journal article·2026-09

Nanoscale silicon modification for enhanced corrosion resistance of polymer-derived SiC in lead-bismuth eutectic

Sijie Liu, Chunfan Liu, Xue Bai, Xueliang Pei, Chengtong Ge, Ping Yu, Bingsheng Li, Fangfang Ge, Qing Huang

Corrosion Science· Volume 270
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Silicon Carbide Semiconductor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (56)

Show source-provided references
1. GEN-IV LFR development: status & perspectives10.1016/j.pnucene.2018.02.005 ↗
2. Advanced fission energy program-ADS transmutation system
3. Experimental investigation of a LBE-helium heat exchanger based the ADS10.1016/j.pnucene.2017.04.013 ↗
4. Design study on reactor structure of Pb–Bi-cooled direct contact boiling water fast reactor (PBWFR)10.1016/j.pnucene.2007.10.026 ↗
5. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors10.1016/j.pmatsci.2022.100920 ↗
6. Radiation effects in SiC for nuclear structural applications10.1016/j.cossms.2012.03.005 ↗
7. Recycling Possibility of the Salty Food Waste by Pyrolysis and Water Scrubbing10.3390/en10020210 ↗
8. Comparative study of neutronic, mechanical and thermodynamic properties of accident tolerant cladding materials: SiC, TiC and ZrC10.1016/j.mseb.2023.116352 ↗
9. The critical issues of SiC materials for future nuclear systems10.1016/j.scriptamat.2017.03.001 ↗
10. Long-time corrosion behavior of ceramic candidates for tritium permeation barriers exposed to flowing lead lithium10.1016/j.corsci.2021.109380 ↗
11. Corrosion resistance of ceramics SiC and Si3N4 in flowing lead-bismuth eutectic10.1016/j.pnucene.2011.04.023 ↗
12. Corrosion investigations of Al–Fe-coated steels, high Cr steels, refractory metals and ceramics in lead alloys at 700 °C10.1016/j.jnucmat.2009.10.025 ↗
13. Fast-flowing LBE corrosion of the SiC pump impeller: Numerical and experimental investigations10.1111/ijac.14201 ↗
14. Dissolution corrosion of 4H-SiC in lead-bismuth eutectic at 550°C10.1002/maco.201910777 ↗
15. The selective dissolution corrosion of silicon carbide grain boundary in lead-bismuth eutectic: Insights from experimental and first-principles investigations10.1016/j.corsci.2025.113125 ↗
16. Simulation and experimental studies of the dissolution corrosion of 4H-SiC in liquid Pb/Bi10.1016/j.apsusc.2022.152686 ↗
17. First-principle Study on Adsorption and Corrosion Behavior of O, Pb and Bi Atoms on SiC Surface
18. Effects of impurity elements on SiC grain boundary stability and corrosion10.1007/s41365-021-00963-2 ↗
19. Oxygen impurity effects on the mechanical properties of SiC studied by first principles calculations10.1016/j.mtcomm.2019.03.006 ↗
20. Research Progress of SiC Fiber Reinforced SiC Composites for Nuclear Application10.15541/jim20220145 ↗
21. Residual carbon trapping effect of nano Si for stoichiometric SiC derived from polycarbosilane and its application in SiCf/SiC composites with largely improved thermal conductivity10.1016/j.jeurceramsoc.2024.05.042 ↗
22. Formation of high density stacking faults in polycrystalline 3C-SiC by vibration-assisted diamond cutting10.1016/j.jeurceramsoc.2022.06.002 ↗
23. A TEM study of in-grown stacking faults in 3C-SiC layers grown by CF-PVT on 4H-SiC substrates10.1016/j.physb.2009.08.190 ↗
24. Irradiation creep of 3C–SiC and microstructural understanding of the underlying mechanisms10.1016/j.jnucmat.2013.09.004 ↗
25. Raman spectroscopy study of heavy-ion-irradiated α-SiC10.1088/0953-8984/18/22/022 ↗
26. Raman Investigation of SiC Polytypes10.1002/1521-396X(199707)162:1<39::AID-PSSA39>3.0.CO;2-L ↗
27. Raman spectroscopy in graphene10.1016/j.physrep.2009.02.003 ↗
28. Surface characterisation of laser irradiated SiC ceramics by AES and XPS10.1007/s002160051467 ↗
29. XPS and XRD study of crystalline 3C-SiC grown by sublimation method10.1016/S0925-8388(98)00994-3 ↗
30. Surface composition of CVD-grown α-SiC layers-an XPS and LEED study10.1016/0169-4332(95)00511-0 ↗
31. Role of helium ion irradiation in the corrosion of CVD−SiC in molten LiF−NaF−KF salt10.1016/j.corsci.2021.109287 ↗
32. XPS study of hydrogen permeation effect on SiC–C films10.1016/S0168-583X(03)00963-7 ↗
33. Synthesis of ultra-thin carbon layers on SiC substrate by ion implantation10.1016/j.carbon.2015.05.046 ↗
34. Study on the corrosion behavior of laser surface remelted and laser cladding of ferritic/martensitic steels after exposure to lead-bismuth eutectic at 700 °C10.1016/j.jnucmat.2023.154888 ↗
35. A review of steel corrosion by liquid lead and lead-bismuth10.1016/j.corsci.2009.03.013 ↗
36. Bonding and wetting in non-reactive metal/SiC systems: weak or strong interfaces?10.1016/S0921-5093(99)00274-9 ↗
37. Wettability of SiC and alumina particles by liquid Bi under liquid Al10.1007/s10853-009-3907-8 ↗
38. Oxidation resistance of SiC ceramics prepared by different proceessing routes10.1016/j.jeurceramsoc.2016.03.016 ↗
39. Active to passive transition in the oxidation of silicon carbide at high temperature and low pressure in molecular and atomic oxygen10.1007/BF02403882 ↗
40. Oxidation behaviour of SiC/SiC ceramic matrix composites in air10.1016/j.jeurceramsoc.2016.05.051 ↗
41. High-temperature oxidation of silicon carbide and silicon nitride10.2320/matertrans1989.38.821 ↗
42. Gas Reactions of Carbon10.1016/S0360-0564(08)60418-6 ↗
43. Carrier depletion near the grain boundary of a SiC bicrystal
44. The fate and role of in situ formed carbon in polymer-derived ceramics10.1016/j.pmatsci.2019.100623 ↗
45. Grains, phases, and interfaces—an interpretation of microstructure
46. Effect of grain size on corrosion: a review10.5006/1.3462912 ↗
47. Crack deflection processes—I. Theory10.1016/0001-6160(83)90046-9 ↗
48. Rice · 2000
49. The roles of amorphous grain boundaries and the β–α transformation in toughening SiC10.1016/S1359-6454(97)00343-1 ↗
50. Embrittlement by Liquid Metals
51. Solute embrittlement of SiC10.1063/1.4895841 ↗
52. Embrittlement by liquid metals10.1016/0079-6425(73)90005-4 ↗
53. Effect of temperature-dependent nano SiC on the ablation resistance of ZrC coating10.1016/j.jeurceramsoc.2024.04.033 ↗
54. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
55. Gale · 2003
56. Cardarelli · 2008