Abstract
The present study demonstrates how the alloying with Co and Ni and chloride-induced nanoscale pitting in Zr-Ni-Al-based metallic glasses can be used to generate nanoporous surfaces via depassivating agents. Partial substitution of Ni with Co or Fe creates catalytically active Ni-Co and Ni-Fe surface layers during dealloying while enhancing the ability to form glasses. In NaCl, all glasses exhibit a lower corrosion rate than pure Zr but reduced pitting resistance due to Al. Electrochemical impedance spectroscopy and anodic polarization reveal that Fe impairs repassivation more severely than Co does. Thiocyanate ions induce a negative shift via complexation with Zr, and increasing SCN − destabilises passivity, as can be seen from the presence of multiple corrosion potentials. A mixed Cl − /SCN − electrolyte exhibits an additive effect. Potentiostatic polarisation at selected potentials enables controlled surface modification: at the pitting potential, the selective dissolution of Zr and Al results in significant Ni enrichment. X-ray photoelectron spectroscopy confirms the transition from a hydrated Zr-rich film to a Ni-enriched oxide surface. Crucially, uniform nanoscale pitting at controlled potentials provides a rationale for selecting depassivating agents to induce homogeneous nanoporous architectures, paving the way for water-splitting electrocatalysts.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Electrodeposition and Electroless Coatings · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. An overview of water electrolysis technologies for green hydrogen production10.1016/j.egyr.2022.10.127 ↗
2. Review – Challenges and opportunities for increased current density in alkaline electrolysis by increasing the operating temperature10.1149/1945-7111/ac34cc ↗
3. Strategic research and innovation
4. Nickel- and cobalt-based catalysts for hydrogen generation by hydrolysis of borohydride10.1016/j.jallcom.2005.08.019 ↗
5. Bridging laboratory electrocatalysts with industrially relevant alkaline water electrolyzers
6. Simple process to nanostructured Raney-nickel electrodes for highly active and cost-efficient hydrogen evolution in alkaline water electrolysis (AWE)10.1016/j.ijhydene.2025.02.398 ↗
7. Co-modification of Ni-based type Raney electrodeposits for hydrogen evolution reaction in alkaline media10.1016/j.jpowsour.2013.05.041 ↗
8. A powder metallurgy route to produce Raney-nickel electrodes for alkaline water electrolysis10.1149/2.0851904jes ↗
9. Improving plasma sprayed Raney-type nickel–molybdenum electrodes towards high-performance hydrogen evolution in alkaline medium10.1038/s41598-020-67954-y ↗
10. Selective dissolution of amorphous and nanocrystalline Zr2Ni10.1016/j.corsci.2013.05.004 ↗
11. L. Road, The electrochemical properties of metallic glasses10.1016/0013-4686(87)87002-0 ↗
12. Baiker · 1994 · 263
13. Properties, mechanisms and advantages of metallic glass for electrocatalysis and HER in water splitting: A review10.1016/j.ijhydene.2023.03.324 ↗
14. Amorphous alloys for electrocatalysis: The significant role of the amorphous alloy structure10.1007/s12274-021-3682-7 ↗
15. Catalytic applications of amorphous alloys: Expectations, achievements, and disappointments10.1016/j.apsusc.2010.12.046 ↗
16. Porous metallic structures by dealloying amorphous alloys10.1016/j.jallcom.2023.172417 ↗
17. Nanoporous metallic structures by de-alloying bulk glass forming Zr-based alloys10.1016/j.intermet.2018.05.002 ↗
18. The mechanism of generating nanoporous Au by de-alloying amorphous alloys10.1016/j.actamat.2016.08.025 ↗
19. Formation of nano-porous Pd(Ni) structure produced by dealloying Zr-Al-Ni-Pd base glassy alloys and their electrochemical properties10.1016/j.jnoncrysol.2019.03.029 ↗
20. Advances in dealloying of Ti and Ti-based alloys for biomedical applications10.3390/ma18184424 ↗
21. Acid treatments of Ti-based metallic glasses for improving corrosion resistance in implant applications10.3390/met14020241 ↗
22. Surface modification of Ti40Cu40Zr11Fe3Sn3Ag3 amorphous alloy for enhanced biocompatibility in implant applications10.1016/j.jmrt.2024.03.225 ↗
23. Nanoporous metals based on metallic glasses: synthesis, structure and functional applications10.1007/s40195-023-01597-6 ↗
24. Metallic glasses and metallic glass nanostructures for functional electrocatalytic applications10.1016/j.cclet.2021.12.013 ↗
25. Recent development of chemically complex metallic glasses: From accelerated compositional design, additive manufacturing to novel applications
26. Designing biocompatible Ti-based metallic glasses for implant applications10.1016/j.msec.2012.11.015 ↗
27. Nine years of research and development on advanced water electrolysis. A review of the research programme of the Commission of the European Communities10.1007/BF01016198 ↗
28. NiFe alloy integrated with amorphous/crystalline NiFe oxide as an electrocatalyst for alkaline hydrogen and oxygen evolution reactions10.1021/acsomega.3c00322 ↗
29. Liquid ejection temperature dependence of structure and glass transition behavior for rapidly solidified Zr-Al-M (M=Ni, Cu or Co) ternary glassy alloys10.1016/j.jallcom.2017.12.318 ↗
30. Influence of ejection temperature on structure and glass transition behavior for Zr-based rapidly quenched disordered alloys10.1016/j.actamat.2016.06.049 ↗
31. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element10.2320/matertrans.46.2817 ↗
32. Abnormal isochronous crystallization behavior of Zr-Al-Ni-Cu-Fe-C bulk metallic glasses10.1016/j.jallcom.2020.156250 ↗
33. Effect of the atomic size distribution on glass forming ability of amorphous metallic alloys10.1016/S0025-5408(01)00715-2 ↗
34. 2011, P.MarcusCorrosion mechanisms in theory and practiceCRC Press.
35. Electrochemical aspects of pitting corrosion10.1016/S0010-938X(67)80073-8 ↗
36. Barsoukov · 2018
37. Impedance of mediated electrochemical processes. Novel impedance element for unequal diffusivities10.1021/jp412769h ↗
38. Kinetik der Metallabscheidung aus Lösungen komplexgebundener Ionen10.1002/cite.330360612 ↗
39. On the atomic structure of Zr-Ni and Zr-Ni-Al metallic glasses10.1063/1.3446131 ↗
40. A study of the glass forming ability in ZrNiAl alloys10.1016/j.msea.2006.08.109 ↗
41. Electrochemical corrosion behavior of industrial pure zirconium in high Cl- containing solutions10.1016/j.ijoes.2024.100485 ↗
42. Pitting corrosion mechanisms of Ti-Cu-(Pd-) based metallic glasses in simulated physiological solution10.1016/j.corsci.2025.112913 ↗
43. Effect of different welding processes on electrochemical and corrosion behavior of pure nickel in 1 M NaCl solution
44. Pitting corrosion of aluminum10.1016/S0010-938X(99)00012-8 ↗
45. Corrosion of aluminum in contact with oxidized titanium and zirconium10.1007/s11003-016-9894-4 ↗
46. Differences in pitting growth kinetics between Zr60Ni25Al15 and Zr60Cu25Al15 metallic glasses exposed to a 0.6 M NaCl aqueous solution10.1016/j.corsci.2017.09.007 ↗
47. Improved biocompatibility of Ti-based bulk metallic glasses by electrochemical formation of nanoporous oxide layers
48. Corrosion resistance and microstructure of electrodeposited nickel – cobalt alloy coatings10.1016/j.surfcoat.2006.06.017 ↗
49. Influence of the alkyl chain length of 2 amino 5 alkyl 1,3,4 thiadiazole compounds on the corrosion inhibition of steel immersed in sulfuric acid solutions10.1016/j.corsci.2011.09.020 ↗
50. The study of the passivation process by the electrode impedance analysis
51. Impedance as a tool for rapid and complete characterization of electrocatalytic systems involving redox mediators10.1016/j.electacta.2015.11.049 ↗
52. J. Kristin, How the multi-phase microstructure of a novel tool steel determines its corrosion behaviour in sulphuric acids10.1016/j.corsci.2024.112091 ↗
53. A Comparative study on the electrochemical corrosion behavior of iron and X-65 Steel in 4.0 wt% sodium chloride solution after different exposure intervals10.3390/molecules19079962 ↗
54. Pitting corrosion of bulk glass-forming zirconium-based alloys10.1016/j.jallcom.2004.01.043 ↗
55. Electroanalytical methods
56. Investigation of Zr(IV), Hf(IV) and Th(IV) thiocyanate complexes by extraction with thenoyltrifluoroacetone and dinonyl napthalene sulphonic acid10.1016/0022-1902(71)80674-7 ↗
57. Uniform and pitting corrosion events induced by SCN- anions on Al alloys surfaces and the effect of UV light10.1016/j.electacta.2010.12.045 ↗
58. Inhibitors for the corrosion of reactive metals: Titanium and zirconium and their alloys in acid media10.1016/0010-938X(81)90004-4 ↗
59. Electrochemical impedance spectroscopic study of passive zirconium10.1016/j.jnucmat.2008.06.011 ↗
60. A guide to polarisation curve interpretation: Deconstruction of experimental curves typical of the Fe/H2O/H+/O2 corrosion system10.1016/j.corsci.2004.10.002 ↗
61. Pedeferri · 2018
62. Electrochemical behaviour of high nitrogen bearing stainless steel in acidic chloride solution: Effects of oxygen, acid concentration and surface roughness10.1016/j.electacta.2008.10.038 ↗
63. A practical anodic and cathodic curve intersection model to understand multiple corrosion potentials of Fe-based glassy alloys in OH- contained solutions
64. Moulder · 1995
65. Effects of oxidizing media on the composition, morphology and optical properties of colloidal zirconium oxide nanoparticles synthesized via pulsed laser ablation in liquid technique10.1166/jnn.2018.15244 ↗