103-610.1016/S0301-679X(99)00103-6 ↗
44. 10.1063/1.154442910.1063/1.1544429 ↗
45. 10.1016/j.actamat.2005.06.03010.1016/j.actamat.2005.06.030 ↗
46. 10.1088/0957-4484/11/3/30710.1088/0957-4484/11/3/307 ↗
47. 10.1299/jsmea.42.54610.1299/jsmea.42.546 ↗
48. 10.1557/JMR.1999.019310.1557/JMR.1999.0193 ↗
49. C. H. Guin, M. D. Katrich, A. I. Savinkov, and M. P. Shaskolskaya, Plastic strain and dislocation structure of the KDP group crystals, Cryst. Res. Technol. 15, 479 (1980).10.1002/crat.19800150413 ↗
50. 10.1039/C2DT32131A10.1039/C2DT32131A ↗
51. 10.1103/PhysRevB.51.930210.1103/PhysRevB.51.9302 ↗
52. 10.1103/PhysRevB.55.285010.1103/PhysRevB.55.2850 ↗
53. 10.1103/PhysRevB.65.13210510.1103/PhysRevB.65.132105 ↗
54. 10.1016/j.commatsci.2015.07.04410.1016/j.commatsci.2015.07.044 ↗
55. 10.1063/1.10049110.1063/1.100491 ↗
56. K. Wang, C. Fang, J. Zhang, S. Wang, X. Sun, Q. Gu, and Y. Li, Research on laser-induced damage mechanisms of KDP crystals. J. Synthetic Crystals, 33, 48 (2004).
57. L. Diao, K. Zhang, and X. Chang, New progresses of KDP crystals in the study of laser damage threshold, J. Synthetic Crystals. 31, 99 (2002).
58. 10.1063/1.9942910.1063/1.99429 ↗
59. 10.1063/1.9663810.1063/1.96638 ↗
60. V. V. Azarov, L. V. Atroshchenko, Y. K. Danileĭko, M. I. Kolybaeva, Y. P. Minaev, V. N. Nikolaev, A. V. Sidorin, and B. I. Zakharkin, Influence of structure defects on the internal optical strength of KDP single crystals, Quant. Electron. 15, 89 (1985).
61. H. Endert and W. Melle, Influence of dislocations in KDP crystals on laser damage threshold, Cryst. Res. Technol. 16, 815 (1981).10.1002/crat.2170160713 ↗
62. 10.1007/s00340005003210.1007/s003400050032 ↗
63. 10.1364/OE.17.02165210.1364/OE.17.021652 ↗
64. 10.1063/1.192134910.1063/1.1921349 ↗
65. 10.1063/1.234525410.1063/1.2345254 ↗
66. 10.1117/12.63882910.1117/12.638829 ↗
67. 10.1117/12.53133010.1117/12.531330 ↗
68. 10.1103/PhysRevLett.91.12740210.1103/PhysRevLett.91.127402 ↗
69. 10.1117/12.83606410.1117/12.836064 ↗
70. 10.1117/12.18091210.1117/12.180912 ↗
71. 10.1063/1.9309510.1063/1.93095 ↗
72. M. Runkel, J. DeYoreo, W. Sell, and D. Milam, Laser Conditioning Study of KDP on the Optical Sciences Laser Using Large Area Beams, Lawrence Livermore National Lab., Livermore, CA (1997).
73. V. I. Salo L. V. Atroschenko S. V. Garnov and N. V. Khodeyeva Structure impurity composition and laser damage threshold of the subsurface layers in KDP and KD*P single crystals In 27th Annual Boulder Damage Symposium: Laser-Induced Damage in Optical Materials. 2714 197 (1996).10.1117/12.240416 ↗
74. 10.1070/QE1977v007n12ABEH00833210.1070/QE1977v007n12ABEH008332 ↗
75. 10.1088/1674-1056/21/5/05030110.1088/1674-1056/21/5/050301 ↗
76. 10.1063/1.366469210.1063/1.3664692 ↗
77. M. J. Chen, J. Cheng, M. Q. Li, Y. Xiao, Study of modulation property to incident laser by surface micro-defects on KH2PO4 crystal, Chin. Phys. B. 21, 064212-1(2012).
78. 10.7567/JJAP.52.03270110.7567/JJAP.52.032701 ↗
79. 10.1364/AO.52.00345110.1364/AO.52.003451 ↗
80. M. Chen, Q. Pang, and X. Liu, Finite element analysis on influence of micro-nano machined surface impurity on optical performance of crystal, High Power Laser Partic. Beams, 20, 1182 (2008).
81. 10.3788/HPLPB20102201.015910.3788/HPLPB20102201.0159 ↗
82. M. Runkel and M. McBurney, Sensing & measurement metrology aims for precision, SPIE, 12, 17 (2003).
83. 10.1177/095440541347826310.1177/0954405413478263 ↗
84. Y. Gao, P. Ge, W. Bi, and Y. Bi, Study on surface defects of KDP crystal sawed by diamond wire saw, J. Synthetic Crystals. 42, 890 (2013).
85. L. K. Jeffrey, Design of a precision saw for manufacturing, Manufact Technol. 85, UCRL-ID-125473, 4–1 (1997).
86. 10.1016/j.cirp.2010.05.00110.1016/j.cirp.2010.05.001 ↗
87. 10.2493/jjspe.65.88810.2493/jjspe.65.888 ↗
88. Y. Namba and M. Katagiri, Ultraprecision grinding of potassium dihydrogen phosphate crystals for getting optical surfaces, Laser-Induc. Damage Opt. Mater. 3578, 692 (1999).
89. D. Wu, X. Cao, Q. Wang, B. Wang, H. Gao, and R. Kang, Damage detection and analysis of machined KDP crystal subsurface, Opt. Precis. Eng. 15, 1721 (2007).
90. Q. Wang, H. Gao, Z. Pei, C. Lu, B. Wang, and X. Teng, Study on the subsurface damage of KDP crystal ground with ultrasonic vibration assistance, J. Synthetic Crystals. 39, 67 (2010).
91. 10.1117/12.78268310.1117/12.782683 ↗
92. K. Yoshida, H. Yoshida, S. Nakai, Y. Katori, and T. Okamoto, Laser damage of optically polished KDP crystal, Laser-Induc. Damage Opt. Mater. 1624, 149 (1992).
93. 10.1149/1.345886910.1149/1.3458869 ↗
94. F. Zhang, S. Guo, Y. Zhang, and D. Luan, Effect of several processing parameters on material removal ratio in the deliquescent polishing of KDP crystals, Proc. SPIE. 7282, 728227-1 (2009).
95. X. Peng, F. Jiao, H. Chen, G. Tie, F. Shi, and H. Hu, Novel magnetorheological figuring of KDP crystal, Chin. Opt. Lett. 9, 102201-1 (2011).
96. 10.1117/12.36917510.1117/12.369175 ↗
97. J. A. Menapace, P. R. Ehrmann, and R. C. Bickel, Magnetorheological Finishing (MRF) of Potassium Dihydrogen Phosphate (KDP) Crystals: Nonaqueous Fluids Development, Optical Finish, and Laser Damage Performance at 1064 nm and 532 nm, Lawrence Livermore National Laboratory (LLNL), Livermore, CA. (2009).
98. Q. Wei, Y. Meng, J. He, G. Tang, D. Zou, and Q. Luo, Design and properties of non-aqueous magnetorhological fluids for polishing KDP crystal, J. Magn. Mater Devices. 42, 41 (2011).
99. Y. Ma, S. Li, X. Peng, and H. Chen, Research on polishing KDP Crystals with MRF, Aviat. Precis. Manufac. Technol. 43, 9 (2007).
100. 10.1117/12.86722910.1117/12.867229 ↗