Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Nuclear reactor physics and engineering · Fusion materials and technologies · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors10.1016/j.pmatsci.2022.100920 ↗
2. Low-temperature oxy-nitriding of 316 L austenitic stainless steel for improved corrosion resistance in liquid lead-bismuth eutectic10.1016/j.scriptamat.2021.114014 ↗
3. The roles of Ni segregation on the oxidation kinetics of austenitic stainless steel 316L exposed to oxygen-containing liquid lead-bismuth eutectic (LBE)10.1016/j.corsci.2024.112644 ↗
4. The effect of Si on the microstructure and corrosion resistance of XSi9Cr ferritic/martensitic steel in oxygen-saturated lead-bismuth eutectic10.1016/j.corsci.2025.113079 ↗
5. Pb corrosion of ferritic/martensitic steels at 600-700 °C10.1016/j.corsci.2025.113142 ↗
6. On oxidation film structure of SIMP steel exposed in stagnant oxygen-saturated LBE at 600 °C10.1016/j.corsci.2024.111927 ↗
7. Influence of temperature on the interaction mode of T91 and AISI 316L steels with Pb-Bi melt saturated by oxygen10.1016/j.corsci.2008.02.006 ↗
8. High temperature oxidation of Fe-9Cr-1Mo steel in stagnant liquid lead-bismuth at several temperatures and for different lead contents in the liquid alloy10.1016/j.jnucmat.2008.02.006 ↗
9. Liquid metal corrosion of T91 and A316L materials in Pb-Bi eutectic at temperatures 400-600 °C10.1016/j.corsci.2005.04.001 ↗
10. Growth and Exfoliation Behavior of the Oxide Scale on 316L and T91 in Flowing Liquid Lead-Bismuth Eutectic at 480 °C10.1007/s11085-019-09953-7 ↗
11. Corrosion behavior of T91 steel in liquid lead-bismuth eutectic at 550 °C: Effects of exposure time and dissolved oxygen concentration10.1016/j.corsci.2022.110405 ↗
12. Honeycomb structure with oxygen-poor pores at the top of magnetite layer on a martensitic steel CLAM exposed to lead-bismuth eutectic at 500 ºC10.1016/j.corsci.2022.110410 ↗
13. Silicon-containing ferritic/martensitic steel after exposure to oxygen-containing flowing lead-bismuth eutectic at 450 and 550 °C10.1016/j.jnucmat.2015.11.058 ↗
14. Oxidative passivation of Fe-Cr-Al steels in lead-bismuth eutectic under oxygen-controlled static conditions at 700° and 800 °C10.1016/j.jnucmat.2019.06.004 ↗
15. Corrosion behaviors of FeCrAl alloys exposed to oxygen-saturated static lead bismuth eutectic at 550 °C10.1016/j.corsci.2022.110767 ↗
16. Effect of silicon on the oxidation resistance of 9 wt% Cr heat resistance steels in 550 °C lead-bismuth eutectic10.1016/j.corsci.2016.04.020 ↗
17. Corrosion resistance of alloys F91 and Fe-12Cr-2Si in lead-bismuth eutectic up to 715 °C10.1016/j.jnucmat.2012.11.010 ↗
18. Silicon enhances high temperature oxidation resistance of SIMP steel at 700 °C10.1016/j.corsci.2020.108519 ↗
19. A Comparative Study of the EP823 Steel Corrosion Resistance in Lead and Lead-Bismuth Coolants10.1007/s10512-023-01008-0 ↗
20. Comparison investigation on corrosion of SIMP and T91 steels exposed to liquid LBE at 450 °C: The role of Si on reducing oxidation rate10.1016/j.corsci.2023.111553 ↗
21. Long-term corrosion performance of T91 ferritic/martensitic steel at 400 °C in flowing Pb-Bi eutectic with 2 × 10−7 mass% dissolved oxygen10.1016/j.corsci.2020.108852 ↗
22. On the LME susceptibility of Si enriched steels10.1016/j.jnucmat.2012.05.017 ↗
23. Effect of silicon on oxidation behavior of 9Cr-ODS steel at 650 °C10.1016/j.fusengdes.2021.112384 ↗
24. Effect of alloying elements on liquid metal embrittlement of pure BCC Fe in contact with liquid lead-bismuth eutectic: Experiments and first principles calculation10.1016/j.corsci.2022.110522 ↗
25. Effect of silicon on the microstructure and mechanical properties of reduced activation ferritic/martensitic steel10.1016/j.jnucmat.2015.01.004 ↗
26. Mechanical properties and microstructure of three Russian ferritic/martensitic steels irradiated in BN-350 reactor to 50dpa at 490 °C10.1016/j.jnucmat.2007.03.161 ↗
27. Effects of pre-formed nanostructured surface layer on oxidation behaviour of 9Cr2WVTa steel in air and liquid Pb-Bi eutectic alloy10.1016/j.corsci.2015.10.021 ↗
28. The role of grain boundaries in the initial oxidation behavior of austenitic stainless steel containing alloyed Cu at 700 °C for advanced thermal power plant applications10.1016/j.corsci.2015.03.014 ↗
29. Grain size effects on the oxidation of two-phase Cu-Fe alloys10.1016/S0010-938X(01)00153-6 ↗
30. Response of equal channel angular extrusion processed ultrafine-grained T91 steel subjected to high temperature heavy ion irradiation10.1016/j.actamat.2014.04.034 ↗
31. Nanostructured metals under irradiation10.1016/j.scriptamat.2009.01.011 ↗
32. Microstructure modification and mechanical property improvement of reduced activation ferritic/martensitic steel by severe plastic deformation10.1016/j.msea.2017.11.095 ↗
33. Evolution of microstructure and mechanical properties of 9Cr ferrite/martensite steels with different Si content after long-term aging at 550 °C10.1016/j.jallcom.2021.159817 ↗
34. Oxidation behavior of ferritic/martensitic steels in stagnant liquid LBE saturated by oxygen at 600 °C10.1016/j.jnucmat.2014.11.018 ↗
35. High corrosion resistance of twin boundaries in medium-entropy alloy exposed to liquid lead-bismuth eutectic at 500 °C: Mechanism exploration by both experiment and first-principles calculation10.1016/j.corsci.2022.110865 ↗
36. The structure dependence of grain boundary passivation of Alloy 690 in high temperature water10.1016/j.actamat.2023.119368 ↗
37. Corrosion behaviors of ODS-FeCrAl in oxygen-saturated lead-bismuth eutectic at 550 °C: Effects of grain boundaries and minor elements10.1016/j.jnucmat.2023.154710 ↗
38. New insight of the enhanced oxidation resistance of T91 steel in 450 °C liquid lead-bismuth eutectic by adding Al and Si element10.1016/j.jmst.2024.03.033 ↗
39. Schroer · Physical Chemistry of Corrosion and Oxygen Control in Liquid Lead and Lead-Bismuth Eutectic · 2007
40. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
41. Corrosion Behavior of Stainless Steels in Simulated PWR Primary Water—Effect of Chromium Content in Alloys and Dissolved Hydrogen10.1080/18811248.2008.9711883 ↗
42. Corrosion of 9Cr Steel in CO2 at Intermediate Temperature I: Mechanism of Void-Induced Duplex Oxide Formation10.1007/s11085-011-9271-5 ↗
43. Modelling of the oxide scale formation on Fe-Cr steel during exposure in liquid lead-bismuth eutectic in the 450-600 °C temperature range10.1002/maco.201005871 ↗
44. Oxidation mechanism of an Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy at 470 °C (Part II)10.1016/j.corsci.2008.06.051 ↗
45. Insights into the corrosion mechanism of a 12Cr F/M steel in oxygen-saturated liquid LBE10.1016/j.corsci.2023.111602 ↗
46. Towards improved prediction of scale exfoliation from steam tubes10.3184/096034007X277933 ↗
47. Microstructural evidence for short-circuit oxygen diffusion paths in the oxidation of a dilute Ni-Cr alloy10.1007/BF01046984 ↗
48. Effect of grain refinement on the resistance of 304 stainless steel to breakaway oxidation in wet air10.1016/j.actamat.2005.07.019 ↗
49. High temperature corrosion behavior of Cu-20Co-30Cr alloys with different grain size10.1016/j.corsci.2013.11.025 ↗
50. Volume and grain-boundary diffusion in 20 Cr/25 Ni/Nb stainless steel10.1179/msc.1969.3.1.93 ↗
51. Calculation of diffusion penetration curves for surface and grain boundary diffusion10.1063/1.1699825 ↗
52. Measurement of oxygen grain boundary diffusion in natural, fine-grained, quartz aggregates10.1016/0016-7037(91)90131-N ↗
53. First study of manganese diffusion in Cr2O3 polycrystals and thin films by SIMS10.1080/14786430601120462 ↗
54. On the role of surface deformation in the oxidation of NiCr alloys at 340-600 °C10.1016/j.corsci.2020.108805 ↗
55. Influence of Si addition on the corrosion behavior of 9 wt% Cr ferritic/martensitic steels exposed to oxygen-controlled molten Pb-Bi eutectic at 550 and 600 °C10.1016/j.corsci.2021.109871 ↗
56. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part I)10.1016/j.corsci.2008.06.050 ↗
57. A kinematical theory of diffraction contrast of electron transmission microscope images of dislocations and other defects10.1098/rsta.1960.0013 ↗
58. Revealing the microstructure evolution and embrittlement of Z3CN20–09 M stainless steel over 60 equivalent service years in PWR10.1016/j.jnucmat.2025.156087 ↗
59. An in-situ TEM characterization of electron beam induced dislocation motion in a single-crystalline gold thin film10.1016/j.matchar.2021.111697 ↗
60. Deformation mechanisms of Al thin films: In-situ TEM and molecular dynamics study10.1016/j.scriptamat.2022.114688 ↗
61. Study of the Influence of Surface Finishing on the Corrosion/Oxidation Behaviour of Stainless Steels in Stagnant Lead Bismuth Eutectic